journal article·2014-01

RETRACTED: Development of microstructure and chemical composition of hydration products of slag activated by ordinary Portland cement

Haining Geng, Qiu Li

This record is marked as retracted by the source. Review the publisher’s notice before using its findings.
Publisher page

Abstract

This article has been retracted: please see Elsevier Policy on Article Withdrawal ( http://www.elsevier.com/locate/withdrawalpolicy ). This article has been retracted at the request of the Editor-in-Chief. The article contained data that the authors did not have permission to use. Hence, this article represents a severe abuse of the scientific publishing system. The scientific community takes a very strong view on this matter and apologies are offered to readers of the journal that this was not detected during the submission process.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete and Cement Materials Research · Magnesium Oxide Properties and Applications · Recycling and utilization of industrial and municipal waste in materials production

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Feret · 1939
2. Davidovits J, Sawyer JL. U.S. Patent No. 4,509,985. U.S.1985.
3. Krivenko · 1986
4. High strength slag-alkaline binders
5. Present state and future of alkaliactivated slag and concretes. Fly Ash, Silica Fume, Slag, and Natural Pozzlons in Concrete
6. Eearly activation and properties of slag cement at early age10.1016/0008-8846(90)90060-B ↗
7. New rapid setting alkali activated cement compositions10.1557/PROC-179-203 ↗
8. Alkali-activated materials: an overview10.1557/PROC-245-153 ↗
9. Hydration products of alkali activated slag cement10.1016/0008-8846(95)00045-E ↗
10. The mineralogy and microstructure of three composite cements with high replacement levels10.1016/S0958-9465(01)00041-5 ↗
11. Influence of mineralogy on the hydraulic properties of ladle slag10.1016/j.cemconres.2011.04.003 ↗
12. Advances in alternative cementitious binders10.1016/j.cemconres.2010.11.012 ↗
13. A review: the comparison between alkali-activated slag (Si plus Ca) and metakaolin (Si plus Al) cements10.1016/j.cemconres.2010.03.020 ↗
14. Alkali-activated slag: hydration process and development of microstructure10.1680/adcr.2000.12.4.163 ↗
15. Hydration and properties of novel blended cements based on cement kiln dust and blast furnace slag10.1016/S0008-8846(03)00061-9 ↗
16. Methods for determination of degree of reaction of slag in blended cement pastes10.1016/j.cemconres.2011.11.010 ↗
17. Pore solution chemistry of alkali-activated ground granulated blast-furnace slag10.1016/S0008-8846(98)00212-9 ↗
18. Sodium silicate-based, alkali-activated slag mortars Part I. Strength, hydration and microstructure10.1016/S0008-8846(02)00717-2 ↗
19. The influence of blast-furnace slag hydration products on microcracking of concrete10.1016/j.matchar.2008.11.011 ↗
20. Microstructure and microanalysis of hardened cement pastes involving ground granulated blast-furnace slag10.1007/BF01133772 ↗
21. Hydration of alkali-activated slag: comparison with ordinary Portland cement10.1680/adcr.2006.18.3.119 ↗
22. Hydration mechanisms of super sulphated slag cement10.1016/j.cemconres.2008.03.004 ↗
23. The nature of C-S-H in model slag-cements10.1016/S0958-9465(00)00022-6 ↗
24. Effect of supplementary cementing materials on the composition of cement hydration products10.1016/1065-7355(95)90024-1 ↗
25. Effect on fresh C-S-H gels of the simultaneous addition of alkali and aluminium10.1016/j.cemconres.2009.08.004 ↗
26. The characterization of hardened alkali-activated blast-furnace slag pastes and the nature of the calciu silicate hydrate (C-S-H) phase10.1016/0008-8846(94)90002-7 ↗
27. Location of aluminum in substituted silicate hydrate (C-S-H) gels as determined by 29Si and 27Al NMR and EELS10.1111/j.1151-2916.1993.tb07765.x ↗
28. Li · 2009
29. Taylor · 1997
30. The effect of temperature on the early hydration of Portland cement and blended cements10.1680/adcr.2000.12.3.121 ↗
31. Hydration of alkali-activated ground granulated blast furnace slag10.1023/A:1004742027117 ↗
32. Structure and behaviour of slag Portland cement hydrates
33. Microstructure and microchemistry of slag cement pastes10.1557/PROC-86-199 ↗
34. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag - Part II: Effect of Al2O310.1016/j.cemconres.2011.08.005 ↗
35. Kocaba · 2009
36. Structure of hydrated glassy blastfurnace in concrete
37. Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags10.1016/j.cemconres.2010.11.016 ↗
38. Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag - Part I: Effect of MgO10.1016/j.cemconres.2011.05.002 ↗
39. Hydration products and reactivity of blast-furnace slag activated by various alkalis10.1111/j.1151-2916.2003.tb03623.x ↗
40. Hydration degree of alkali-activated slags: a 29Si NMR study10.1111/j.1551-2916.2011.04828.x ↗
41. Density and water content of nanoscale solid C-S-H formed in alkali-activated slag (AAS) paste and implications for chemical shrinkage10.1016/j.cemconres.2011.11.003 ↗