Achieving strength-ductility synergy in nanotwinned steels prepared by cryogenic deformation

Tengfei Jing, Shaodi Dong, Lin Shen, Huabei Peng, Yuhua Wen

Publisher page

Abstract

Nanotwins introduced by cryogenic pre-deformation at the optimum temperature can remarkably improve both strength and ductility. In the present study, the effects of temperature on the tensile properties , stacking faults and mechanical twinning of Fe-17Mn-1.0Si-1.1C steel were systematically investigated to introduce mechanical nanotwins. With decreasing temperature, more stacking faults and thinner mechanical twins are produced in the solution-treated steel; however, the product of strength and ductility of the solution-treated steel is firstly increased and then decreased, achieving the greatest (about 125 GPa ▪ %) at −40°C. For the nanotwinned steel prepared by cryogenic pre-deformation, there exists an optimum pre-deformation temperature for the greatest strength-ductility combination. After introducing mechanical nanotwins at −40°C, the nanotwinned steel obtains the greatest strength-ductility combination of yield strength (1215 MPa), ultimate tensile strength (1521 MPa) and ductility (45.2%).
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and mechanical properties · Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Ultrahigh strength and high electrical conductivity in copper10.1126/science.1092905 ↗
2. Revealing the maximum strength in nanotwinned copper10.1126/science.1167641 ↗
3. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
4. Strengthening an austenitic Fe-Mn steel using nanotwinned austenitic grains10.1016/j.actamat.2012.03.035 ↗
5. Ultra-high tensile strength nanocrystalline CoCrNi equi-atomic medium entropy alloy processed by high-pressure torsion10.1016/j.msea.2018.08.079 ↗
6. Evolution of dislocations and twins in a strong and ductile nanotwinned steel10.1016/j.actamat.2016.03.057 ↗
7. Fracture behavior of heterogeneous nanostructured 316L austenitic stainless steel with nanotwin bundles10.1016/j.actamat.2018.02.065 ↗
8. Microstructural evolution and nanostructure formation in copper during dynamic plastic deformation at cryogenic temperatures10.1016/j.actamat.2007.09.020 ↗
9. Homogeneously introducing more and thinner nanotwins by engineering annealing twin boundaries: a TWIP steel as an example
10. Enhancement of strength-ductility combination in recovery-annealed Fe-Mn-C twinning-induced plasticity steels by Si alloying
11. Nanostructured steel with high work-hardening by the exploitation of the thermal stability of mechanically induced twins10.1016/j.scriptamat.2009.01.004 ↗
12. On the applicability of recovery-annealed twinning-induced plasticity steels: potential and limitations10.1016/j.msea.2015.09.096 ↗
13. Supper strong nanostructured TWIP steels for automotive applications10.1016/j.pnsc.2014.01.004 ↗
14. Tensile properties and deformation mode of Si-added Fe-18Mn-0.6C steels10.1016/j.actamat.2017.11.023 ↗
15. A fracture-resistant high-entropy alloy for cryogenic applications10.1126/science.1254581 ↗
16. Exceptional damage-tolerance of a medium-entropy alloy CrCoNi at cryogenic temperatures10.1038/ncomms10602 ↗
17. Superb cryogenic strength of equiatomic CrCoNi derived from gradient hierarchical microstructure10.1016/j.jmst.2018.12.002 ↗
18. Modulating the prestrain history to optimize strength and ductility in CoCrFeMnNi high-entropy alloy10.1016/j.scriptamat.2019.01.012 ↗
19. Superior cryogenic tensile properties of ultrafine-grained CoCrNi medium-entropy alloy produced by high-pressure torsion and annealing10.1016/j.scriptamat.2019.01.016 ↗
20. Heavily twinned CoCrNi medium-entropy alloy with superior strength and crack resistance10.1016/j.msea.2020.139591 ↗
21. Stacking fault energy and deformation mechanisms in Fe-xMn-0.6C-yAl TWIP steel10.1016/j.msea.2016.08.106 ↗
22. The influence of stacking fault energy on the microstructural and strain-hardening evolution of Fe-Mn-Al-Si steels during tensile deformation10.1016/j.actamat.2015.08.030 ↗
23. On the more persistently-enhanced strain hardening in carbon-increased Fe-Mn-C twinning-induced plasticity steel10.1016/j.msea.2015.05.044 ↗
24. Diffusion of carbon in austenite with a discontinuity in composition
25. The effects of Si on the mechanical twinning and strain hardening of Fe-18Mn-0.6C twinning-induced plasticity steel10.1016/j.actamat.2013.02.031 ↗
26. Simultaneous twinning nucleation mechanisms in an Fe-Mn-Si-Al twinning induced plasticity steel10.1016/j.actamat.2017.04.046 ↗
27. Deformation twinning10.1016/0079-6425(94)00007-7 ↗
28. Effect of stacking faults on the ductility of Fe-18Mn-1.5Al-0.6C twinning-induced plasticity steel at low temperatures10.1016/j.scriptamat.2017.04.037 ↗
29. Remarkable improvement of damping capacity in FeMn-based alloys by a long annealing10.1080/02670836.2020.1780002 ↗
30. Effect of nitrogen on stacking fault formation probability and mechanical properties of twinning-induced plasticity steels10.1007/s11661-007-9434-9 ↗
31. Severe plastic deformation of 6061 aluminum alloy tube with pre and post heat treatments10.1016/j.msea.2012.11.025 ↗
32. Evaluation of the dislocation density and dislocation character in cold rolled type 304 steel determined by profile analysis of X-ray diffraction10.1016/j.actamat.2011.03.055 ↗
33. XRD, microstructural and EPR susceptibility characterization of combustion synthesized nanoscale Mg1−xNixO solid solutions10.1016/j.jpcs.2007.08.006 ↗
34. On the analysis of grain size in bulk nanocrystalline materials via X-ray diffraction10.1007/s11661-003-0246-2 ↗
35. A study of work hardening in austenitic Fe-Mn-C and Fe-Mn-Al-C alloys10.1016/0956-7151(92)90054-I ↗
36. The effect of aluminum on the work hardening and wear resistance of hadfield manganese steel10.1007/BF02646146 ↗
37. High Mn TWIP steels for automotive applications
38. On the mechanisms of different work-hardening stages in twinning-induced plasticity steels10.1007/s11661-015-3100-4 ↗
39. Strain hardening behavior and deformation substructure of Fe-20/27Mn-4Al-0.3C non-magnetic steels10.1016/j.matdes.2015.12.038 ↗
40. Deformation mechanisms during large strain deformation of high Mn TWIP steel10.1016/j.msea.2017.05.039 ↗
41. On the relationship between work hardening and twinning rate in TWIP steels10.1016/j.msea.2012.01.123 ↗
42. Comparison of work hardening and deformation twinning evolution in Fe-22Mn-0.6C-(1.5Al) twinning-induced plasticity steels10.1016/j.scriptamat.2013.02.060 ↗
43. Twinning-induced plasticity (TWIP) steels10.1016/j.actamat.2017.06.046 ↗
44. Newer insights into the discrimination of pole mechanisms of twinning in a face-centered cubic high-Mn steel
45. Effect of carbon content on the mechanical properties and microstructural evolution of Fe-22Mn-C steels10.1016/j.msea.2014.10.042 ↗
46. Real-time nanoscale observation of deformation mechanisms in CrCoNi-based medium- to high-entropy alloys at cryogenic temperatures10.1016/j.mattod.2019.03.001 ↗
47. Tensile fracture modes in Fe-22Mn-0.6C and Fe-30Mn-3Si-3Al twinning-induced plasticity (TWIP) steels10.1007/s11661-017-4263-y ↗
48. High strength Fe±Mn±(Al, Si) TRIP/TWIP steels development- properties- application10.1016/S0749-6419(00)00015-2 ↗
49. Partially-recrystallized, Nb-alloyed TWIP steels with a superior strength-ductility balance10.1016/j.msea.2017.11.012 ↗
50. Precipitation hardening of a FeMnC TWIP steel by vanadium carbides10.1088/1742-6596/240/1/012023 ↗
51. Influence of annealing temperature on mechanical properties and microstructures of a high manganese austenitic steel10.1016/j.jmatprotec.2014.11.027 ↗
52. The effect of thermo-mechanical treatment and adding niobium and titanium on microstructure and mechanical properties of TWIP steel10.7763/IJAPM.2011.V1.38 ↗
53. The simultaneous improvement of strength and plasticity of a novel alloying steel by precipitation recovery annealing10.1016/j.matlet.2020.127710 ↗
54. Precipitation strengthening in high manganese austenitic TWIP steels10.3139/146.110508 ↗
55. Microstructure evolution and strengthening mechanisms of Fe-23Mn-0.3C-1.5Al TWIP steel during cold rolling10.1016/j.msea.2014.08.051 ↗
56. High manganese austenitic twinning induced plasticity steels: a review of the microstructure properties relationships10.1016/j.cossms.2011.04.002 ↗
57. Mechanical behaviors of a lower-Mn-added Fe-11Mn-10Al-1.25C lightweight steel with distinguished microstructural features10.1016/j.matlet.2019.01.115 ↗
58. Effects of annealing temperature on the microstructure and properties of the 25Mn-3Si-3Al TWIP steel10.1016/S1674-4799(09)60026-1 ↗
59. Effects of alloying addition on deformation mechanisms, microstructure, texture and mechanical properties in Fe-12Mn-0.5C austenitic steel10.1016/j.msea.2018.05.071 ↗
60. Thermodynamic calculation of stacking fault energy of the Fe-Mn-Si-C high manganese steels10.1016/j.msea.2014.01.046 ↗
61. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe-Mn-C alloys10.1016/j.msea.2004.01.059 ↗
62. The effect of grain size and grain orientation on deformation twinning in a Fe-22wt.% Mn-0.6wt.% C TWIP steel10.1016/j.msea.2010.02.041 ↗
63. On the stress dependence of partial dislocation separation and deformation microstructure in austenitic stainless steels10.1016/S1359-6454(03)00117-4 ↗
64. Effect of Al on the stacking fault energy of Fe-18Mn-0.6C twinning-induced plasticity10.1016/j.scriptamat.2011.05.014 ↗
65. Equivalent twinning criteria for FCC alloys under uniaxial tension at high temperatures10.1016/j.msea.2006.12.113 ↗
66. Tensile deformation behavior of high manganese austenitic steel: the role of grain size10.1016/j.matdes.2010.01.049 ↗
67. Micromechanics of twinning in a TWIP steel10.1016/j.msea.2015.03.082 ↗
68. Kinetics of f.c.c. deformation twinning and its relationship to stress-strain behaviour10.1016/0001-6160(78)90170-0 ↗
69. Modelling of TWIP effect on work-hardening10.1016/S0921-5093(00)02019-0 ↗
70. The influence of aluminum on hot deformation behavior and tensile properties of high-Mn TWIP steels10.1016/j.msea.2007.02.074 ↗
71. The effect of Al on mechanical properties and microstructures of Fe-32Mn-12Cr-xAl-0.4C cryogenic alloys10.1016/S0921-5093(96)10501-3 ↗
72. Dependence of tensile deformation behavior of TWIP steels on stacking fault energy, temperature and strain rate10.1016/j.actamat.2010.05.049 ↗
73. Review on superior strength and enhanced ductility of metallic nanomaterials10.1016/j.pmatsci.2018.02.002 ↗