Unexpected thermal aging effect on brittle fracture and elemental segregation in modern dissimilar metal weld

Andrea Fazi, Pedro A. Ferreirós, Yanling Ge, Song Lu, Mattias Thuvander, Zaiqing Que

Abstract

A full-scale dissimilar metal weld safe-end mock-up, precisely replicating a critical component of a modern nuclear power plant, was investigated. The brittle fracture behavior, carbide evolution and nanoscale elemental segregation in the heat-affected zone (HAZ) of low alloy steel (LAS) were analyzed under both post-weld heat-treated and thermally-aged conditions (400 °C for 15,000 h, equivalent to 90 years of operation) using analytical electron microscopy and atom probe tomography. The observed increase in grain boundary (GB) decohesion and intergranular cracking on the fracture surface and the decrease of fracture toughness are primarily attributed to P and Mn segregation to GBs and the coarsening of carbides upon long-term thermal aging. The direct observations of significant elemental segregation to GBs and the consequent reduction in fracture toughness in the HAZ are unexpected for modern low-phosphorus LASs, highlighting potential concerns for evaluating the structural integrity of modern nuclear power plants. • Effect of long-term thermal aging (400 °C for 15,000 h) on modern low-P DMW. • Detailed microstructure studies with STEM, TKD and APT. • Thermal aging induces nanoscale P and Mn segregation and carbide coarsening. • Aging unexpectedly results in IG cracking and low fracture toughness in low-P LAS.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Microstructure and Mechanical Properties of Steels · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (53)

Show source-provided references
1. Thermal ageing and mechanical performance of narrow-gap dissimilar metal welds
2. Microstructure and stress corrosion cracking behaviour of the weld metal in alloy 52-A508 dissimilar welds10.2320/matertrans.M2010294 ↗
3. Microstructural and mechanical investigation of the near fusion boundary region in thermally aged 18MND5 / alloy 52 narrow-gap dissimilar metal weld
4. TEM observation of Martensite layer at the weld Interface of an A508III to Inconel 82 dissimilar metal weld joint10.1007/s11661-015-3171-2 ↗
5. Effect of thermal ageing at 400°C on the microstructure of ferrite-austenite interface of nickel-base alloy narrow-gap dissimilar metal weld10.3390/met10030421 ↗
6. Characterisation of microstructures in nickel based transition joints10.1023/A:1004846607046 ↗
7. Microstructure and mechanical property of the fusion boundary region in an alloy 182-low alloy steel dissimilar weld joint10.1007/s10853-010-4581-6 ↗
8. Root cause failure analysis of defected J-groove welds in steam generator drainage nozzles
9. Structural assessment of defected nozzle to safe-end welds in Ringhals-3 and -4
10. Analysis of a defected dissimilar metal weld in a PWR power plant
11. Brittle fracture initiation in decommissioned boiling water reactor pressure vessel head weld
12. Microstructural evolution and corrosion behaviour of thermally aged dissimilar metal welds of low-alloy steel and nickel-based alloy10.1016/j.corsci.2019.03.032 ↗
13. Role of welding residual strain and ductility dip cracking on corrosion fatigue behavior of alloy 52/52M dissimilar metal weld in borated and lithiated high-temperature water10.1016/j.jmst.2019.10.012 ↗
14. In situ Raman spectroscopic analysis of surface oxide films on Ni-base alloy/low alloy steel dissimilar metal weld interfaces in high-temperature water10.1016/j.jnucmat.2014.03.038 ↗
15. Fracture toughness in the ductile-brittle transition and thermal ageing behavior of decarburized heat affected zone of Alloy 52 dissimilar metal welds of nuclear components
16. The effect of thermal aging on fracture properties of a narrow-gap alloy 52 dissimilar metal weld
17. Fracture in the Ductile-To-Brittle Transition Region of A Narrow-Gap Alloy 52 and Alloy 52 Dissimilar Metal Weld With Buttering
18. Mouginot · 2017
19. Fracture mechanism of a dissimilar metal welded joint in nuclear power plant10.1016/j.engfailanal.2012.10.005 ↗
20. Que · 2023
21. Fusion Boundary Microstructure and Fracture Behaviour of a narrow-gap Alloy 52 Dissimilar Metal Weld and an Alloy 52 Dissimilar Metal Weld and an Alloy 52 Dissimilar Metal Weld with Buttering
22. Local mechanical properties of a dissimilar metal welded joint in nuclear power systems10.1016/j.msea.2013.01.037 ↗
23. Effects of thermal aging on the microstructure of type-II boundaries in dissimilar metal weld joints10.1016/j.jnucmat.2015.01.009 ↗
24. Brittle fracture analysis of dissimilar metal welds10.1016/j.engfracmech.2014.07.005 ↗
25. Effect of microstructure on mechanical behavior of Ni-base Alloy Dissimilar Metal Welds
26. Study of fusion boundary microstructure and local mismatch of SA508/alloy 52 dissimilar metal weld
27. Effect of thermal aging on microstructure and carbides of SA508/alloy 52 dissimilar metal weld
28. Investigation of solute segregation behavior using a correlative EBSD/TKD/APT methodology in a 16MND5 weld10.1016/j.jnucmat.2019.06.002 ↗
29. Quantitative atom probe analysis of carbides10.1016/j.ultramic.2010.12.024 ↗
30. In situ site-specific specimen preparation for atom probe tomography10.1016/j.ultramic.2006.06.008 ↗
31. The disconnection mechanism of coupled migration and shear at grain boundaries10.1016/j.actamat.2012.01.001 ↗
32. Thermal ageing effect on solute segregation and precipitation in the heat-affected-zone of dissimilar metal welds for nuclear power plants
33. Measurement of the Gibbsian interfacial excess of solute at an interface of arbitrary geometry using three-dimensional atom probe microscopy10.1016/S0921-5093(01)01885-8 ↗
34. Texture, grain boundary characterization and segregation of phosphorus in an annealed interstitial free steel10.1016/S1006-706X(14)60151-5 ↗
35. The distribution of substitutional alloying elements during the bainite transformation10.1007/BF02656567 ↗
36. Grain boundary segregation engineering and austenite reversion turn embrittlement into toughness: example of a 9 wt.% medium Mn steel10.1016/j.actamat.2014.12.021 ↗
37. On the effect of nickel substitution in duplex stainless steel10.1179/174328408X276116 ↗
38. Influence of the thermodynamic parameters on the temper embrittlement of SA508 Gr.4N Ni–Cr–Mo low alloy steel with variation of Ni, Cr and Mn contents
39. Influence of Mn on kinetics of P segregation in low-alloy steel10.1179/030634582790427550 ↗
40. Tracer diffusion of P in Iron and Iron alloys10.2320/matertrans1960.24.589 ↗
41. Grain boundary segregation of impurities in iron and steels and effects on steel properties
42. Study on the segregation behavior in SA508 Gr. 4N low alloy steel
43. Effects of thermal history and microstructure on segregation of phosphorus and alloying elements in the heat-affected zone of a low alloy steel10.1007/s11661-014-2582-9 ↗
44. Competitive grain boundary segregation of phosphorus and carbon governs delamination crack in a ferritic steel10.1016/j.matchar.2018.08.060 ↗
45. Equilibrium segregation in a ternary solution: a model for temper embrittlement10.1016/0039-6028(75)90125-9 ↗
46. The thermodynamics of interactive co-segregation of phosphorus and alloying elements in iron and temper-brittle steels10.1007/BF02647825 ↗
47. Role of molybdenum in phosphorus-induced temper embrittlement10.1179/030634580790438163 ↗
48. First-principles study on the P-induced embrittlement and de-embrittling effect of B and C in ferritic steels
49. Phosphorus and transition metal co-segregation in ferritic iron grain boundaries and its effects on cohesion
50. First-principles calculations on co-segregation of p and transition metal elements at fe grain boundaries
51. Effect of carbon on the grain boundary segregation of phosphorus in α-iron10.1016/0036-9748(83)90225-9 ↗
52. Aluminum depletion induced by co-segregation of carbon and boron in a bcc-iron grain boundary
53. Fracture mechanical characterisation of ferrite-austenite dissimilar metal welds (DMWs) for elevated temperature service in view of metallurgical mismatch