journal article·2025-07Open access

The precipitation of Ni₃Al reducing the corrosion resistance of alumina-forming austenitic (AFA) steels exposed to 600 °C lead‑bismuth eutectic (LBE) with 10−8 wt% oxygen

Decang Zhang, Xiaoxin Zhang, Xian Zeng, Fanao Meng, Chenxi Zhu, Qingzhi Yan

Abstract

This study investigated the corrosion behavior of two AFA steels (Fe-24Ni-15Cr wt%) with 3Al and 4Al, exposed LBE containing 10 −8 wt% oxygen at 600 °C. Unexpectedly, the 4Al steel exhibited much more severe corrosion than the 3Al steel. To explore the anomalous relationship between Al content and corrosion resistance, validation experiments were conducted using advanced high-resolution characterization techniques. The higher Al concentration in the 4Al steel promotes the early precipitation of Ni 3 Al. These Ni 3 Al nanoprecipitates undergo in-situ internal oxidation, forming alumina nanoparticles that inhibit the formation of external protective alumina scales and thereby result in extensive dissolution attack.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Advanced ceramic materials synthesis · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. New insights into selective leaching and ferritization in 15-15Ti austenitic steel in lead-bismuth eutectic through parent phase reconstruction10.1016/j.scriptamat.2024.116316 ↗
2. Twin boundary-accelerated ferritization of austenitic stainless steels in liquid lead–bismuth eutectic10.1016/j.scriptamat.2016.02.029 ↗
3. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors10.1016/j.pmatsci.2022.100920 ↗
4. Creep-resistant, Al₂O₃-forming austenitic stainless steels10.1126/science.1137711 ↗
5. Overview of strategies for high-temperature creep and oxidation resistance of alumina-forming austenitic stainless steels10.1007/s11661-010-0295-2 ↗
6. Effect of variation in oxygen concentration in static Pb-bi eutectic on long-term corrosion performance of Al-alloyed austenitic steels at 500°C10.1016/j.corsci.2021.109963 ↗
7. Dissolution and oxidation behaviour of various austenitic steels and Ni rich alloys in lead-bismuth eutectic at 520°C10.1016/j.jnucmat.2015.11.005 ↗
8. Long term corrosion resistance of alumina forming austenitic stainless steels in liquid lead10.1016/j.jnucmat.2015.03.011 ↗
9. Fe-14Ni-14Cr-2.5Al steel showing excellent corrosion-resistance in flowing LBE at 550°C and high temperature strength10.1016/j.jnucmat.2023.154703 ↗
10. The influence of Y and Nb addition on the corrosion resistance of Fe-Cr-Al-Ni model alloys exposed to oxygen-containing molten Pb10.1016/j.corsci.2020.109152 ↗
11. Corrosion behaviour of Al-added high Mn austenitic steels in molten lead bismuth eutectic with saturated and low oxygen concentrations at 450°C10.1016/j.corsci.2020.108864 ↗
12. Effect of aluminium addition on the oxidation and carburization behaviour of austenitic stainless in high-temperature SCO2 environments10.1016/j.corsci.2023.111666 ↗
13. High-resolution characterization reveals the role of Al content in the evolution of oxide scales formed on alumina-forming alloy exposed to supercritical water10.1016/j.corsci.2024.111968 ↗
14. Microstructures, tensile properties and corrosion behaviors of Fe20Cr25NiNb stainless steels with different Al contents in supercritical carbon dioxide10.1016/j.jmrt.2023.02.224 ↗
15. Corrosion resistance and microstructural stability of austenitic Fe-Cr-Al-Ni model alloys exposed to oxygen-containing molten lead10.1016/j.jnucmat.2019.06.043 ↗
16. Nano-scale evidence for coupled interfacial dissolution-reprecipitation (CDR) controlling corrosion of alumina-forming austenitic (AFA) steel in static lead-bismuth eutectic (LBE) at 600°C10.1016/j.corsci.2024.112597 ↗
17. High-resolution characterization revealing the effect of dissolved oxygen in lead-bismuth eutectic (LBE) on oxide scale and subsurface phase transformation layer in alumina-forming austenitic (AFA) steel10.1016/j.corsci.2024.112671 ↗
18. Anomalous oxidation rate-temperature dependence of alumina-forming austenitic stainless steels exposed to 500-600°C supercritical water10.1016/j.corsci.2024.111936 ↗
19. New insights into the initial oxidation behavior of an ultra-corrosion resistant alumina-forming austenitic steel in supercritical carbon dioxide: the effects of precipitated intragranular intermetallic compounds10.1016/j.corsci.2023.111260 ↗
20. Barrier effect of intergranular precipitation in alumina-forming austenitic steel against dissolution corrosion exposed to lead-bismuth eutectic10.1016/j.corsci.2024.112643 ↗
21. Synergistic inhibition to dissolution corrosion by de-twinning and precipitation in alumina-forming austenitic steel exposed to lead-bismuth eutectic with 10−8 wt.% oxygen at 600°C10.1016/j.jmst.2024.10.009 ↗
22. Precipitation sequence and its effect on age hardening of alumina-forming austenitic stainless steel10.1016/j.msea.2015.08.005 ↗
23. Effect of oxygen on corrosion of an alumina-forming duplex steel in static liquid lead-bismuth eutectic at 550°C10.1016/j.corsci.2021.109591 ↗
24. Intergranular precipitation-enhanced wetting and phase transformation in an Al0.4CoCrFeNi high-entropy alloy exposed to lead-bismuth eutectic10.1016/j.corsci.2021.110038 ↗
25. Effect of silicon on the formation of protective scale on Fe-10Ni-10Cr-4Al alloy pre-oxidized at low oxygen pressure
26. M23C6 precipitates induced inhomogeneous distribution of silicon in the oxide formed on a high-silicon ferritic/martensitic steel10.1016/j.scriptamat.2014.10.028 ↗
27. Oxidation of multicomponent two-phase alloys10.1007/BF01046728 ↗
28. An approximate analysis of the external oxidation of ternary alloys forming insoluble oxides. II: low oxidant pressures10.1023/A:1012549601688 ↗
29. The oxidation of two Fe-Nb alloys under low oxygen pressures at 600-800°C10.1007/BF01046899 ↗
30. Composition, microstructure, and water vapor effects on internal/external oxidation of alumina-forming austenitic stainless steels10.1007/s11085-009-9161-2 ↗