journal article·2005-07

Microstructural analysis of a single pass 2.25% Cr–1.0% Mo steel weld metal with different manganese contents

Luís Felipe Guimarães de Souza, Ivaní de Souza Bott, Jorge Carlos Ferreira Jorge, Ari Sauer Guimarães, Ronaldo Pinheiro Rocha Paranhos

Materials Characterization· Volume 55· Issue 1
Publisher page

Abstract

Abstract Weld metals of the 2.25% Cr–1.0% Mo type with 0.84%, 1.21% and 2.3% Mn produced by submerged-arc welding were analyzed in the as-welded (AW), post weld heat treatment (PWHT) and PWHT followed by step-cooling (SC) heat treatment conditions. Fracture surface analysis revealed an evolution in the mode of fracture due to Mn content variations and heat treatment conditions, the occurrence of intergranular fracture being observed in welds with 2.30% Mn that were step-cooled. Transmission electron microscopy revealed that the microstructure was predominantly composed of bainite, although martensite was also observed for high Mn contents. A marked carbide precipitation was observed, preferentially at grain boundaries. This could be attributed to the SC heat treatment and associated with the embrittlement. However, the application of a de-embrittlement heat treatment to this step cooled weld metal has proved efficient, because the impact energy levels after this heat treatment surpassed those obtained in the stress relieved condition. This indicates that segregation of impurities to grain boundaries was responsible for the low impact energy levels observed after SC of weld metal containing > 0.84% Mn.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. 1990 · vol. 1 · 617
2. Sèferian · 1962
3. Temper embrittlement of 2,25 Cr–1 Mo steel weld metal–a literature survey
4. Alloy and impurity effects on temper brittleness of steel
5. Temper embrittlement characteristics of 2 1/4 Cr–1 Mo steels10.2355/isijinternational1966.22.434 ↗
6. On kinetics of phosphorus segregation in Cr–Mo–V low alloy steel10.1016/0956-716X(94)90462-6 ↗
7. Prevention of temper embrittlement in 2 1/4 Cr–1 Mo weld metal by metallurgical actions
8. Fragilización del revenido en metal de aceros 2,25 Cr–1 Mo
9. Effects of Mn, Si and purity on the design of 3.5 Ni CrMoV, 1 CrMoV and 2.25 Cr–1.0 Mo bainitic alloy steels
10. Temper embrittlement10.1179/095066078790136661 ↗
11. A review on reversible temper embrittlement in Cr–Mo steel weld metals
12. Influence of long-term ageing and superimposed creep stress on the microstructure of 2.25% Cr–1 Mo steel10.1007/BF02657318 ↗
13. The effects of phosphorus on the temper embrittlement susceptibility of 2 1/4 Cr–1 Mo steel
14. Metallurgical aspects in welding Cr–Mo–V turbine rotor steels: Part 1. Evaluation of base material and heat affected zone10.1179/mst.1991.7.1.42 ↗
15. Metallurgical aspects in welding Cr–Mo–V turbine rotor steels: Part 2. Evaluation of narrow gap submerged arc weldment10.1179/mst.1991.7.2.147 ↗
16. Teixeira, Uma Avaliação da Fragilização ao Revenido de Metais de Solda de Aços 2,25Cr–1Mo
17. Failure analysis of a service-exposed hot reheated steam line in a utility steam plant
18. Temper embrittlement and creep embrittlement of 2 1/4 Cr–1 Mo shielded metal arc weld deposits