Enhancing the mechanical and tribological properties of Mg2Si-rich aluminum alloys by multi-pass friction stir processing
Source abstract
Abstract
Abstract Particle strengthening of in-situ Al-Mg2Si composites hinges on effective geometrical parameters (size, distribution, morphology, and volume fraction) of the inherent primary Mg2Si particles. The use of solid-state friction stir processing (FSP) in a multi-pass mode is recognized as a secondary processing route capable of achieving desirable geometrical parameters of Mg2Si particles in Al-Mg2Si composites as compared to other routes. This paper thus studies the microstructure, mechanical properties, and tribological behavior of the multi-pass FSPed in-situ Al-25Mg2Si composite with a threaded triangular pin tool. The FSP was conducted at constant tool rotational and traverse speeds of 1000 rpm and 80 mm/min for 1–6 passes. The results showed a decline in the average Mg2Si size (115–3.25 μm), porosity content (5.8–0.14%), and primary Mg2Si particle-depleted region as the FSP passes are increased (0–6). Improved geometrical parameters of the primary Mg2Si particles enhance microhardness (178–272 HV), tensile strength (102–233 MPa) and wear resistance of the Al-25%Mg2Si composite via particle dispersion and dislocation strengthening effects, grain refinement, and microstructural densification. Multi-pass FSP can be adopted as a better substitute to element addition, casting modification, heat treatment and electromagnetic stirring in effectively controlling the geometrical parameters of the primary Mg2Si in in-situ Al-Mg2Si composites for improved mechanical and tribological properties.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Effect of Fe-impurity on tribological properties of Al−15Mg2Si composite10.1016/S1003-6326(18)64744-2 ↗
2. Effect of ultrasonic on morphology of primary Mg2Si in in-situ Mg2Si/Al composite10.1016/S1003-6326(13)62806-X ↗
3. Effects of the addition of lanthanum and ultrasonic stirring on the microstructure and mechanical properties of the in situ Mg2Si/Al composites10.1016/j.matdes.2015.10.159 ↗
4. Role of Sr on microstructure, mechanical properties, wear and corrosion behavior of an Al–Mg2Si–Cu in-situ composite10.1016/j.matchemphys.2019.121954 ↗
5. Microstructure and mechanical properties of Al−Mg2Si composite fabricated in-situ by vibrating cooling slope10.1016/S1003-6326(18)64693-X ↗
6. Microstructure and mechanical properties of high-pressure-assisted solidification of in situ Al–Mg2Si composites10.1016/j.msea.2018.07.032 ↗
7. Effect of superheating melt treatment on Mg2Si particulate reinforced in Al-Mg2Si-Cu in situ composite10.1016/j.proeng.2017.04.144 ↗
8. Microstructural characteristics of Mg2Si/Al composite under different superheat and electromagnetic stirring10.1016/S1875-5372(15)30042-4 ↗
9. Compressive creep behavior of a cast Al–15Mg2Si in-situ composite10.1016/j.msea.2016.05.058 ↗
10. Effect of hot extrusion on microstructural evolution and tensile properties of Al-15%Mg2Si-xGd in-situ composites10.1016/j.jallcom.2018.04.131 ↗
11. Microstructure and corrosion behavior of Al–10%Mg2Si cast alloy after heat treatment10.1016/j.matchar.2016.10.027 ↗
12. The effect of La-intermetallic compounds on tensile properties of Al-15%Mg2Si in-situ composite10.1016/j.mspro.2015.11.085 ↗
13. Effect of La inoculation on composition, content, granularity and mechanical properties of in-situ Al-30wt%Mg2Si Composite10.1016/j.msea.2017.08.010 ↗
14. Effect of in-situ TiB2 particles on microstructure and mechanical properties of Mg2Si/Al composites10.1016/j.jallcom.2018.10.301 ↗
15. Corrosion behavior of Al–Mg2Si alloys with/without addition of Al–P master alloy10.1016/j.matchar.2015.10.028 ↗
16. Effect of gadolinium addition on microstructural evolution and solidification characteristics of Al-15%Mg2Si in-situ composite10.1016/j.matchar.2017.10.018 ↗
17. Machinability characteristics, thermal and mechanical properties of Al-Mg2Si in-situ composite with Bismuth10.1016/j.measurement.2017.06.028 ↗
18. Effect of primary and eutectic Mg2Si crystal modifications on the mechanical properties and sliding wear behaviour of an Al–20Mg2Si–2Cu–xBi composite10.1016/j.jmst.2016.01.014 ↗
19. The influence of multipass friction stir processing on the corrosion behavior and mechanical properties of zircon-reinforced Al metal matrix composites10.1016/j.msea.2016.05.056 ↗
20. Simulation of strain rate, material flow, and nugget shape during dissimilar friction stir welding of AA6061 aluminum alloy and Al-Mg2Si composite10.1016/j.jallcom.2018.03.145 ↗
21. Microstructure and mechanical properties of friction stir welded Al/Mg2Si metal matrix cast composite10.1016/j.matdes.2010.07.008 ↗
22. Effect of tool pin profile on the microstructure and tribological properties of friction stir processed Al-20wt% Mg2Si composite10.1115/1.4044672 ↗
23. Correlating the microstructure to mechanical properties and wear behavior of an accumulative back extruded Al-Mg2Si in-situ composite10.1016/j.triboint.2017.05.034 ↗
24. Influence of multi-pass FSP on the microstructure, mechanical properties and tribological characterization of Al/B4C composite fabricated by accumulative roll bonding (ARB)10.1016/j.surfcoat.2019.01.043 ↗
25. High temperature tensile properties of centrifugally cast in-situ Al-Mg2Si functionally graded composites for automotive cylinder block liners10.1016/j.jallcom.2017.06.306 ↗
26. Understanding the role of welding parameters and tool profiles on the morphology of expelled flash of spot welds10.1016/j.matdes.2016.07.013 ↗
27. Microstructures of dissimilar friction stir welded joints between 2024-T4 aluminum alloy and Al/Mg2Si metal matrix cast composite10.1016/j.compositesb.2011.05.025 ↗
28. Microstructural and tribological properties of Al5083 based surface hybrid composite produced by friction stir processing10.1016/j.wear.2012.01.009 ↗
29. Microstructure and texture evolution of friction stir welded dissimilar aluminum alloys: AA2024 and AA606110.1016/j.jmapro.2018.01.016 ↗
30. Evaluation of dynamic development of grain structure during friction stir welding of pure copper using a quasi in situ method10.1016/j.jmst.2019.01.018 ↗
31. Mechanical properties and wear behavior of AA5182/WC nanocomposite fabricated by friction stir welding at different tool traverse speeds10.1007/s11665-018-3297-7 ↗
32. Dissimilar friction stir welding of 7075 aluminum alloy to AZ31 magnesium alloy using SiC nanoparticles
33. Fabrication of in situ Cu/SiC composites using multi-pass friction stir processing: evaluation of microstructural, porosity, mechanical and electrical behavior10.1016/j.compositesa.2011.06.010 ↗
34. Grain structure formation during friction stir welding observed by the ‘stop-action technique’10.1016/j.actamat.2005.03.044 ↗
35. Thermal history analysis and structure-property validation of friction stir welded Al-7079-TiC in-situ metal matrix composites10.1016/j.jallcom.2019.152131 ↗
36. Fabrication of in situ carbon fiber/aluminum composites via friction stir processing: evaluation of microstructural, mechanical and tribological behaviors10.1016/j.compositesb.2017.12.001 ↗
37. Through-thickness inhomogeneity in microstructure and tensile properties and tribological performance of friction stir processed AA1050-Al2O3 nanocomposite10.1016/j.compositesb.2019.107061 ↗
38. Relationship of Mg2Si morphology with Mg2Si content and its effect on properties of in-situ Mg2Si/Al-Cu composites10.1016/j.jallcom.2019.151771 ↗
39. Effect of hot extrusion on wear properties of Al–15 wt.% Mg2Si in situ metal matrix composites10.1016/j.matdes.2013.07.084 ↗