Electron microscopy study of the formation mechanism of catalytic nickel-rich particles and the role of carbonyl sulphide in the suppression of carbon deposition on 20Cr-25Ni steel
Source abstract
Abstract
Austenitic stainless steel is used as fuel cladding in advanced gas-cooled nuclear reactors (AGR). At elevated temperatures, when the steel is exposed to CO2 based environments filamentary carbon deposits form on the surface of the steel. This filamentary carbon deposition is known to be catalysed by metallic nickel-rich particles. Adding trace amount of carbonyl sulphide (COS) into the gas mixtures suppresses the carbon deposition. In this current work, it has been shown that at 600 °C, the formation of filamentary carbon was suppressed by the addition of 215 ppb COS to a depositing gas mixture (containing approximately 1000 vppm C2H4/1% CO/bal. CO2) which was known to provide the environment suitable for carbon deposition. Samples exposed to the gas mixtures with and without 215 ppb COS were characterised using electron microscopy techniques to understand the formation mechanism of the nickel-rich particles and the inhibition mechanism due to the addition of COS. Electron diffraction study shows that the nickel-rich particles in the oxide layers assume the same crystallography as that of the austenitic metal underneath, regardless of the COS addition. The current observations also show that the metal-oxide interfaces was nickel-rich and a simple model has been proposed to explain the formation of nickel-rich particles within the subsurface oxide. Furthermore, it was found that when COS was added the surface of the nickel-rich particles in the oxide layer was found to be sulphur-rich by energy dispersive spectroscopy (EDS) on a scanning transmission electron microscope (STEM). It is believed that the surface sulphur adsorption onto the nickel-rich particles, rather than bulk sulphide formation, resulted in the inhibition of carbon deformation on the steel.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · nanoparticles nucleation surface interactions · Catalytic Processes in Materials Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Dyer · 1980
2. High temperature corrosion and deposition phenomena on stainless steels10.1179/mst.1994.10.12.1090 ↗
3. The influence of oxide layers on the initiation of carbon deposition on stainless steel10.1023/A:1010320727492 ↗
4. Recent advances in understanding metal dusting: a review10.1002/maco.201005675 ↗
5. Microprocesses in nickel accompanying metal dusting10.1016/j.actamat.2007.09.010 ↗
6. Carbon deposition on stainless steel in oxidising environments10.1179/mht.2003.062 ↗
7. The resistance of 20Cr/25Ni steels to carbon deposition. IV. The influence of alloy silicon content10.1002/maco.19870380503 ↗
8. Inhibition of carbon deposition on iron and steel surfaces10.1016/0008-6223(71)90083-2 ↗
9. Sulfur-passivated nickel catalysts for carbon-free steam reforming of methane10.1016/0021-9517(84)90107-6 ↗
10. Effect of sulphur on the interaction on nickel with ethylene10.1016/0920-5861(94)80030-8 ↗
11. The interplay between sulphur adsorption and carbon decomposition on cobalt catalysts10.1006/jcat.1993.1289 ↗
12. The effect of various sulfides on carbon deposition on nickel-iron particles10.1016/S0920-5861(00)00441-7 ↗
13. The Effect of temperature and carbonyl sulphide on carbon deposition on 20Cr25Ni stainless steel10.1007/s11085-017-9723-7 ↗
14. The influence of carbonyl sulphide on the inhibition of filamentary carbon deposition on stainless steel10.1002/maco.200303733 ↗
15. The resistance of 20Cr/25Ni steels to carbon deposition. I. The role of surface grain size10.1002/maco.19870380304 ↗
16. Carbon deposition on iron–nickel during interaction with ethylene–hydrogen mixtures10.1006/jcat.1998.2226 ↗
17. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys10.1149/1.2779605 ↗
18. Compositional changes in the underlying alloy during the protective oxidation of alloys10.1016/0001-6160(67)90173-3 ↗
19. Chromium-depleted zones and the oxidation process in stainless steels10.1007/BF00612157 ↗
20. Behavior of the Scale on a 9.5Cr steel under cyclical10.1007/BF00656645 ↗
21. Limits of the oxidation resistance of several heat-resistant steels under isothermal and cyclic oxidation as well as under creep in air at 650 °C10.1080/09603409.1997.11689565 ↗
22. The effect of S, N, and C on the oxidation of Ni-20%Cr and Fe-20%Cr10.1007/BF02134788 ↗
23. Surface and interface segregation in the oxidation of metals10.1002/1096-9918(200008)30:1<112::AID-SIA777>3.0.CO;2-G ↗
24. Gamsjäger · 2005 · Vol. 6
25. Vignes · 2013
26. The crystal structure of heazlewoodite, and metallic bonds in sulfide minerals
27. Long term variations in hydrogen concentration in AGR gas circuits
28. Ni-S (nickel-sulfur)10.1007/s11669-008-9430-9 ↗
29. The crystal chemistry of iron-nickel thiospinels
30. Chemisorption of hydrogen sulfide on a supported nickel catalyst10.1016/0021-9517(68)90035-3 ↗
31. Sulfur poisoning of nickel in CO hydrogenation
32. Thermodynamics of sulfur chemisorption on metals. I10.1063/1.439156 ↗
33. Computational study of sulfur–nickel interactions: a new S-Ni phase diagram10.1016/j.elecom.2007.06.022 ↗