Microstructure and performance characterization of in-situ Co2FeO4 whiskers reinforced YIG/YIG joints

Qianqian Chen, Panpan Lin, Xuanyu Du, Wumo Du, Tiesong Lin, Peng He

Publisher page

Abstract

Abstract Bismuth-based glasses doped with different CoO contents were designed to realize the in-situ growth of Co2FeO4 whiskers in YIG/YIG joint. The microstructure, mechanical and dielectric properties of the joints were systematically investigated. The optimized processing joint with 23 mol% CoO doping, brazed at 725 °C for 15 min, under bonding pressure of 6 kPa was achieved. And the shear strength of joint reached a maximum of 72 MPa, which is attributed to the increased number and optimized spatial distribution of Co2FeO4 whiskers. The in-situ Co2FeO4 whiskers acted as effective hard phases in the glass matrix. The shear strength of YIG/YIG joint was enhanced by the crack propagation deflection and pulling out result from Co2FeO4 whiskers. The dielectric constant of YIG joints decreased from 16.2 to 15.3 at the frequency of 10 MHz, which is closer to that of the original YIG material with the CoO doping increasing. The dielectric loss tangent increased slightly with the growth of Co2FeO4 whiskers due to the hole hopping between Co3+⇔Co2+ ions. The effective bonding of YIG materials has broad application prospects for the integration of ferrite microwave devices.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magneto-Optical Properties and Applications · Microwave Dielectric Ceramics Synthesis · Ferroelectric and Piezoelectric Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Low-temperature synthesis and microstructure-property study of single-phase yttrium iron garnet (YIG) nanocrystals via a rapid chemical coprecipitation10.1016/j.matchemphys.2010.10.004 ↗
2. Route toward semiconductor magnonics: light-induced spin-wave nonreciprocity in a YIG/GaAs structure10.1103/PhysRevB.99.054424 ↗
3. Nonlinear spin wave effects in the system of lateral magnonic structures10.1134/S0021364018010113 ↗
4. Spin-wave intermodal coupling in the interconnection of magnonic units10.1063/1.5027057 ↗
5. Aqueous gelcasting of yttrium iron garnet10.1016/j.jeurceramsoc.2012.11.002 ↗
6. Broadband TE optical isolators and circulators in silicon photonics through Ce: YIG bonding10.1109/JLT.2019.2896650 ↗
7. Effect of Bi2O3 on structure and wetting studies of Bi2O3–ZnO–B2O3 glasses10.1016/j.jallcom.2011.03.087 ↗
8. Enhanced bonding strength of Al2O3/AlN ceramics joined via glass frit with gradient thermal expansion coefficient10.1016/j.ceramint.2020.02.050 ↗
9. Ceramics bonding using solder glass frit10.1007/s11664-004-0093-y ↗
10. Microstructure and properties of SiCf/SiC joint brazed by Y-Al-Si-O glass10.1016/j.ceramint.2018.02.092 ↗
11. Low-temperature brazing of alumina ceramics with bismuth-borate glass in air10.1016/j.matchar.2019.01.020 ↗
12. Customized glass sealant for ceramic substrates for high temperature electronic application10.1016/j.microrel.2014.07.005 ↗
13. Microstructure and mechanical properties of tempered glass joint bonded with Bi-B-Zn low melting glass10.1016/j.jmatprotec.2019.02.017 ↗
14. Influence of whisker-aspect-ratio on densification, microstructure and mechanical properties of Al2O3 whiskers-reinforced CeO2-stabilized ZrO2 composites10.1016/j.jeurceramsoc.2017.11.037 ↗
15. Preparation and properties of in-situ mullite whiskers reinforced aluminum chromium phosphate wave-transparent ceramics10.1016/j.jeurceramsoc.2017.05.055 ↗
16. Microstructural evolution of Li-Ti ferrite/composite braze/Li-Ti ferrite joints reinforced by Bi5(Ti3Fe)O15 whiskers10.1016/j.jeurceramsoc.2016.06.039 ↗
17. Microstructure and properties of YIG/bismuth-based composite glass/YIG joints with growth of in situ MgFe2O4 whiskers10.1016/j.matchar.2020.110593 ↗
18. Structural phase stability and magnetism in Co2FeO4 spinel oxide10.1016/j.solidstatesciences.2008.10.012 ↗
19. Sol-gel synthesis of MnxNi1-xCo2O4 spinel phase materials: structural, electronic, and magnetic properties10.1016/j.jallcom.2018.01.139 ↗
20. Structural and morphological characterization of FeCo2O4 and CoFe2O4 spinels prepared by a coprecipitation method10.1016/S1293-2558(03)00011-6 ↗
21. Microstructure evolution and properties of dielectric magnesium titanate ceramic joints fabricated with bismuth glasses10.1016/j.ceramint.2020.08.070 ↗
22. Influence of Al2O3 whisker concentration on mechanical properties of WC-Al2O3 whisker composite10.1016/j.ceramint.2015.07.167 ↗
23. Flexural fracture mechanisms and fatigue behaviors of Bi4Ti3O12-based high-temperature piezoceramics sintered at different temperatures10.1016/j.ceramint.2018.06.107 ↗
24. Mechanical properties of polypropylene by diversely compatibilizing with titanate whiskers in composites10.1016/j.compscitech.2018.05.036 ↗
25. Improved dispersion of SiC whisker in nano hydroxyapatite and effect of atmospheres on sintering of the SiC whisker reinforced nano hydroxyapatite composites10.1016/j.msec.2018.05.003 ↗
26. Improved fracture toughness of laminated ZrB2-SiC-MoSi2 ceramics using SiC whisker10.1016/j.ceramint.2018.02.078 ↗
27. Fracture toughness and R-curve behavior of laminated ZrB2–SiC/SiCw ceramic10.1016/j.jallcom.2018.12.304 ↗
28. Evolutionary mechanism of YBO3 whisker and its effect on the properties of YIG ferrite joint brazed by Bi2O3–B2O3–SiO2–ZnO glass10.1016/j.ceramint.2020.08.211 ↗
29. Dielectric properties and signature of multi-ferroelectricity in Co2FeO4: a structurally single phased and bi-phased spinel oxide10.1016/j.jallcom.2013.11.219 ↗
30. Improvement of mechanical and dielectric properties of PIP-SiCf/SiC composites by using Ti3SiC2 as inert filler10.1016/j.ceramint.2014.12.108 ↗
31. Tailoring of thermal and dielectric properties of LDPE-matrix composites by the volume fraction, density, and surface modification of hollow glass microsphere filler10.1016/j.compositesb.2013.10.029 ↗
32. Improved electromagnetic absorbing properties of Si3N4–SiC/SiO2 composite ceramics with multi-shell microstructure10.1016/j.jeurceramsoc.2013.03.021 ↗
33. Co–Ti- and Mn–Ti-substituted barium ferrite for electromagnetic property tuning and enhanced microwave absorption synthesized via mechanical alloying10.1007/s41779-017-0056-4 ↗