Abstract

Abstract The microstructure evolution and mechanical properties of the compressively deformed AgInCd alloy during annealing treatment have been investigated in the present study. In the deformed AgInCd alloy, many deformation markings are formed and these deformation markings are mainly composed of nanoscale deformation twins. The AgInCd alloy exhibits a significant work hardening capability because of the formation of deformation twins. The recrystallization temperature of the deformed AgInCd alloy is between 300 °C and 350 °C. In the AgInCd alloy annealed at 300 °C, the deformation twins are eliminated and a large number of dark strips consisting of stacking faults are presented in the un-recrystallized regions, indicating that the deformation twins are transformed into stacking faults by the detwinning mechanism. The annealing twins show higher thermal stability than the deformation twins. The strength and microhardness of the deformed AgInCd alloy gradually decrease with the increase of annealing temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Experiments on silver–indium–cadmium control rod failure during severe nuclear accidents10.1016/j.anucene.2016.11.039 ↗
2. Design, construction and simulation of a multipurpose system for precision movement of control rods in nuclear reactors10.1016/j.anucene.2010.07.017 ↗
3. Microstructure and creep mechanism of the Ag–In–Cd alloy under compressive load at 300–400 °C10.1016/j.matdes.2014.09.048 ↗
4. Understanding the behaviour of absorber elements in silver–indium–cadmium control rods during PWR severe accident sequences10.1016/j.pnucene.2009.09.012 ↗
5. Control rod materials and burnable poisons
6. Anderson · 1962
7. Bourgoin · 1994
8. The compressive deformation mechanisms of a coarse-grained AgInCd alloy10.1016/j.matchar.2017.11.015 ↗
9. Lifetime of PWR silver–indium–cadmium control rods
10. The behaviour of control rod absorber under irradiation10.1016/S0022-3115(99)00124-5 ↗
11. The recrystallization process in some polycrystalline metals10.1098/rspa.1962.0080 ↗
12. Stored energy and recrystallization temperature of rolled copper and silver single crystals with defined solute contents10.1016/0001-6160(79)90176-7 ↗
13. Diffusion annealing of copper–silver bimetallic strips at different temperatures10.1016/S1044-5803(01)00182-6 ↗
14. Recrystallization mechanisms of low stacking fault energy metals as characterized on model silver single crystals10.1016/j.actamat.2006.08.061 ↗
15. Experimental determination and simulation of annealing textures in cold rolled TWIP and TRIP steels10.1002/srin.201000261 ↗
16. Effect of crystallographic orientation on the corrosion of magnesium: comparison of film forming and bare crystal facets using electrochemical impedance and Raman spectroscopy10.1016/j.electacta.2016.12.107 ↗
17. Influence of grain orientation on the incipient oxidation behavior of Haynes 230 at 900 °C10.1016/j.matchar.2015.06.029 ↗
18. Twin-slip interaction in f.c.c. crystals10.1016/0001-6160(61)90110-9 ↗
19. Disconnections and other defects associated with twin interfaces10.1016/j.pmatsci.2016.07.003 ↗
20. Interactions between non-screw lattice dislocations and coherent twin boundaries in face-centered cubic metals10.1016/j.actamat.2007.11.020 ↗
21. Dislocation–twin interactions in nanocrystalline fcc metals10.1016/j.actamat.2010.10.028 ↗
22. Strain hardening regimes and microstructural evolution during large strain compression of low stacking fault energy fcc alloys that form deformation twins10.1007/s11661-997-0109-3 ↗
23. Deformation twinning in nanocrystalline materials10.1016/j.pmatsci.2011.05.001 ↗
24. Stacking fault energies and slip in nanocrystalline metals10.1038/nmat1136 ↗
25. The influence of stacking fault energy on the mechanical properties of nanostructured Cu and Cu–Al alloys processed by high-pressure torsion10.1016/j.scriptamat.2011.01.041 ↗
26. Deformation mechanisms of face-centered-cubic metal nanowires with twin boundaries10.1063/1.2721367 ↗
27. Influence of stacking fault energy on deformation mechanism and dislocation storage capacity in ultrafine-grained materials10.1016/j.scriptamat.2008.08.032 ↗
28. Humphreys · 2017
29. The effect of long term high temperature annealing on twinning and detwinning of the wrought Ni3Al-based alloy10.1016/j.matchar.2017.09.015 ↗
30. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
31. Ultrahigh strength and high electrical conductivity in copper10.1126/science.1092905 ↗
32. High-strength and thermally stable bulk nanolayered composites due to twin-induced interfaces10.1038/ncomms2651 ↗
33. Grain boundary formation by remnant dislocations from the de-twinning of thin nano-twins10.1016/j.scriptamat.2015.01.001 ↗
34. Kula · 1982