Structural, mechanical and tribological behavior of TiCN, CrAlN and BCN coatings in lubricated and non-lubricated environments in manufactured devices
Source abstract
Abstract
Abstract This paper presents the structural, mechanical and tribological behaviors for AISI 1045 steel uncoated and coated with Titanium Carbo-nitride (TiCN), Aluminum Chrome Nitride (CrAlN) and Boron Carbo-nitride (BCN) under lubricated and non-lubricated environments. The coating's natural effect on the crystalline structure, chemical composition, as well as the mechanical properties were determined by X-ray diffraction (XRD), X-ray photo-electron spectroscopy (XPS), atomic force microscopy (AFM), scanning electron microscopy (SEM), nanoindentation and tribological characterization techniques. The results show that the material with the lowest elastic modulus was TiCN (224 GPa), followed by CrAlN (235 GPa), and the BCN (251 GPa). The friction coefficient results for the coatings without lubrication were 0.74, 0.66 and 0.60, respectively, and with lubrication were 0.24, 0.23 and 0.21, respectively. These results indicate that the tribological properties are strongly dependent on the lubricated environment's nature and the coating's nature. Advanced surface treatments are increasingly used in the daily manufacture of parts for the metalworking and automotive industry due to high mechanical and tribological requirements; therefore, TiCN, CrAlN and BCN coatings can be used as future materials for elements subject to high stress and wear in lubricated environments.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Diamond and Carbon-based Materials Research · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. TiCN/TiNbCN multilayer coatings with enhanced mechanical properties10.1016/j.apsusc.2010.03.071 ↗
2. Magnetron sputtering of tin protective coatings for medical applications10.1016/0924-0136(95)01856-5 ↗
3. “Carbon-containing Ti–C:H and Cr–C:H PVD hard coatings10.1016/S0042-207X(02)00748-0 ↗
4. Synthesis and characterization of Ti-cx-N1-x coatings prepared by arc ion plating
5. “Microstructure, micro-mechanical and tribological properties of the nc-WC/a-C nanocomposite coatings magnetron sputtered on non-hardened and oxygen hardened Ti – 6Al – 4V alloy10.1016/j.surfcoat.2010.10.039 ↗
6. Design of hard surfaces with metal (Hf/V) nitride multinanolayers10.3103/S1063457614060021 ↗
7. Mechanical, tribological and electrochemical behavior of Cr1-xAlxN coatings deposited by r.f . reactive magnetron co-sputtering method10.1016/j.apsusc.2009.10.071 ↗
8. Deposition and characterization of CrN/Si3N4 and CrAlN/Si3N4 nanocomposite coatings prepared using reactive DC unbalanced magnetron sputtering10.1016/j.surfcoat.2007.04.002 ↗
9. Influence of the microestructure on the electrochemical porperties of Al-Cr-N coatings deposited by Co-sputtering method from a Cr-Al binary target10.1590/S1516-14392012005000171 ↗
10. Protective properties of the chromium-titanium carbonitride composite coatings10.1016/S0257-8972(03)00716-3 ↗
11. Effects of PVD sputtered coatings on the corrosion resistance of AISI 304 stainless steel10.1016/S0921-5093(02)99999-5 ↗
12. Effects of the thickness of Ti buffer layer on the mechanical properties of TiN coatings10.1016/S0257-8972(03)00243-3 ↗
13. Arc-evaporated CrN , CrN and CrCN coatings10.1016/j.vacuum.2008.05.005 ↗
14. Characterization of Zr-based hard coatings for medical implant applications10.1016/j.surfcoat.2009.11.022 ↗
15. Structural, mechanical and electrochemical comparison of TiN and TiCN coatings on XC48 steel substrates in NaCl 3.5% water solution10.1016/j.apsusc.2014.04.167 ↗
16. Mechanical and electrochemical characterization of vanadium nitride (VN) thin films10.1016/j.apsusc.2011.08.057 ↗
17. Thermal induced structural changes of a-C and a-C:Ti films analized by NEXAFS and XPS
18. Oxidation tuning in AlCrN coatings10.1016/j.surfcoat.2006.09.089 ↗
19. Structure and properties of pulsed-laser deposited carbon nitride thin films10.1016/j.tsf.2005.09.172 ↗
20. Evolution of physical properties in hafnium carbonitride thin films10.1016/j.jallcom.2016.08.109 ↗
21. 2017 · 1
22. 2017 · 1
23. Structure evolution and properties of TiAlCN/VCN coatings deposited by reactive HIPIMS10.1016/j.surfcoat.2014.07.065 ↗
24. Evidence of electrochemical resistance on ternary V-C-N layers10.1007/s12633-018-9782-7 ↗
25. Synthesis and characterization of CNx/TiN multilayers on Si(100) substrates10.1016/j.surfcoat.2004.10.015 ↗
26. Síntesis y caracterización de nanoestructuras estequiométricas de nitruro de boro
27. A practical application of X-ray spectroscopy in Ti-Al-N and Cr-Al-N thin films
28. Pierson · 1996 · 1
29. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗
30. On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimised tribological behaviour10.1016/S0043-1648(00)00488-9 ↗
31. Microtribological characterization of group V and VI metal-carbide wear-resistant coatings effective in the metal casting industry10.1016/S0257-8972(00)00948-8 ↗