journal article·2011-02

Characterization of precipitation behaviors in a non-stoichiometric Cu-24.5at.%Al-19.4at.%Mn alloy

S.C. Jeng

Materials Characterization· Volume 62· Issue 2
Publisher page

Abstract

Abstract Scanning and transmission electron microscopy examinations of Cu-24.5at.% Al-19.4at.%Mn (similar to Cu 2.2 Mn 0.8 Al) alloy were performed after aging at temperatures ranging from 350 °C to 700 °C for various durations. It was observed that only γ-brass type and L-J phases were formed after aging at or below 400 °C. On the other hand, the β-Mn phase was formed after aging at temperatures ranging from 500 °C to 650 °C. It is noteworthy that the precipitation behaviors of the γ-brass type and β-Mn phases are different at different aging temperatures. This remarkable result differs from those reported in previous studies on the Cu 3 − X Mn X Al alloys with X ≦ 1.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgy and Material Science · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Das Dreistoffsystem Kupfer-Mangan-Aluminium
2. Phase equilibria and Heusler phase stability in the Cu-rich portion of the Cu-Al-Mn system10.1016/S0925-8388(97)00425-8 ↗
3. Phase transformations and shape memory effect in copper-aluminium-manganese alloys
4. Aging of Cu-Mn-Al Heusler alloys
5. TEM study of the decomposition of the Heusler alloy Cu2MnAl10.1007/BF01133330 ↗
6. Phase transitions and modulated structures in ordered (Cu-Mn)3Al alloys10.1016/0001-6160(75)90159-5 ↗
7. Order–disorder phase transitions in ternary alloys Cu3-XMnXAl10.1002/pssa.2210630204 ↗
8. Investigation of low-temperature precipitation in copper-manganese-aluminium alloys deviating from stoichiometric composition
9. Structural changes during disintegration of Cu-Mn-Al alloys
10. Electron microprobe analysis of phase segregation in the Heusler alloy Cu2.00Mn1.00Al1.0010.1007/BF00700791 ↗
11. X-ray diffraction quantitative analysis of the Heusler alloy Cu2.00Mn1.00Al1.00 annealed at temperature between 423 and 973K10.1007/BF00735559 ↗
12. Decomposition of β-phase in the Heusler alloy Cu2.00Mn1.00Al1.0010.1007/BF00752258 ↗
13. L-J phase in a Cu2.2Mn0.8Al alloy10.1007/BF02647586 ↗
14. Microstructural evolution in a Cu-24.5at.%Al-19.4at.%Mn alloy inside the miscibility gap10.1016/j.jallcom.2006.09.112 ↗
15. Precipitation at superlattice domain boundaries with particular reference to a copper-aluminium-nickel alloy10.1080/14786436608211944 ↗
16. Mechanisms of phase transformations within the miscibility gap of Fe-rich Fe-Al alloys10.1016/0001-6160(76)90063-8 ↗
17. Orientation relationship between β-Mn and L21 matrix in a Cu2MnAl alloy10.1007/s11661-999-0170-1 ↗
18. Decomposition of the Heusler alloy Cu2MnAl at 360°C10.1007/BF00737017 ↗
19. Phase transformations in a Cu-35at.%Mn-25at.%Al alloy10.1016/j.jallcom.2005.09.021 ↗