Abstract TC11/Ti2AlNb welding joints undergoing hot deformation were thermally exposed at the range of 500–700 °C for 100, 200 and 500 h. In present research, typical microstructures of five different zones of the joints were investigated, fusion zone, two interfaces and two base alloys included. The microstructures of fusion zone, Ti2AlNb-based alloy and the interface between them were characterized by the coarsening of O phase during thermal exposure, while those of TC11 alloy and the interface between it and fusion zone featured the coarsening of αs phase. The transformation from B2 to β and O phase was stifled below 600 °C and Ti2AlNb-based alloy thus was verified to be stable at this temperature range. αs phase was stable during exposure at 500 °C. When exposed above 600 °C, αs phase coarsened by at least 52% with the extension of holding time. Due to the low thermal stability of αs phase compared with that of O phase, the fracture position of the samples tested at room temperature moved from fusion zone to TC11 alloy when temperature rose. In spite of different thermal exposure conditions, the samples tested at 300 and 500 °C all fractured at TC11 alloy for the severe coarsening of αs phase. The decrease of interfacial area resulting from the coarsening of O and αs phases facilitated the dislocation slipping and the strength of joints thus deteriorated. The mechanical properties of TC11/Ti2AlNb joints measured at room temperature, 300 and 500 °C were all correlated with the lamellar thickness of O and αs phases.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Microstructural evolution and tensile behavior of Ti2AlNb alloys based alpha(2)-phase decomposition10.1016/j.msea.2016.03.058 ↗
2. Microstructure control and mechanical properties from isothermal forging and heat treatment of Ti–22Al–25Nb (at.%) orthorhombic alloy10.1016/j.intermet.2014.07.011 ↗
3. Tensile behavior of Ti-22Al-24Nb-0.5Mo in the range 25–650 °C10.1016/j.msea.2016.10.047 ↗
4. Microstructure evolution of electron beam welded Ti3Al-Nb joint10.1016/j.matchar.2004.11.006 ↗
5. Transient liquid phase diffusion bonding of Ti-24Al-15Nb-1Mo alloy to TiAl intermetallics10.1016/j.msea.2015.10.075 ↗
6. Solid state joining of metals by linear friction welding: a literature review10.1179/026708310X520510 ↗
7. Effect of heat treatment before welding on microstructure and property of Ti-22Al-25Nb/TC11 dissimilar alloy joint
8. Effect of hot working on microstructure and mechanical properties of TC11/Ti2AlNb dual-alloy joint welded by electron beam welding process10.1016/S1003-6326(14)63494-4 ↗
9. Effects of welding condition on weld shape and distortion in electron beam welded Ti2AlNb alloy joints10.1016/j.matdes.2016.11.083 ↗
10. The influence of high temperature exposure on fracture behaviors of TC11 titanium alloy
11. Effects of thermal exposure on microstructure and mechanical properties of TC11 titanium alloy
12. Influence of thermal exposure on the tensile properties and microstructures of Ti60 titanium alloy10.1016/j.msea.2011.10.011 ↗
13. Effect of microstructure on oxygen rich layer evolution and its impact on fatigue life during high-temperature application of alpha/beta titanium10.1016/j.actamat.2016.01.058 ↗
14. Long-term oxidation of orthorhombic alloy Ti-22Al-25Nb in air between 650 and 800 °C10.1016/S1359-6462(99)00234-1 ↗
15. Instability of the O-phase in Ti-22Al-25Nb alloy during elevated-temperature deformation10.1016/j.jallcom.2013.05.018 ↗
16. Effects of high temperature air and vacuum exposures on the room temperature tensile behavior of the (O+B2) titanium aluminide Ti-22Al-23Nb10.1016/0921-5093(95)10049-0 ↗
17. Microstructure evolution and mechanical properties of linear friction welded Ti2AlNb alloy10.1016/j.jallcom.2015.05.198 ↗
18. Microstructural evolution and mechanical properties of linear friction welded Ti2AlNb joint during solution and aging treatment10.1016/j.msea.2016.05.030 ↗
19. In situ investigation of the tensile deformation of laser welded Ti2AlNb joints10.1016/j.matchar.2016.11.009 ↗
20. Oxidation behavior of three different zones of linear friction welded Ti2AlNb alloy10.1002/adem.201600529 ↗
21. Alpha phase precipitation in Ti-30Nb-1Fe alloys - phase transformations in continuous heating and aging heat treatments10.1016/j.msea.2016.09.023 ↗
22. Superplastic forming and diffusion bonding of Ti-22Al-24Nb alloy10.1016/j.jmatprotec.2015.03.005 ↗
23. The effect of aging on microstructure of the O-phase in Ti-24Al-14Nb-3V-0.5Mo alloy10.1016/S0167-577X(00)00357-8 ↗
24. On the B2 → O phase transformation in Ti-Al-Nb alloys10.1016/S0921-5093(02)00507-5 ↗
25. Transformations in a Ti-24Al-15Nb alloy: part I. phase equilibria and microstructure10.1007/BF02801158 ↗
26. Microstructural evolution, creep, and tensile behavior of a Ti-22Al-25Nb (at%) orthorhombic alloy10.1016/j.msea.2014.02.004 ↗
27. Zhang · 2001
28. A rationalization of stress-strain behavior of 2-ductile phase alloys10.1007/BF02645919 ↗
29. The Arrhenius formula in kinetic theory and Witten's spectral asymptotics10.1088/1751-8113/44/21/215202 ↗
30. Effect of the addition of palladium on grain growth kinetics of pure titanium10.1016/S0925-8388(97)00135-7 ↗
31. Behaviour of normal grain growth kinetics in single phase titanium and titanium alloys10.1016/S0921-5093(00)00731-0 ↗