Microstructure and mechanical properties of hot-pressed Ti–Co–Si compounds reinforced by intermetallic phases
Source abstract
Abstract
Abstract Monolithic TiCo and Ti5Si3 phases and Co(ss)/Ti5Si3–Ti3Co2Si nanocomposite were fabricated via mechanical alloying followed by hot-pressing (HP). The XRD patterns of bulk samples showed a general decrease in peak widths after hot-pressing owing to an increase in crystal size caused by exposure to high temperature during the HP process. Nevertheless, the nano-crystallinity of the structure was retained after HP and no new phase was formed. As a dominant fracture mode, this material exhibited an intergranular fracture feature with low dimpled ruptures. Dry-sliding wear behavior was evaluated at room and high temperatures. The mean coefficient of friction and wear rate gradually decreased with increasing temperature due to the presence of discontinuous thin tribo-oxide and tribo-nitride layers on the worn surface. The wear rate obtained in this work was ~10 times lower than that previously reported for Ti compounds.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced materials and composites · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Effect of temperature on wear behavior in a Ti-V-Cr Base fireproof titanium alloy10.1007/s12541-017-0184-3 ↗
2. Friction and Wear characteristics of 20Cr steel substrate and TiAlN coating under different lubrication conditions10.1007/s12541-018-0179-8 ↗
3. High temperature oxidation and wear behaviors of Ti–V–Cr fireproof titanium alloy10.3390/met7060226 ↗
4. Research on the cutting performances and wear mechanisms of TiAlCrN coated tools during dry turning10.1007/s12541-019-00026-y ↗
5. Wear and oxidation behaviour of high-chromium white cast irons10.1016/j.matchar.2007.05.021 ↗
6. Microstructure and properties of Ti–Co–Si ternary intermetallic alloys10.1016/j.jallcom.2007.09.106 ↗
7. Tribological properties of Ti–4Si–xZr–yY2O3/5TiO2 composites prepared by high-energy milling, cold pressing and sintering10.1007/s12541-019-00193-y ↗
8. The BCC/B2 morphologies in AlxNiCoFeCr high-entropy alloys
9. Effect of temperature and pressure on the densification of titanium silicide compound, metals
10. Change in the primary solidification phase from fcc to bcc-based B2 in high entropy or complex concentrated alloys10.1016/j.scriptamat.2016.09.023 ↗
11. Microstructure and wear properties of laser clad TiCo/Ti2Co intermetallic coatings on titanium alloy10.1016/j.apsusc.2004.09.073 ↗
12. The production of nanocrystalline cobalt titanide intermetallic alloy via mechanical alloying10.1016/j.intermet.2012.05.012 ↗
13. Effect of Si addition on the microstructures and mechanical properties of TiAl intermetallics10.4028/www.scientific.net/AMR.239-242.413 ↗
14. Microstructure and compression properties of in situ dual phase nanosized (TiB2–Ti5Si3)/TiAl matrix composites fabricated by combustion synthesis and hot press consolidation10.1179/1743290115Y.0000000010 ↗
15. Characterization and mechanical properties of in situ synthesized Ti5Si3/TiAl composites10.1016/S0921-5093(03)00133-3 ↗
16. Intermetallic 201610.3390/met7100446 ↗
17. Friction and wear behavior of Ti following laser surface alloying with Si, Al and Si+Al10.1016/S0043-1648(00)00363-X ↗
18. Microstructure and tribological properties of laser clad Ti2Ni3Si/NiTi intermetallic coatings10.1016/S1359-6454(03)00465-8 ↗
19. Microstructure and wear resistance of laser clad Ti5Si3/NiTi2 intermetallic composite coating on titanium alloy10.1016/S0921-5093(02)00076-X ↗
20. Westbrook · 2002 · 3
21. Fracture toughness: the role of indentation techniques
22. Sliding wear study on the valve-seat insert contact
23. Consolidation of mechanical alloyed Ti–37.5 at.% Si powder mixture using an electro-discharge technique10.1016/j.msea.2007.02.076 ↗
24. Magnetic and structural properties of SmCo 7− x Ti x magnets10.1016/S0304-8853(01)00451-6 ↗
25. Fabrication of a powder metallurgy Ti2AlNb-based alloy by spark plasma sintering and associated microstructure optimization10.1016/j.matdes.2015.10.042 ↗
26. Influence of mechanical alloying on the microstructure and mechanical properties of powder metallurgy Ti2AlNb-based alloy10.1016/j.powtec.2017.03.034 ↗
27. Thermodynamic aspects of nanostructured Ti5Si3 formation during mechanical alloying and its characterization
28. Formation mechanism of titanium silicide by mechanical alloying10.1023/A:1004816210156 ↗
29. Magnetic properties of mechanically alloyed Co–Ti powder10.1016/S0921-4526(02)00716-0 ↗
30. Spark plasma sintering versus hot pressing–densification, bending strength, microstructure, and tribological properties of Ti5Al2.5Fe alloys10.1080/00325899.2018.1441777 ↗
31. Comparative study of Wear behaviors of a selected titanium alloy and AISI H13 steel as a function of temperature and load10.1080/10402004.2014.916372 ↗
32. Wear behavior of TC11 and AISI M2 in pin–disk tribo-system10.1007/s42243-019-00246-6 ↗