Modification of Mg2Si morphology in Mg–9%Al–0.7%Si alloy by the SIMA process
Source abstract
Abstract
Abstract The effect of predeformation on the semisolid microstructure of Mg–9%Al–0.7%Si alloy produced by the strain induced melt activation (SIMA) process was studied. Experimental results indicated that a non-dendritic microstructure could be obtained by the SIMA process in the alloy. With the reduction ratio varying from 0% to 30%, the volume fraction of liquid gradually enlarged from 37.26 vol.% to 48.28 vol.%, and the morphology of α-Mg grains transformed from dendritic shape to spherical shape, with a size of 52.16 μm. Also, the liquid islands in the grains become less with the increase of the reduction ratio. In addition, the eutectic Mg 2 Si phase transformed from Chinese script shape to globular shape during the isothermal heat treatment. A possible reason of the modification of Mg 2 Si morphology is the shifting of the eutectic composition of the liquid towards lower silicon contents with increasing Al content.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. The effect of mechanical milling on the formation of nanocrystalline Mg2Si through solid-state reaction10.1016/S1359-6462(03)00241-0 ↗
2. Modification of Mg2Si in Mg–Si alloys with K2TiF6, KBF4 and KBF4+K2TiF610.1016/j.jallcom.2004.06.027 ↗
3. Microstructural development of Al–15wt.%Mg2Si in situ composite with mischmetal addition10.1016/S0921-5093(99)00732-7 ↗
4. Magnesium alloying, some potentials for alloy development10.2464/jilm.42.679 ↗
5. High strength and high strain rate superplasticity in a Mg–Mg2Si composite10.1016/0956-716X(95)00140-Q ↗
6. Elevated temperature mechanical properties of magnesium alloys containing Mg2Si10.1179/mst.1996.12.1.35 ↗
7. Fabrication and properties of rapidly solidified magnesium and Mg–Si alloys10.1179/mst.1990.6.7.629 ↗
8. Microstructure and mechanical properties of mechanically alloyed intermetallic Mg2Si–Al alloys
9. Effects of silicon on microstructure, fluidity, mechanical properties, and fracture behaviour of Mg–6Al alloy10.1179/026708301101509872 ↗
10. Modification of Mg2Si morphology in squeeze cast Mg–Al–Zn–Si alloys by Ca or P addition10.1016/S1359-6462(99)00172-4 ↗
11. Microstructure refinement of Mg–Al–Zn–Si alloys10.1016/S0167-577X(02)00417-2 ↗
12. Effect of Mg2Si particles on the elevated temperature tensile properties of squeeze-cast Mg–Al alloys10.1007/s11661-004-0268-4 ↗
13. Microstructure and mechanical properties of Si and Sb added AZ91 magnesium alloy10.1007/s11661-005-0342-6 ↗
14. Modification of Mg2Si morphology in as-cast Mg–Al–Si alloys with strontium and antimony10.4028/www.scientific.net/MSF.510-511.238 ↗
15. Quimby · 2006 · 535
16. An investigation on hot-crack mechanism of Ca addition into AZ91D alloy10.1007/s10853-005-2440-7 ↗
17. The rheology of a partially solid alloy
18. Structural evolution of conventional cast dendritic and spray-cast non-dendritic structures during isothermal holding in the semi-solid state10.1016/S1359-6462(97)00394-1 ↗
19. Evolution of near-equiaxed microstructure in the semisolid state10.1016/S0921-5093(00)00908-4 ↗
20. Generation of dislocations and subgrains in stir cast Al–6.2Si alloy during semisolid state processing10.1179/mst.1998.14.8.770 ↗
21. A comparative characterization of near-equiaxed microstructures as produced by spray casting, magnetohydrodynamic casting and the stress induced, melt activated process10.1016/S0921-5093(00)00907-2 ↗
22. The melting behaviour of extruded Mg–8%Al–2%Zn alloy10.1016/S1359-6454(03)00163-0 ↗
23. Effect of semi-solid isothermal heat treatment on the microstructure of Mg–6A1–1Zn–0.7Si alloy10.1016/j.jmatprotec.2007.12.041 ↗
24. Effect of holding time on microstructure of Mg–9Al–1Si alloy during semisolid isothermal heat treatment10.1016/S1003-6326(10)60512-2 ↗
25. Effect of predeformation on the semisolid microstructure of Mg–9Al–0.6Zn alloy10.1016/j.matlet.2004.07.044 ↗
26. Microstructure evolution of in situ Mg2Si/Al–Si–Cu composite in semisolid remelting processing10.1016/j.msea.2005.07.021 ↗
27. Microstructure of stir-cast metals10.1016/0025-5416(84)90211-8 ↗
28. Effect of holding temperature on microstructure of an AS91 alloy during semisolid isothermal heat treatment10.1016/j.jallcom.2010.02.115 ↗
29. Microstructural evolution of Mg–5Si–1Al alloy during partial remelting10.1016/j.jallcom.2008.05.016 ↗