Creep failure of cracking heater at a petrochemical plant

A. El-Batahgy, B. Zaghloul

Materials Characterization· Volume 54· Issue 3
Publisher page

Abstract

After two and half years of operation, a bend tube in a cracking heater at an ethylene plant failed due to creep cracking. Creep damage occurred as a result of metallurgical instability including coarsening of carbides that caused softening and initiation of voids or wedge-type intergranular cracks. This was accelerated due to increasing inner surface temperature during decoking process. Thermal fatigue contributed to the failure as a result of temperature variations due to several shutdown-startup operations. To minimize such failure in futures, periodic inspection to monitor crack formation was scheduled. Nondestructive tests including dye penetrant test for surface cracking and radiographic test for internal crack were implemented.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Mechanical Failure Analysis and Simulation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. Barer · 1991
2. 1996
3. Colangelo · 1987
4. Brooks · 1993
5. Fontana · 1987
6. Degradation of Nimonic 80A due to high temperature creep deformation
7. Grain boundary precipitation strengthening due to carbides in high temperature creep of inconel 617
8. Failure of gas turbine duct at a power generating plant