High-temperature fatigue investigation of SS316L fabricated via laser wire-directed energy deposition

Ritam Pal, Ajay Kushwaha, Kun-Hao Huang, Amrita Basak

Publisher page

Abstract

Additive manufacturing (AM) techniques offer opportunities to fabricate structural components with complex geometries in automobile, maritime, and other industries, where the components may undergo dynamic loadings at elevated temperatures. Stainless steel 316L (SS316L) is a popular material in these industries because of its high toughness and ductility. It possesses excellent weldability, making it suitable for AM fabrication techniques such as laser-powder bed fusion (L-PBF) and directed energy deposition (DED). DED provides numerous advantages over L-PBF like low material waste, less fabrication time, and the presence of commercial-ready feedstock. Although low cycle fatigue (LCF) investigations of L-PBF SS316L specimens at elevated temperatures have been reported, there is a lack of understanding of the high-temperature LCF behavior of SS316L fabricated via laser wire-directed energy deposition (LW-DED). This work addresses this research gap by performing LCF investigations of LW-DED SS316L specimens at elevated temperatures. The specimens are fabricated in a MELTIO M450 system with system-specific parameters. Computed tomography (CT) is then employed to characterize the fabricated specimens, showing that the maximum porosity area is 1.3 %, and lack-of-fusion pores are dominant over gas pores in the specimens. The fatigue investigation includes four different temperatures and two strain ranges at reversed loading conditions. Besides total fatigue life, initiation lives are obtained by compliance evaluation from the load-displacement data. It is observed that the fatigue life decreases with the increase in temperature and strain range, and the initiation life is proportional to the fatigue life. The fractography analysis presents unconventional fractured surfaces where the initiation zone is found in the interior of the specimens. CT and electron back-scattered diffraction analysis further confirm that these unconventional fractured surfaces are due to lack-of-fusion pores. In summary, compared to wrought specimens, coarse columnar microstructures and lack-of-fusion pores originating from the printing process are found to deteriorate the fatigue life of LW-DED SS316L specimens.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Joining of different thickness dissimilar materials SS 316L/SS 310 by μ-PAW process
2. Structural assessment of printed circuit heat exchangers in supercritical CO2 waste heat recovery Systems for Ship Applications10.1007/s11630-022-1493-0 ↗
3. Tribological investigation of HVOF sprayed Ni-based coatings on SS 316L in water-cooled nuclear reactor10.1016/j.matpr.2022.02.210 ↗
4. High ductility and corrosion resistance chromium gradient stainless steel for fuel cell bipolar plates fabricated via laser powder bed fusion10.1016/j.jmatprotec.2023.118002 ↗
5. A study on the effect of test temperatures on tensile and fracture behavior of SS 316LN10.1520/MPC20210086 ↗
6. Microstructure and mechanical properties of welded additively manufactured stainless steels SS316L10.1007/s12540-019-00264-9 ↗
7. A critical review of fatigue life prediction on 316LN SS
8. Scale and shape effects on the fatigue behaviour of additively manufactured SS316L structures: A preliminary study
9. Studying the effect of thermal fatigue on multiple cracks propagating in an SS316L thin flange on a shaft specimen using a multi-physics numerical simulation model10.5545/sv-jme.2019.6073 ↗
10. Goswami · 2001
11. Effect of temperature on the fatigue crack growth behaviour of SS316L(N)10.1016/j.ijfatigue.2020.105815 ↗
12. Experimental and numerical creep-fatigue study of type 316 stainless steel failure under high temperature LCF loading condition with different hold time10.1016/j.engfracmech.2015.05.007 ↗
13. Goswami · 1999
14. Ngo · 2018
15. Tensile properties of SS316L produced by LPBF: influence of specimen dimensions and surface condition10.1016/j.matchar.2023.113117 ↗
16. Microstructural and mechanical evaluation of post-processed SS 316L manufactured by laser-based powder bed fusion10.1016/j.jmrt.2021.02.090 ↗
17. Analysis of the effect of surface morphology on tensile behavior of LPBF SS316L microstruts10.1016/j.msea.2021.142226 ↗
18. Process optimization for directed energy deposition of SS316L components10.1007/s00170-020-06113-z ↗
19. Prediction of mechanical behaviors of L-DED fabricated SS 316L parts via machine learning10.1007/s00170-022-09509-1 ↗
20. Parametric investigation and characterization on SS316 built by laser-assisted directed energy deposition
21. Low cycle fatigue of additively manufactured thin-walled stainless steel 316L10.1016/j.msea.2021.141598 ↗
22. The influence of surface finish and build orientation on the low cycle fatigue behaviour of laser powder bed fused stainless steel 316L10.1016/j.msea.2023.144593 ↗
23. The influence of energy density on the low cycle fatigue behaviour of laser powder bed fused stainless steel 316L10.1016/j.ijfatigue.2023.108123 ↗
24. Svetlizky · 2021
25. Laser Shock Peening of Laser Based Directed Energy Deposition and Powder Bed Fusion Additively Manufactured Parts: A Review10.1007/s12540-022-01334-1 ↗
26. Process-influenced fatigue behavior of AISI 316L manufactured by powder- and wire-based laser direct energy deposition10.1016/j.msea.2021.141383 ↗
27. Influence of cellular subgrain feature on mechanical deformation and properties of directed energy deposited stainless steel 316 L
28. Kersten · 2020 · 730
29. Mechanical and microstructural properties of laser direct energy deposited 15–5 PH and SS 316L stainless steel10.1016/j.matpr.2022.06.249 ↗
30. Tensile properties of built and rebuilt/repaired specimens of 316L stainless steel using directed energy deposition10.1007/s11665-020-05087-z ↗
31. An investigation of the microstructure and fatigue behavior of additively manufactured AISI 316L stainless steel with regard to the influence of heat treatment10.3390/met8040220 ↗
32. Thompson · 2015
33. Defect distribution and microstructure heterogeneity effects on fracture resistance and fatigue behavior of EBM Ti–6Al–4V10.1016/j.ijfatigue.2016.06.001 ↗
34. Low cycle fatigue, deformation and fracture behaviour of Inconel 617 alloy10.1016/j.msea.2019.138286 ↗
35. Cowles · 1996
36. Lawton · 1968
37. Chen
38. Low cycle fatigue behavior of additive manufactured 316LN stainless steel at 550 °C: effect of solution heat treatment10.1016/j.ijfatigue.2023.108066 ↗
39. Evaluating deposits of SS316L powder and wire consolidated using co-axial laser directed energy deposition10.1007/s00170-024-13243-1 ↗
40. Guide
41. Fatigue life prediction of rough Hastelloy X specimens fabricated using laser powder bed fusion
42. Pop-in fracture: observations on load drop, displacement increase, and crack advance10.1007/BF00035042 ↗
43. 2017
44. Yi · 2024
45. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
46. Azarniya · 2019
47. Bernard · 2023
48. A data-driven approach for predicting printability in metal additive manufacturing processes10.1007/s10845-020-01541-w ↗
49. High cycle fatigue behavior of 316L steel fabricated by laser powder bed fusion: effects of surface defect and loading mode10.1016/j.ijfatigue.2022.106843 ↗
50. Comparative assessment of strain-controlled fatigue performance of SS 316L at room and low temperatures10.1016/j.ijfatigue.2022.107251 ↗
51. Microstructure mechanism, cyclic deformation behavior of an Fe-Ni-Cr alloy considering non-Masing behavior10.1016/j.ijfatigue.2019.06.035 ↗
52. Quantitative assessment and analysis of non-Masing behavior of materials under fatigue10.1007/s11665-021-05494-w ↗
53. Experimental and numerical study on the fatigue behaviour of pre and post heat treated additively manufactured SS 316L specimens10.1016/j.engfailanal.2024.108605 ↗
54. Wang · 2025
55. Effect of build height on the properties of large format stainless steel 316L fabricated via directed energy deposition
56. Thermal behavior and microstructural evolution during laser deposition with laser-engineered net shaping: part I. Numerical calculations10.1007/s11661-008-9557-7 ↗
57. A study of low cycle fatigue life and its correlation with microstructural parameters in IN713C nickel based superalloy10.1016/j.msea.2018.01.083 ↗
58. Grain size manipulation by wire laser direct energy deposition of 316L with ultrasonic assistance10.2351/7.0001090 ↗