Abstract Interdiffusion behavior of Fe-FeSi diffusion couple at 1050–1150 °C for up to 12 h under 6 T strong magnetic field has been investigated, and the dual-effects of strong magnetic field on interdiffusion behavior have been observed. Strong magnetic field significantly promotes diffusion of solid solution layer with the increased thickness about 425 μm and Si content about 6.3 wt% at 1100 °C for 12 h because of the increased frequency factor rather than the activation energy. The increased dislocation density was demonstrated by the broadening and shifting of X-ray diffraction peaks and the atomic scale observations with high resolution transmission electron microscope. The dislocation on the Fe20 wt%Si side increases lattice parameters of Fe3Si, and the suppressed diffusion of Fe3Si under magnetic field is primary due to the decreased frequency factor.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electromagnetic Effects on Materials · Metallic Glasses and Amorphous Alloys · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Effect of annealing on the microstructure and magnetic properties of soft magnetic Fe-Si produced via laser additive manufacturing10.1016/j.scriptamat.2017.08.042 ↗
2. Calorimetric study and microstructure analysis of the order-disorder phase transformation in silicon steel built by SLM10.1016/j.jallcom.2017.06.085 ↗
3. Ordered phases and microhardness of Fe-6.5%Si steel sheet after hot rolling and annealing10.1016/j.msea.2015.09.068 ↗
4. Evolution of microstructure and texture in grain-oriented 6.5%Si steel processed by strip-casting10.1016/j.matchar.2017.02.022 ↗
5. Study on the pulse reverse electrodeposition of Fe-nano-Si composite coatings in magnetic field10.1016/j.apsusc.2014.05.030 ↗
6. The effect of heat treatments and Si contents on B2 ordering reaction in high-silicon steels10.1016/S0921-5093(00)01960-2 ↗
7. Behavior of Fe/nano-Si particles composite electrodeposition with a vertical electrode system in a static parallel magnetic field10.1016/j.electacta.2013.07.225 ↗
8. Magnetic properties and workability of 6.5% Si steel sheet10.1016/0304-8853(96)00128-X ↗
9. A study on magnetic properties of high Si steel obtained through powder rolling processing10.1016/j.jmmm.2007.05.008 ↗
10. 6.5 wt%Si high silicon steel sheets prepared by composite electrodeposition in magnetic field10.1016/j.jmst.2018.06.004 ↗
11. Magnetic properties of high silicon iron sheet fabricated by direct powder rolling10.1016/j.jmmm.2004.04.098 ↗
12. Metallurgy of high-silicon steel parts produced using Selective Laser Melting10.1016/j.actamat.2016.03.037 ↗
13. Effects of parallel magnetic field on electrocodeposition behavior of Fe/nano-Si particles composite electroplating10.1016/j.apsusc.2013.06.022 ↗
14. On the theory of diffusion in a magnetic field10.1139/p64-204 ↗
15. Influence of strong static magnetic field on intermediate phase growth in Mg-Al diffusion couple10.1016/j.jallcom.2006.09.032 ↗
16. Phase formation and growth in Al-Mg couple with an electromagnetic field10.1016/j.matlet.2003.10.019 ↗
17. Phase growth in diffusion couples under an low frequency alternating magnetic field10.1016/j.scriptamat.2004.05.025 ↗
18. Effect of static magnetic field on microstructure and interdiffusion behavior of Fe/Fe-Si alloy diffusion couple10.1016/j.jallcom.2015.04.226 ↗
19. Enhanced diffusivity in Ni-Al system by alternating magnetic field
20. Alternating-magnetic-field induced enhancement of diffusivity in Ni-Cr alloys10.1038/s41598-017-18500-w ↗
21. An investigation on the role of texture evolution and ordered phase transition in soft magnetic properties of Fe-6.5wt%Si electrical steel10.1016/j.jmmm.2017.01.054 ↗
22. Effect of silica additive on the high-temperature fireside tube corrosion during the air-firing and oxy-firing of lignite (Xinjiang coal) - characteristics of bulk and cross-sectional surfaces for the tubes10.1016/j.fuel.2016.09.040 ↗
23. Preparation of high silicon steel by multi-arc ion coating and diffusion10.1016/S1875-5372(16)30023-6 ↗
24. Mehrer · 1990