Preferential distribution behavior of B and its enhancement on creep strength of alumina-forming austenitic heat-resistant steel
Source abstract
Abstract
The addition of a trace amount of 20 ppm B significantly enhanced the creep performance of the 2.5Al-AFA alloy at 650 °C, demonstrating sustained improvement even after prolonged thermal aging. Boron (B) preferentially distributed in the Laves phase within the matrix, rather than in the NiAl or Cr - rich phases. APT analysis revealed M23C6 may serve as a reservoir of B, gradually allowing B diffusing into the surrounding Laves phase at grain boundaries (GBs). Creep cracks propagated mainly along GBs, with the σ phase serving as initiation sites. The average volume fraction of σ phase exhibited a linear correlation with the reciprocal of creep rupture time. B accelerated the precipitation of Laves with a larger size and higher volume fraction, which played a dual role of improved GB strengthening and more effective suppression of σ phase growth.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (45)
Show source-provided references
1. Effects of silicon additions on the oxide scale formation of an alumina-forming austenitic alloy10.1016/j.corsci.2012.08.039 ↗
2. The effect of thermo-mechanical treatment on the high temperature tensile behavior of an alumina-forming austenitic steel10.1016/j.msea.2015.11.036 ↗
3. Effect of tungsten addition on high-temperature properties and microstructure of alumina-forming austenitic heat-resistant steels10.1016/j.msea.2015.09.018 ↗
4. The precipitation control in aged alumina-forming austenitic stainless steels Fe-15Cr-25Ni-3Al-NbWCu by W addition and its effect on the mechanical properties10.1016/j.matchar.2020.110233 ↗
5. Alumina-forming austenitic stainless steels strengthened by laves phase and MC carbide precipitates10.1007/s11661-007-9319-y ↗
6. The development of alumina-forming austenitic stainless steels for high-temperature structural use10.1007/s11837-008-0083-2 ↗
7. Effects of minor alloy additions and oxidation temperature on protective alumina scale formation in creep-resistant austenitic stainless steels10.1016/j.scriptamat.2007.08.032 ↗
8. Overview of strategies for high-temperature creep and oxidation resistance of alumina-forming austenitic stainless steels10.1007/s11661-010-0295-2 ↗
9. Effect of alloying additions on phase equilibria and creep resistance of alumina-forming austenitic stainless steels10.1007/s11661-009-9886-1 ↗
10. Creep-resistant, Al2O3-forming austenitic stainless steels10.1126/science.1137711 ↗
11. Composition, microstructure, and water vapor effects on internal/external oxidation of alumina-forming austenitic stainless steels
12. Corrosion resistance of candidate cladding materials for supercritical water reactor10.1016/j.anucene.2018.12.007 ↗
13. Overview on performance degradation behavior of 20Cr25NiNb steel for gas cooled reactor cladding during service10.3389/fmats.2022.1058045 ↗
14. Alomari · 2019
15. Aging effects on the mechanical properties of alumina-forming austenitic stainless steels
16. The effect of aging on the microstructure and mechanical behavior of the alumina-forming austenitic stainless steel Fe–20Cr–30Ni–2Nb–5Al10.1016/j.msea.2014.12.072 ↗
17. Effect of grain boundary Fe2Nb laves phase on creep of austenitic heat resistant steel of Fe-20Cr-30Ni-2Nb in steam atmosphere10.2355/tetsutohagane.100.1158 ↗
18. Tarigan · 2012
19. Precipitate characteristics and their effects on the high-temperature creep resistance of alumina-forming austenitic stainless steels10.1016/j.msea.2014.11.013 ↗
20. Improved creep strength of alumina-forming austenitic heat-resistant steels through W addition10.1016/j.msea.2017.04.062 ↗
21. Ultrahigh stability and strong precipitation strengthening of nanosized NbC in alumina-forming austenitic stainless steels subjecting to long-term high-temperature exposure10.1016/j.msea.2018.09.081 ↗
22. The effect of isothermal aging on creep behavior of modified 2.5Al alumina-forming austenitic steel10.1016/j.msea.2020.140219 ↗
23. Relative effect of B and N concentrations on the microstructural stability and mechanical properties of modified 9Cr-1Mo steel10.1016/j.jallcom.2021.158971 ↗
24. Effect of boron on microstructure and creep strength of advanced ferritic power plant steels
25. Tarigan · 2011 · 317
26. Precipitation behavior of Fe 2 Nb laves phase on grain boundaries in austenitic heat resistant steels10.1016/j.msea.2014.07.104 ↗
27. Effect of boron and carbon addition on microstructure and mechanical properties of the aged gamma-prime strengthened alumina-forming austenitic alloys10.1016/j.intermet.2017.06.011 ↗
28. Atom probe tomography study of Fe segregation at phase interface in Zr–2.5Nb alloy10.1007/s40195-019-00927-x ↗
29. Improved creep resistance of 20Cr25NiNb heat resistant steels through grain boundary intermetallic precipitation strengthening10.1016/j.jmrt.2023.06.213 ↗
30. Evolution of microstructure and tensile properties of Fe–18Ni–12Cr based AFA steel during aging at 700°C10.1016/j.msea.2016.06.060 ↗
31. Microstructural changes in austenitic stainless-steels during long-term aging10.1179/mst.1986.2.8.795 ↗
32. The precipitation characteristics of 20-percent CR 25-percent NI-NB stabilized stainless-steel10.1016/0001-6160(88)90105-8 ↗
33. Precipitation in creep resistant austenitic stainless steels10.1179/026708301101508972 ↗
34. Precipitation in a 20 percent cr – 25 percent ni steel stabilized with niobium
35. The formation of G-phase in 20/25 Nb stainless steel AGR fuel cladding alloy and its effect on creep properties10.1007/BF01086484 ↗
36. Effect of high-temperature exposure on the mechanical properties of 18Cr–8Ni–W–Nb–V–N stainless steel10.1016/j.msea.2012.06.011 ↗
37. Evolution of boron segregation during tempering in B doped 9%Cr ferritic steel10.1016/j.matchar.2021.111192 ↗
38. Non-equilibrium grain boundary segregation of boron in austenitic stainless steel – I. Large scale segregation behaviour10.1016/0001-6160(88)90023-5 ↗
39. On diffusion and interfacial enrichment of boron in the Laves phase: an in situ TEM-heat-treatment study on newly developed 3Co–3W–9Cr steel10.1080/09500839.2019.1670880 ↗
40. Atom probe tomography characterization of ion and neutron irradiated Alloy 800H10.1016/j.jnucmat.2020.152598 ↗
41. Irradiation-induced precipitation and inverse coarsening of G-phase in austenitic stainless steel weld metal10.1016/j.matchar.2019.03.035 ↗
42. The effect of isothermal aging on microstructure and mechanical behavior of modified 2.5Al alumina-forming austenitic steel10.1016/j.msea.2019.01.087 ↗
43. Precipitates evolution during isothermal aging and its effect on tensile properties for an AFA alloy containing W and B elements10.1007/s10853-023-08663-5 ↗
44. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
45. Laves phase precipitation behavior in HiperFer (high performance ferritic) steel with and without boron alloying10.3390/met13020235 ↗