Nanoporous electrodes of phase-dealloyed Fe83.3-xCoxSi4B8P4Cu0.7 (x = 4, 10 and 20 at.%) precursors with superior Redox performances and high stabilities
Source abstract
Abstract
Abstract Co substitutions for Fe83.3Si4B8P4Cu0.7 precursors are effective to stabilize the nanoporous structures during dealloying in H2SO4 solutions and improve Redox performances of nanoporous electrodes in alkaline conditions. Heterogeneous nanocrystalline structures of Co-substituted Fe83.3-xCoxSi4B8P4Cu0.7 (x = 0, 4, 10 and 20 at.%) alloys consist of two phases: α-Fe(Co) phases and continuously distributed residual amorphous phases. The nanopores on as-dealloyed Fe-Co-Si-B-P-Cu alloys are smaller in size with higher Co concentrations. This is ascribed to the finer α-Fe(Co) phases distributed in the precursor alloys after nanocrystallization. Nanoporous architectures after dealloying inherit the microstructural characteristics of Fe-Co-Si-B-P-Cu precursor alloys. The short-term and long-term CV curves of nanoporous Redox electrodes in 0.5 M KOH solution demonstrate that Redox reactions have been enhanced by partial substitution of Fe by Co and the best Redox performance can be obtained on as-dealloyed Fe79.3Co4Si4B8P4Cu0.7 alloys because of the highest Redox peak current density of 90 mA cm−2 after 150 CV cycles. However, the stabilities of nanoporous Fe79.3Co4Si4B8P4Cu0.7 electrodes have a predictable decline due to the overgrowth of Fe3O4 octahedra and destruction of the ligaments during long-term Redox cycling. On the other hand, the better Redox stabilities has achieved on as-dealloyed Fe63.3Co20Si4B8P4Cu0.7 alloys with stable oxidation peak current densities of 45–47 mA cm−2 from 950 to 3000 CV cycles, about 2.3 times the nanoporous Co-free Fe83.3Si4B8P4Cu0.7 electrodes. The stabilities are considered to result from the relatively small Fe3O4 octahedra, the stabilization of the amorphous Co3O4 outmost layers and the transformation of amorphous and crystalline Co3O4 phases during long-term Redox cycling. The Co substitution of Fe83.3Si4B8P4Cu0.7 precursor alloys can achieve the high Redox performances and good stabilities of nanoporous electrodes.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nanoporous metals and alloys · Electrocatalysts for Energy Conversion · Supercapacitor Materials and Fabrication
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Rapid degradation of azo dye by Fe-based metallic glass powder10.1002/adfm.201103015 ↗
2. Decolorization of azo dye solution by Fe-Mo-Si-B amorphous alloy10.1016/j.jnoncrysol.2010.06.019 ↗
3. Influence of thermal relaxation and nanocrystallisation on the corrosion behaviour of Fe73.5-xCu1Nb3Si13.5B9Cox (1, 2, 3, 4, 5) metallic amorphous alloys
4. Effects of Al on the magnetic properties of nanocrystalline Fe73.5Cu1Nb3Si13.5B9 alloys10.1063/1.352574 ↗
5. Effect of Co content on structure and magnetic behaviors of high induction Fe-based amorphous alloys10.1016/j.jmmm.2016.02.055 ↗
6. Influence of nickel content on the electrochemical behavior of Finemet type amorphous and nanocrystalline alloys10.1016/j.jnoncrysol.2006.12.088 ↗
7. New Fe-based soft magnetic alloys composed of ultrafine grain structure10.1063/1.342149 ↗
8. FeSiBP metallic glasses with high glass-forming ability and excellent magnetic properties10.1016/j.mseb.2007.09.010 ↗
9. A study of structure and magnetic properties of low purity Fe-Co-based metallic glasses10.3390/ma10060625 ↗
10. Effect of iron on the thermal and the magnetic properties for cobalt-based amorphous alloys10.3938/jkps.67.2120 ↗
11. Thermal and electrochemical properties of cobalt containing Finemet type alloys10.1016/j.electacta.2003.08.012 ↗
12. Effects of Co addition in nanocrystalline Fe83.3Si4B8P4Cu0.7 soft magnetic alloy
13. Effects of minor precipitation of large size crystals on magnetic properties of Fe-Co-Si-B-P-Cu alloy10.1016/j.jallcom.2017.03.193 ↗
14. von Goldbeck · 1982
15. Electrochemical and surface characterization of electrocatalytically active amorphous Ni-Co alloys10.1016/0013-4686(92)87119-K ↗
16. A microscopic and impedance spectroscopy study of Finemet-Co amorphous alloys10.1016/S0010-938X(02)00146-4 ↗
17. Electrocatalysis by amorphous metals of hydrogen and oxygen evolution in alkaline solution10.1016/0022-0728(86)90088-4 ↗
18. Influence of deposition potential on the electrodeposited ternary CoFeCu films
19. Enhanced redox properties of amorphous Fe63.3–83.3Co0-20Si4B8P4Cu0.7 alloys via long-term CV cycling10.1016/j.jallcom.2018.04.119 ↗
20. Annealing effect of amorphous Fe-Si-B-P-Cu precursors on microstructural evolution and redox behavior of nanoporous counterparts10.1016/j.jallcom.2017.08.045 ↗
21. Structural inheritance and Redox performance of nanoporous electrodes from nanocrystalline Fe85.2B10-14P0-4Cu0.8 alloys10.3390/nano7060141 ↗
22. Mechanism of active dissolution of nanocrystalline Fe-Si-B-P-Cu soft magnetic alloys10.1016/j.matchar.2016.08.012 ↗
23. The electrochemical and electrocatalytic behaviour of glassy metals10.1007/s10800-005-4726-5 ↗
24. Trends in activity for the water electrolyser reactions on 3d M (Ni, Co, Fe, Mn) hydr (oxy) oxide catalysts10.1038/nmat3313 ↗
25. Effect of Si addition on the corrosion properties of amorphous Fe-based soft magnetic alloys10.1016/j.jnoncrysol.2014.05.007 ↗
26. Effects of P addition on corrosion properties of soft magnetic FeSiB alloys10.2320/matertrans.MAW201307 ↗
27. Effect of substitution of Cu by Au and Ag on nanocrystallization behavior of Fe83.3Si4B8P4Cu0.7 soft magnetic alloy10.1016/j.jallcom.2016.05.027 ↗
28. Competition driven nanocrystal -lization in high Bs and low coreloss Fe–Si–B–P–Cu soft magnetic alloys10.1016/j.scriptamat.2014.08.023 ↗
29. The nickel/iron battery10.1016/0378-7753(91)80002-F ↗
30. Redox switching and oxygen evolution at oxidized metal and metal oxide electrodes: iron in base10.1039/c1cp22470k ↗
31. Voltammetric study of an iron electrode in alkaline electrolytes10.1016/0378-7753(89)85003-7 ↗
32. The potentiodynamic behavior of iron in alkaline solutions10.1016/0013-4686(79)87026-7 ↗
33. The crystallization of amorphous Fe60Co20Si10B10 and its effect on the electrocatalytic activity for H2 evolution10.1063/1.345528 ↗
34. A study of anodically grown hydroxide films on an amorphous Ni78Si8B14 alloy10.1149/1.2721765 ↗
35. A highly efficient and self-stabilizing metallic-glass catalyst for electrochemical hydrogen generation10.1002/adma.201603880 ↗
36. Visualizing under-coordinated surface atoms on 3D nanoporous gold catalysts10.1002/adma.201504032 ↗
37. CuxCo3-xO4 used as bifunctional electrocatalyst physicochemical properties and electrochemical characterization for the oxygen evolution reaction10.1149/1.2338631 ↗
38. Facile preparation of graphene nanosheets encapsulated Fe3O4 octahedra composite and its high lithium storage performances10.1016/j.cej.2017.01.023 ↗
39. The raman spectra of Co3O410.1088/0022-3719/21/7/007 ↗
40. Study of the redox properties of Noble metal/Co3O4 by electrical conductivity measurements10.1007/s10562-008-9463-z ↗
41. Characterization of spinel Co3O4 and Li-doped Co3O4 thin film electrocatalysts prepared by the sol–gel route10.1016/S0013-4686(00)00543-0 ↗
42. Conducting spinel oxide films with infrared transparency10.1016/S0040-6090(02)00740-X ↗