Influence of MgO whisker addition on microstructures and mechanical properties of WC-MgO composite
Source abstract
Abstract
Abstract WC-MgO whisker composite (abbreviated as WC-MgOw composites) has been sintered by hot pressing. The purpose of present study is to investigate the influence of various content of MgO whisker addition on mechanical performance of WC-MgOw composites. Vickers hardness and fracture toughness of WC-MgOw composites first increase and then decrease with the addition of MgO whisker. The optimal values of Vickers hardness and fracture toughness are achieved, respectively 20.92 GPa and 9.85 MPa m1/2, when the MgO whiskers content reaches 1 wt%. The fracture toughness of WC-MgOw composite is about higher 10.2% than the sample's without MgO whiskers. However, the relative density of the WC-MgOw composites decreases continuously with the addition of MgO whiskers. When the content of MgO whisker is relatively high, the fracture mode is changed and large pores appear. Thus, the mechanical properties of WC-MgOw composite is decreased. The main toughening mechanisms can attribute to crack deflection, crack bridging and whisker pull-out. The mixture of intergranular and transgranular fracture mode also increase the fracture toughness.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Powder Metallurgy Techniques and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Grain size optimization for nanoscale tungsten carbide cobalt using master sintering curve model10.1016/j.ijrmhm.2017.12.034 ↗
2. Multi-layer graphene reinforced nano-laminated WC-Co composites10.1016/j.msea.2018.03.040 ↗
3. Complexions in WC-Co cemented carbides10.1016/j.actamat.2018.02.018 ↗
4. Synthesis, sintering, and mechanical properties of nanocrystalline cemented tungsten carbide – a review10.1016/j.ijrmhm.2008.07.011 ↗
5. Consolidation and properties of binderless sub-micron tungsten carbide by field-activated sintering10.1016/j.ijrmhm.2004.08.003 ↗
6. Consolidation of ultra fine WC and WC–Co hard materials by pulsed current activated sintering and its mechanical properties10.1016/j.ijrmhm.2005.11.004 ↗
7. Corrosion properties of Co-based cemented carbides in acidic solutions10.1016/S0263-4368(03)00027-1 ↗
8. Study of processing routes for WC-MgO composites with varying MgO contents consolidated by FAST/SPS10.1016/j.jeurceramsoc.2017.01.005 ↗
9. Influence of Ni and ZrO2 contents on sintering and mechanical properties of WC-2wt.%ZrO2-1wt.%Ni composites10.1016/j.ceramint.2019.02.198 ↗
10. Microstructure and characterization of WC-2.8wt% Al2O3-6.8wt% ZrO2 composites produced by spark plasma sintering10.1016/j.ceramint.2016.06.044 ↗
11. Fabrication of nanocrystalline WC and nanocomposite WC–MgO refractory materials at room temperature10.1016/S0925-8388(99)00508-3 ↗
12. Corrosion and corrosive wear behavior of WC–MgO composites with and without grain-growth inhibitors10.1016/j.jallcom.2014.06.137 ↗
13. Two-step hot-pressing sintering of nanocomposite WC–MgO compacts10.1016/j.jeurceramsoc.2011.04.001 ↗
14. VC and Cr3C2 doped WC–MgO compacts prepared by hot-pressing sintering10.1016/j.matdes.2012.04.030 ↗
15. Lawn · 1993
16. 4.19 - particle and whisker reinforced brittle matrix composites
17. Study of the mechanical properties, toughening and strengthening mechanisms of Si3N4/Si3N4w/TiN nanocomposite ceramic tool materials10.1016/j.actamat.2007.03.016 ↗
18. Influence of SiC whisker morphology and nature of SiC/Al2O3 interface on thermomechanical properties of SiC reinforced Al2O3 composites10.1016/j.jeurceramsoc.2004.09.026 ↗
19. Effect of SiC nano-whisker addition on WC–Ni based cemented carbides fabricated by hot-press sintering10.1016/j.ijrmhm.2012.10.009 ↗
20. Spark plasma sintering and hot pressing of ZrB2–SiCw ultra-high temperature ceramics10.1016/j.jallcom.2007.11.018 ↗
21. High temperature mechanical properties of Al2O3-based ceramic tool material toughened by SiC whiskers and nanoparticles10.1016/j.ceramint.2016.10.057 ↗
22. Effect of multi-walled carbon nanotubes on microstructure and fracture properties of carbon fiber-reinforced ZrB2-based ceramic composite10.1016/j.ceramint.2017.03.018 ↗
23. Preparation of MgO whisker from magnesite tailings and its application10.1016/S1003-6326(11)60973-4 ↗
24. Strengthening and toughening of poly(L-lactide) composites by surface modified MgO whiskers10.1016/j.apsusc.2015.01.167 ↗
25. Effects of MgO whiskers on mechanical properties and crystallization behavior of PLLA/MgO composites10.1016/j.matdes.2015.09.157 ↗
26. Indentation fracture of WC-Co cermets10.1007/BF00555296 ↗
27. Colloidal processing of SiC whisker composites10.1111/j.1151-2916.1995.tb08646.x ↗
28. Development of advanced composite ceramic tool material10.1016/S0025-5408(96)00078-5 ↗
29. Fabrication and mechanical properties of Al2O3-SiCw-TiCnp ceramic tool material10.1016/j.ceramint.2017.05.049 ↗
30. Synergistically toughening effect of SiC whiskers and nanoparticles in Al2O3-based composite ceramic cutting tool material10.3901/CJME.2016.0411.049 ↗
31. In-situ fabricated TiB2 particle-whisker synergistically toughened Ti(C, N)-based ceramic cutting tool material10.3901/JME.2015.01.001 ↗
32. Bulk WC–Al2O3 composites prepared by spark plasma sintering10.1016/j.ijrmhm.2011.07.003 ↗
33. Fabrication and properties of silver-matrix composites reinforced by carbon nanotubes10.1016/j.matchar.2005.05.003 ↗
34. Effect of SiC whisker addition on the microstructures and mechanical properties of Ti(C, N)-based cermets10.1016/j.matdes.2010.07.028 ↗
35. 4.04–Toughening mechanisms in short fiber and particle toughened ceramics10.1016/B0-08-042993-9/00089-9 ↗
36. Fracture toughness predictions for crack bowing in brittle particulate composites10.1111/j.1151-2916.1983.tb09975.x ↗
37. The effect of residual stress on whisker reinforcements in SiCw-Al2O3 composites during cooling10.1016/j.jallcom.2017.07.192 ↗
38. Crack bridging by uncracked ligaments during fatigue-crack growth in SiC-reinforced aluminum-alloy composites10.1007/BF02651656 ↗
39. Crack‐interface grain bridging as a fracture resistance I, mechanism in ceramics: I, experimental study on alumina10.1111/j.1151-2916.1987.tb04982.x ↗
40. Crack‐interface grain bridging as a fracture resistance mechanism in ceramics: II, theoretical fracture mechanics model10.1111/j.1151-2916.1987.tb04983.x ↗
41. Microstructure, mechanical properties and toughening mechanisms of graphene reinforced Al2O3-WC-TiC composite ceramic tool material10.1016/j.ceramint.2019.02.087 ↗
42. Strain-rate dependence of the compressive strength of WC–Co hard metals10.1016/j.msea.2014.06.020 ↗