Characterization of 3-phase (ternary-like) n-type and p-type thermoelectric materials fabricated by explosive (shock-wave) consolidation
Source abstract
Abstract
Abstract Three-phase powder mixtures of Bi–Te–Se and Bi–Te–Sb were prepared by cylindrical explosive consolidation to emulate traditional, melt-grown n-type and p-type doped Bi 2 Te 3 thermoelectric materials. The powder diameters ranged from 40 μm to 3 μm, with starting Bi and Te particle Vickers microindentation hardnesses of 0.18 and 0.56 GPa, respectively, in contrast to average shocked n-type and p-type monolith microindentation hardnesses of 1.15 and 1.31 GPa, respectively. The values may also be contrasted to 0.72 and 0.68 GPa hardnesses for melt-grown n-type and p-type materials, respectively. Shock consolidated monolith microstructures were characterized by optical metallography, SEM and TEM along with EDS analysis and XRD of all materials, including the melt-grown materials which had measured thermoelectric parameters considerably in excess of the shock (explosively) consolidated monoliths. Notable shock microstructures were characterized by deformation twins, while the melt-grown materials contained considerable, fine eutectic microstructures. These shock-grown microstructures do not appear to be conducive to thermoelectric figure of merit optimization.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Thermal properties of materials · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. 1995
2. Holas · 2001
3. Thermoelectricity in semiconductor nanostructures10.1126/science.1093164 ↗
4. Thermal conductivity of Si/SiGe superlattice nanowires10.1063/1.1619221 ↗
5. Thermal conductivity reduction and thermoelectric figure of merit increase by embedding nanoparticles in crystalline semiconductors10.1103/PhysRevLett.96.045901 ↗
6. Nanostructuring expands thermal limits10.1016/S1748-0132(07)70018-X ↗
7. Low thermal conductivity in W/Al2O3 nanolaminates10.1126/science.1093711 ↗
8. Thermal conductivity of GaN films: effects of impurities and dislocations10.1063/1.1497704 ↗
9. The effect of boundary scattering in the high-temperature thermal conductivity of silicon
10. The maximum possible conversion efficiency of silicon–germanium thermoelectric generators10.1063/1.349385 ↗
11. 2002
12. Prümmer · 1987
13. An improved method for shock consolidation of powders10.1016/0001-6160(88)90147-2 ↗
14. 1988
15. Murr LE, Staudhammer KP. Shock wave sensitization, shock-induced reactivity, and new materials fabrication, Chap. 12, ibid, p. 441.
16. Shock-induced and shock-assisted solid-state chemical reactions10.1063/1.357624 ↗
17. Twinned crystals10.1080/00018735400101223 ↗
18. Magnetoplastic effect upon twinning of bismuth single crystal
19. Effect of plastic deformation on the thermal conductivity of bismuth crystals10.1143/JPSJ.41.1692 ↗
20. Determination of the dynamic phase transitions in bismuth with in-material manganin gausges10.1063/1.333855 ↗
21. Phase transition and Hugoniot data in shock loaded bismuth
22. Solid–liquid and solid–solid phase transitions in some pure methods at high temperatures and pressures
23. Murr · 1991
24. Staudhammer · 1973
25. Grain boundary influence on the electrical properties of tellurium microstructures ingots and nanocluster crystals10.4028/www.scientific.net/MSF.508.25 ↗
26. Study of dislocations in deformed Te by electron microscopy
27. High performance N-type bismuth telluride with highly stable thermoelectric figure of merit10.1063/1.1712013 ↗