Abstract
Abstract The corrosion behavior of Ni–P deposits with the phosphorous contents of 20, 24 and 28 at.% (denoted as Ni–20P, Ni–24P, and Ni–28P, respectively) and annealed in air at different temperatures was systemically compared in a brine medium containing 3 wt.% NaCl. The anticorrosive properties of these Ni–P deposits were further examined in a brine-fog test (using a 5 wt.% NaCl solution) under 37 °C for 24 h. In the electrochemical studies, the Ni–28P deposit showed the lowest corrosion rate when it has been annealed between 200 and 300 °C. This deposit also exhibited the highest corrosion resistance in the studies of linear sweep voltammetry (LSV) and electrochemical impedance spectroscopy (EIS). In the brine-fog study, the weight loss of the Ni–P deposits was found to decrease with increasing the phosphorous content. After the brine-fog test, there was no obvious change in morphologies for all Ni–P deposits with the annealing treatment at 300 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Electrodeposition and Electroless Coatings · Electrochemical Analysis and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Bakonyi · Z. Metallkd. · 1996 · 77 · 425
2. Dietz · J. Phys. · 1990 · 2 · 2196
3. Lin · J. Electrochem. Soc. · 1989 · 136 · 380310.1149/1.2096552 ↗
4. Zeller · Corrosion · 1994 · 50 · 45710.5006/1.3293524 ↗
5. Garcia-Alonso · Corros. Sci. · 1996 · 38 · 51510.1016/0010-938X(96)00151-5 ↗
6. Lo · J. Electrochem. Soc. · 1995 · 142 · 9110.1149/1.2043954 ↗
7. Duncan · Plat. Surf. Finish. · 1986 · 73 · 52
8. Sha · J. Alloy Compd. · 1992 · 182 · L110.1016/0925-8388(92)90568-T ↗
9. Zou · Surf. Coat. Technol. · 1988 · 36 · 45510.1016/0257-8972(88)90173-9 ↗
10. Gillot · J. Alloy Compd. · 1992 · 189 · 15110.1016/0925-8388(92)90699-A ↗
11. Bozzini · Spcripta Mater. · 1997 · 36 · 124510.1016/S1359-6462(97)00032-8 ↗
12. B. Bozzini, P.L. Cavallotti, A. Buratti, F. Kruger, Proceedings of the Interfinish’92, Sao Paulo, Brazil, 1992, p. 156.
13. Bozzini · Wear · 1999 · 225–229 · 80610.1016/S0043-1648(98)00389-5 ↗
14. Kreye · Metalloberfläche. · 1993 · 47 · 387
15. Boylan · Scripta Metall. Mater. · 1991 · 25 · 271110.1016/0956-716X(91)90144-P ↗
16. Lu · Electrochim. Acta · 2002 · 47 · 296910.1016/S0013-4686(02)00198-6 ↗
17. Kreye · Z. Metallkd. · 1992 · 83 · 449
18. He · Surf. Coat. Technol. · 1992 · 53 · 9310.1016/0257-8972(92)90108-M ↗
19. Delplancke · J. Electrochem. Soc. · 1993 · 140 · 280010.1149/1.2220913 ↗
20. Yamamoto · Jpn. J. Appl. Phys. · 1993 · 32 · 358610.1143/JJAP.32.3586 ↗
21. Hu · Surf. Coat. Technol. · 2001 · 137 · 18110.1016/S0257-8972(00)01117-8 ↗
22. Hu · Mater. Chem. Phys. · 2002 · 77 · 21510.1016/S0254-0584(01)00592-2 ↗
23. Hu · J. Appl. Electrochem. · 2001 · 31 · 56510.1023/A:1017525507665 ↗
24. Hu · Mater. Chem. Phys. · 2003 · 79 · 4910.1016/S0254-0584(02)00455-8 ↗
25. M. Pourbaix, Atlas of Electrochemical Equilibria in Aqueous Solutions, National Association of Corrosion Engineers, Houston, TX, 1966.
26. Paseka · Electrochim. Acta · 1995 · 40 · 164110.1016/0013-4686(95)00077-R ↗
27. Hu · J. Electroanal. Chem. · 2001 · 503 · 10510.1016/S0022-0728(01)00385-0 ↗
28. Angelo · J. Electrochem. Soc. · 1995 · 142 · 331310.1149/1.2049980 ↗