Low cycle fatigue behavior of salt coated and pre-exposed IN-617 alloy
Source abstract
Abstract
Abstract The present investigation deals with low cycle fatigue (LCF) behavior of the IN-617 alloy, after oxidation at 850 °C for varying durations, without and with mixed salt coating. LCF tests were conducted under fully reversed axial strain controlled mode at a strain rate of 5 × 10−3 s−1 and strain amplitude of ±0.25% at 850 °C to examine the influence of oxidation and mixed salt coating of 10%NaCl+90%Na2SO4, on fatigue life and deformation behavior under cyclic loading. Oxidation of the samples up to 1000 h did not show any significant effect on fatigue life, whereas fatigue life of the salt coated and pre-exposed samples was drastically reduced with increase in duration of the exposure. Stress amplitude decreased with increase in the duration of the exposure. Salt coated samples exhibited lower stress amplitude compared to that of the oxidized samples. XRD analysis and Electron Probe Micro Analysis (EPMA) elemental mapping confirmed formation of effective Cr2O3 layer on the surface and Al2O3 layer beneath the surface which provided good oxidation resistance at this temperature. The depth of oxide layer increased with increase in the duration of oxidation. Under salt environment, these oxide layers were broken and the substrate was exposed to corrosive environment, which caused severe intergranular hot corrosion of the samples. The depth of intergranular corrosion was increased with increase in the duration of exposure. Chromium sulphide was found to be the detrimental product formed along the grain boundaries and was the prime reason for rapid crack propagation and reduction in the fatigue life.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Microstructure and phase stability of Inconel alloy 61710.1007/BF02643879 ↗
2. Inconel alloy 617- a new high-temperature alloy
3. Hot corrosion of four superalloys: HA-188, S-57, IN-617, and TD-NiCrAl10.1007/BF00605108 ↗
4. High temperature cyclic oxidation of Ni based superalloys at different temperatures in air10.1016/j.jallcom.2017.05.130 ↗
5. Thermal degradation behavior of Inconel 617 alloy10.3365/met.mat.2008.12.739 ↗
6. Cyclic oxidation kinetics and oxide scale morphologies developed on alloy 61710.1016/j.apsusc.2014.04.199 ↗
7. Response of Inconel 617 to sea salt and re-entry conditions10.2514/3.25089 ↗
8. Hot corrosion behaviour of Inconel 617 in mixed salt environment at 900 and 1000°C for gas turbine applications
9. Hot corrosion behavior of Ni based Inconel 617 and Inconel 738 superalloys10.1016/j.apsusc.2016.03.181 ↗
10. Hot corrosion in gas turbine components10.1016/S1350-6307(00)00035-2 ↗
11. Oxidation and hot corrosion of superalloys
12. Effect of high-temperature hot corrosion on the low cycle fatigue behavior of a directionally solidified nickel-base superalloy10.1016/j.ijfatigue.2014.08.011 ↗
13. Low cycle fatigue behaviour of cast nickel-base superalloy IN-738LC in air and in hot corrosive environments10.1016/0025-5416(83)90144-1 ↗
14. Influence of hot corrosion on low cycle fatigue behavior of nickel base superalloy SU 26310.1016/j.ijfatigue.2013.02.006 ↗
15. Effect of salt coatings on low cycle fatigue behavior of nickel base superalloy GTM-SU-71810.1016/j.proeng.2013.03.339 ↗
16. Effect of hot corrosion on low cycle fatigue behavior of superalloy IN71810.1016/j.ijfatigue.2013.08.009 ↗
17. Interaction of hot corrosion and creep in alloy 61710.1016/j.engfailanal.2016.03.012 ↗
18. Dynamic strain aging, deformation and fracture behaviour of the nickel base superalloy Inconel 61710.1016/j.msea.2018.10.123 ↗
19. Low cycle fatigue, deformation and fracture behaviour of Inconel 617 alloy10.1016/j.msea.2019.138286 ↗
20. An overview of Na2SO4 and/or V2O5 induced hot corrosion of Fe-and Ni-based superalloys
21. The role of microstructure on oxidation of Ni-Cr-Al base alloys at 1023 and 1123 K in air10.1007/BF00665666 ↗
22. Mueller · 2007
23. Gulsoy · 2014
24. Phase equilibria in the Ni–Cr–Ti system at 850° C10.1016/S0925-8388(98)00505-2 ↗
25. Diffusion paths of silicide coatings on Nb-Si-based alloys during pack cementation process10.1007/s11661-019-05204-1 ↗
26. Thermo-Calc & DICTRA
27. Influence of the different salt deposits on the fatigue behavior of a directionally solidified nickel-based superalloy10.1016/j.ijfatigue.2015.11.020 ↗
28. Oxidation of Ni-Cr-Al alloys between 1000 and 1200°C10.1149/1.2407837 ↗
29. Mechanisms of high-temperature corrosion in helium containing small amounts of impurities. II. Corrosion of the nickel-base alloy Inconel 61710.1007/BF00656643 ↗
30. Fatigue behavior of nickel based super alloy 718 in a hot corrosive environment10.1520/MPC20130039 ↗
31. Hot corrosion studies on Ni-base superalloy at 650°C under marine like environment conditions using three salt mixture (Na2SO4+NaCl+NaVO3)10.1016/j.corsci.2016.01.008 ↗
32. Effect of pre hot corrosion on high cycle fatigue behavior of the superalloy IN718 at 600°C10.1016/j.ijfatigue.2018.05.021 ↗
33. Hot corrosion behavior of CM 247 LC alloy in Na2SO4 and NaCl environments10.1023/A:1018831025272 ↗