Role of PVD oxide coatings on HK40 cast steel during short and long exposure to C-rich atmospheres
Source abstract
Abstract
Abstract The role of Cr/Cr oxide thin film coatings on HK40 steel substrates during exposure to C-rich atmospheres was investigated. The coatings were produced via reactive magnetron sputtering as an alternative method to protect these materials against metal dusting. Coated and uncoated substrates were exposed at 1073 K to an Ar + CH 4 atmosphere with residual oxygen for 10, 30, 60 min and 50 h. Analysis of the products formed on both samples indicated that attack in the uncoated samples involves both C and O from the atmosphere together with Cr, Fe, and Ni outward diffusion in which the dendritic structure plays an important role. The presence of even a residual amount of oxygen in the carburizing atmosphere had a remarkable effect on the corrosion mechanism in these samples as well. In the coated samples, the Cr/Cr oxide film minimized internal alloy attack not only by limiting carbon ingress, but also minimizing the role of oxygen and outward Cr (Fe and Ni) diffusion from the alloy.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metal and Thin Film Mechanics · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Grabke · 2007 · 154
2. Micromechanisms of metal dusting on Fe-base and Ni-base alloys10.1002/(SICI)1521-4176(199805)49:5<309::AID-MACO309>3.0.CO;2-1 ↗
3. Mechanism and control of carbon deposition on high temperature alloys10.1149/1.2750447 ↗
4. Inhibition of metal musting of alloy 800H by laser surface melting10.1016/j.apsusc.2005.05.040 ↗
5. Grabke · Oxid Met · 1998 · 50 · 24110.1023/A:1018888321213 ↗
6. Protective behaviour of newly developed coatings against metal dusting10.1002/maco.200303736 ↗
7. Metal dusting behavior of coatings
8. Production, characterization and evaluation of protective Cr oxide coatings against metal dusting10.1016/j.surfcoat.2009.09.058 ↗
9. Role of Al oxide PVD coatings in the protection against metal dusting10.1016/j.surfcoat.2009.09.060 ↗
10. Metal dusting protective coatings. a literature review10.1007/s11085-011-9248-4 ↗
11. Initiation and growth of iron metal dusting in CO–H2–H2O gas mixtures10.1016/j.corsci.2007.11.021 ↗
12. Carburization mechanisms of high chromium alloys10.1149/1.2114333 ↗
13. An active corrosion mechanism for metal dusting on 304L stainless steel10.1016/S0010-938X(02)00053-7 ↗
14. Mechanisms and driving forces of metal dusting10.1002/maco.200303737 ↗
15. Chun · 2007 · 25
16. In situ environmental scanning electron microscope observations of catalytic processes encountered in metal dusting corrosion on iron and nickel10.1016/S0926-860X(01)00539-7 ↗
17. Structure of centrifugally cast austenitic stainless steels: part 1 HK 40 as cast and after creep between 750 and 1000°C10.1179/mst.1985.1.5.385 ↗
18. Recent advances in understanding metal dusting: a review10.1002/maco.201005675 ↗
19. A study on the solubility and distribution of carbon in oxides10.1016/0038-1098(85)91021-X ↗