Characterization of W–20Cu ultrafine composite powder prepared by spray drying and calcining-continuous reduction technology
Source abstract
Abstract
Abstract W–20Cu ultrafine composite powder, whose average grain size was about 500 nm, was fabricated by spray drying and calcining-continuous reduction technology. In the W–20Cu ultrafine powder the nanocrystalline Cu grain can wet W grain by the CuO transitional layer, the special non-metal–metal nanocomposite structure would play very important roles in obtaining W–Cu alloy with good mechanical properties, thermal conductivity and homogeneous microstructure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Powder Metallurgy Techniques and Materials · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. Thermal conductivity of W–Cu composites at various temperatures10.1016/S0167-577X(01)00330-5 ↗
2. Microstructure and sintering behavior of W–Cu nanocomposite powder produced by thermo-chemical process10.1016/S0263-4368(02)00003-3 ↗
3. Fabrication of W–20wt% Cu composite nanopowder and sintered alloy with high thermal conductivity10.1016/S0167-577X(03)00071-5 ↗
4. Segregation of Fe during the sintering of doped W–Cu alloys10.1016/S1359-6462(03)00244-6 ↗
5. The initial stage of sintering for the W–Cu nanocomposite powder prepared from W–CuO mixture10.1016/j.matlet.2003.07.044 ↗
6. Apparent viscosity of W–Cu powder compacts during sintering10.1016/j.msea.2004.05.050 ↗
7. Mechanical properties, phases and microstructure of ultrafine hardmetals prepared by WC–6.29Co nanocrystalline composite powder10.1016/j.msea.2004.09.043 ↗
8. Viscosity and thermal conductivity of copper oxide nanofluid dispersed in ethylene glycol