Recrystallization behavior of a co-cast AA3xxx–AA6xxx aluminum alloy laminate — Effect of annealing conditions and cold reduction levels
Source abstract
Abstract
Abstract The annealing behavior of a laminated AA3xxx–AA6xxx alloy system is investigated at temperatures and conditions which represent fine particle presence or dissolution in the AA6xxx (i.e. core) layer, as well as 60 or 80% cold reduction levels. The through-thickness microstructural characteristics of the cold rolled and annealed laminates are analyzed using various methods. It is found that the average grain size of the AA3xxx (i.e. clad) layer is generally finer than that of the core layer and the grains are more equiaxed in that layer for all conditions studied. The annealed microstructure of the core layer is also more strongly affected by the change in the annealing conditions. The dependencies of the average grain size and grain size aspect ratio on the annealing conditions are dictated by the presence, size, distribution and thermal stability of particles. A higher level of cold reduction results in reversing the trend of change in the grain size aspect ratios of both layers with annealing temperature in the range of 380 to 420 °C (1 h), while it yields characteristics similar to that obtained by 60% reduction when annealing is conducted for 30 s at 540 °C. These results are explained through the microstructural evolution parameters that are affected by cold rolling and annealing conditions.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Direct chill casting of aluminium–manganese against aluminium–silicon layer via Novelis Fusion process10.1179/175355507X214069 ↗
2. The deformation of clad aluminum sheet produced by direct chill casting10.1007/s11661-010-0298-z ↗
3. The distribution of magnesium and silicon across the as-cast interface of aluminum laminates produced via the Novelis Fusion™ process10.1007/s11837-007-0107-3 ↗
4. Enhanced ductility in sheet metals produced by cladding a ductile layer10.1115/1.4000926 ↗
5. Humphreys · 2004
6. Influence of particles on recrystallisation textures and microstructures of aluminium alloy 310310.1179/mst.1997.13.2.93 ↗
7. Current issues in recrystallization: a review10.1016/S0921-5093(97)00424-3 ↗
8. The effect of coarse non-deformable particles on the deformation and static recrystallization of aluminium alloys10.1080/14786430410001689990 ↗
9. The effect of finely dispersed particles on primary recrystallisation textures in AlMnSi alloys10.1016/S0921-5093(96)10571-2 ↗
10. Correlation between electrical resistivity, particle dissolution, precipitation of dispersoids, and recrystallization behavior of AA7020 aluminum alloy10.1007/s11661-009-9917-y ↗
11. Comparison of recrystallization and recrystallization textures in cold-rolled DC and CC AA 5182 aluminum alloys10.1016/S0921-5093(03)00264-8 ↗
12. Interactions between precipitation and recrystallisation in an Al–Mg–Si alloy10.1179/026708300101507037 ↗
13. The effect of particles on recrystallisation textures and microstructures10.1155/TSM.26-27.385 ↗
14. Particle-stimulated nucleation of recrystallization for grain-size control and superplasticity in an Al–Mg–Si–Cu alloy10.1016/S0921-5093(00)01235-1 ↗
15. On the Zener10.1016/0001-6160(85)90214-7 ↗
16. The effect of particle size and spacing on the retardation of recrystallization in two-phase copper crystals10.1007/BF00752135 ↗
17. The effect of solutes on grain boundary mobility during recrystallization and grain growth in some single-phase aluminium alloys10.1016/j.matchemphys.2011.11.018 ↗
18. Recrystallization behavior of a supersaturated Al–Mn alloy10.1016/j.matlet.2010.05.046 ↗
19. Recrystallization of a supersaturated Al–Mn alloy10.1016/j.scriptamat.2008.05.016 ↗
20. Effect of concurrent precipitation on recrystallization and evolution of the P-texture component in a commercial Al–Mn alloy10.1007/s11661-010-0265-8 ↗
21. Effect of cold work and non-isothermal annealing on the recrystallization behavior and texture evolution of a precipitation-hardenable aluminum alloy10.1016/j.scriptamat.2010.08.014 ↗
22. Interaction between precipitation and annealing phenomena during non-isothermal processing of an AA6xxx alloy
23. Modeling of solutionizing and solute redistribution in a co-cast bi-layer al alloy system10.1007/s11661-011-1068-2 ↗
24. Sepehrband · 2010
25. Newby · 1985
26. Liao · 2013
27. Texture control by thermomechanical processing of AA6xxx Al–Mg–Si sheet alloys for automotive applications—a review10.1016/S0921-5093(01)01968-2 ↗
28. Solid-state intermetallic phase tranformations in 3XXX aluminium alloys10.1016/S1359-6454(02)00085-X ↗
29. Microstructural path of recrystallization in a commercial Al–Mn–Fe–Si (AA3003) alloy10.1590/S1516-14392003000400030 ↗
30. Thermo-mechanical processing of an Al–Mg–Si–Cu alloy10.1016/S1359-6462(98)00045-1 ↗
31. Dispersoid formation and recrystallization behavior in an Al–Mg–Si–Mn alloy10.1016/S1005-0302(10)60040-0 ↗
32. Effect of particles on microstructural evolution during cold rolling of the aluminum alloy AA310410.1016/j.jallcom.2009.03.183 ↗
33. Engler · 2009
34. The role of particle distribution in recrystallization in two-phase alloys10.1016/0025-5416(88)90418-1 ↗
35. Recrystallisation behaviour of supersaturated Al–Mn alloys Part 1 — Al–1.3wt.% Mn10.1179/026708303225008626 ↗
36. Formation of recrystallization texture with rolling orientation in Al–1.3%Mn alloy
37. Changes in microstructures during annealing after cold-rolling at 30% and 50% reduction on Al–Mg–Si alloy10.2320/matertrans.L-MZ201122 ↗
38. Frank · 1978