Abstract

Abstract Ti TiB2 composites were fabricated from powder mixtures via spark plasma sintering method. Mechanical behavior of the sintered composites were then investigated via both routine and nanoindentation methods. Results indicated a significant increase in ultimate tensile strength and hardness of the composite, when the sintering temperature is raised. Besides common increase in the relative density of the composite, such a behavior was also attributed to the higher amounts of in-situ formed TiB whiskers. The remarkable reduction in bending strength is probably due to limited formability of unreacted coarse TiB2 particles and agglomerated in-situ formed phases. Such findings were then discussed in detail, based on the nanomechanical behavior of the primary and in-situ formed phases in Ti TiB2 composite sintered at 1200 °C. It was concluded that the superiority of mechanical properties in the mentioned sample may be due to high strength primary and in-situ formed reinforcements distributed homogenously in the matrix. Such reinforcement also provided high strength interfaces, according to interfacial nanoindentation approaches.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Metal and Thin Film Mechanics · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Effects of sintering temperature on microstructure and mechanical properties of spark plasma sintered titanium10.1016/j.matchemphys.2017.09.069 ↗
2. In situ observation of fracture behavior of in situ TiBw/Ti composites10.1016/j.msea.2004.04.071 ↗
3. In situ (TiBw + TiCp)/Ti6Al4V composites with a network reinforcement distribution10.1016/j.msea.2010.07.025 ↗
4. Microstructure and mechanical properties of in-situ synthesized TiB whiskers reinforced titanium matrix composites by high-velocity compaction10.1016/j.powtec.2014.07.048 ↗
5. Effects of in-situ formed TiB whiskers on microstructure and mechanical properties of spark plasma sintered Ti–B4C and Ti–TiB2 composites
6. Effects of sintering parameters on the microstructure and tensile properties of in situ TiBw/Ti6Al4V composites with a novel network architecture10.1016/j.matdes.2011.02.023 ↗
7. Effect of aspect ratios of in situ formed TiB whiskers on the mechanical properties of TiBw/Ti–6Al–4V composites10.1016/j.scriptamat.2011.12.024 ↗
8. Microstructural development and mechanical properties of hot pressed SiC reinforced TiB2 based composite10.1016/j.ijrmhm.2015.03.014 ↗
9. Densification and microstructural studies of titanium–boron carbide (B4C) powder mixture during spark plasma sintering10.1016/j.powtec.2014.05.050 ↗
10. Evolution of microstructural characteristic and tensile properties during preparation of TiB/Ti composite sheet10.1016/j.matdes.2011.11.060 ↗
11. Formation of equiaxed alpha and titanium nitride precipitates in spark plasma sintered TiB/Ti–6Al–4V composites10.1016/j.matlet.2012.05.132 ↗
12. Evolution of microstructure and tensile properties of in situ titanium matrix composites with volume fraction of (TiB + TiC) reinforcements10.1016/j.msea.2012.04.004 ↗
13. Effect of TiB2 content on the characteristics of spark plasma sintered Ti–TiBw composites10.1016/j.apt.2017.03.028 ↗
14. Spark plasma sintering reaction synthesized TiB reinforced titanium matrix composites10.1016/j.compositesa.2004.09.003 ↗
15. Microstructural characterisation and mechanical properties of spark plasma-sintered TiB2-reinforced titanium matrix composite10.1080/00325899.2016.1265805 ↗
16. Effects of spark plasma sintering temperature on densification, hardness and thermal conductivity of titanium carbide10.1016/j.ceramint.2018.05.071 ↗
17. Microstructure and mechanical properties of in situ TiB reinforced titanium matrix composites based on Ti–FeMo–B prepared by spark plasma sintering10.1016/j.compscitech.2004.05.013 ↗
18. Investigation of the Young's modulus of TiB needles in situ produced in titanium matrix composite10.1016/S0921-5093(02)00188-0 ↗
19. Spark plasma sintering of TiAl–Ti3AlC2 composite10.1016/j.ceramint.2018.08.272 ↗
20. Critical review of analysis and interpretation of nanoindentation test data10.1016/j.surfcoat.2005.03.018 ↗
21. Elastic modulus of biomedical titanium alloys by nano-indentation and ultrasonic techniques—a comparative study10.1016/j.msea.2007.12.029 ↗
22. A review of nanoindentation continuous stiffness measurement technique and its applications10.1016/S1044-5803(02)00192-4 ↗
23. Densification improvement of spark plasma sintered TiB2-based composites with micron-, submicron- and nano-sized SiC particulates10.1016/j.ceramint.2018.03.202 ↗
24. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology10.1557/jmr.2004.19.1.3 ↗
25. Elastic properties of titanium monoboride measured by nanoindentation10.1111/j.1551-2916.2006.01280.x ↗
26. Microstructural development during spark plasma sintering of ZrB2–SiC–Ti composite10.1016/j.ceramint.2018.07.011 ↗
27. Estimation of distinctive mechanical properties of spark plasma sintered titanium–titanium boride composites through nano-indentation technique
28. Material behavior of the hexagonal alpha phase of a titanium alloy identified from nanoindentation tests10.1016/j.euromechsol.2010.11.001 ↗
29. Characterization of interfacial mechanical properties in carbon fiber/aluminium matrix composites by the nanoindentation technique10.1016/j.compscitech.2005.04.013 ↗
30. Nanoindentation studies of titanium single crystals10.1016/S0142-9612(98)00257-9 ↗
31. A nano-indentation study on the mechanical behaviour of the matrix material in an AA6061 - Al2O3 MMC10.1023/A:1013896032331 ↗
32. Characterization of deformation anisotropies in an a-Ti alloy by nanoindentation and electron microscopy10.1016/j.actamat.2013.05.005 ↗
33. Study of particle–matrix interaction in Al/AlB2 composite via nanoindentation10.1016/j.matchar.2009.11.002 ↗
34. Prawoto · 2017
35. Prawoto · 2013
36. Dynamic recrystallization in commercially pure titanium
37. Dry reciprocating sliding wear behavior and mechanisms of bulk metallic glass composites10.1016/j.wear.2016.01.003 ↗
38. Electrochemical and friction characteristics of metallic glass composites at the microstructural length-scales10.1038/s41598-018-19488-7 ↗