In-situ observation of fluxless soldering of Sn-3.0Ag-0.5Cu/Cu under a formic acid atmosphere
Source abstract
Abstract
Abstract Formic acid, which can provide efficient reduction for most solders, is widely used in fluxless soldering. In this study, to establish a reliable fluxless soldering process, a formic acid atmosphere was used to reduce the oxides of Sn-3.0Ag-0.5Cu solders and Cu substrates. The wetting behavior of Sn-Ag-Cu solder balls on Cu pads under a formic acid atmosphere was observed in situ, and the wettability was investigated by evaluating the contact angle and spreading rate. We confirmed the effect of formic acid on the interfacial reaction between the solder and Cu substrate. After the fluxless soldering, impact tests were conducted on the formed solder bumps. The results indicate that the contact angle of solder under a formic acid atmosphere was similar to that of the solder using rosin mildly activated (RMA) liquid flux; however, its spreading rate was much lower than that using the RMA flux. Some residues were found around the solders formed under a formic acid atmosphere after the reflow process (the substrate turned gray), whereas the same area on the substrate remained clean when using the RMA flux. Some pores were observed near the intermetallic compound layers in the samples soldered under a formic acid atmosphere, but the pores barely affected the impact strength.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Adhesion, Friction, and Surface Interactions
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Lead-free solders in microelectronics10.1016/S0927-796X(00)00010-3 ↗
2. In search of new lead-free electronic solders10.1007/BF02651363 ↗
3. A review of mechanical properties of lead-free solders for electronic packaging10.1007/s10853-008-3125-9 ↗
4. Effect of Sn grain orientation on formation of Cu6Sn5 intermetallic compounds during electromigration10.1016/j.scriptamat.2016.09.028 ↗
5. A review: lead free solder and its wettability properties10.1108/SSMT-08-2015-0022 ↗
6. Flux effect on void quantity and size in soldered joints10.1016/j.microrel.2016.03.009 ↗
7. Effects of cosmic rays on atmospheric chlorofluorocarbon dissociation and ozone depletion10.1103/PhysRevLett.87.078501 ↗
8. Fluxless chip join process using formic acid atmosphere in a continuous mass reflow furnace
9. Problem with no-clean flux spattering on in-circuit testing pads diagnosed by EDS analysis10.1016/j.microrel.2015.10.020 ↗
10. Analysis of no-clean flux spatter during the soldering process10.1016/j.jmatprotec.2019.116289 ↗
11. Process development and reliability of sintered high power chip size packages and flip chip LEDs
12. Solder process for fluxless solder paste applications
13. Residual free solder process for fluxless solder pastes10.1108/SSMT-10-2017-0030 ↗
14. Study of fluxless soldering using formic acid vapor10.1109/6040.803451 ↗
15. Humpston · 2004
16. Formation of solder cap on Cu pillar bump using formic acid reduction
17. Development of fluxless flip chip reflow process for high density flip chip interconnect
18. Effect of substrate metallization on the impact strength of Sn-Ag-Cu solder bumps fabricated in a formic acid atmosphere
19. Low-pressure Cu-Cu bonding using in-situ surface-modified microscale Cu particles for power device packaging10.1016/j.scriptamat.2016.04.018 ↗
20. Pressureless sintering bonding using hybrid microscale Cu particle paste on ENIG, pure Cu and pre-oxidized Cu substrate by an oxidation–reduction process10.1007/s10854-016-6220-8 ↗
21. Study of Cu film surface treatment using formic acid vapor/solution for low temperature bonding10.1149/2.0121804jes ↗
22. Cu film surface reduction through formic acid vapor/solution for 3-D interconnection
23. Effect of substrates on fracture mechanism and process optimization of oxidation–reduction bonding with copper microparticles10.1007/s11664-019-07046-4 ↗
24. Effect of thermal aging on the impact strength of soldered bumps under formic acid atmosphere
25. Thermogravimetric investigation on the interaction of formic acid with solder joint materials10.1039/C6NJ02396G ↗
26. Contact angle temperature dependence for water droplets on practical aluminum surfaces10.1016/0017-9310(96)00184-6 ↗
27. Use of thermodynamic data to calculate surface tension and viscosity of Sn-based soldering alloy systems10.1007/s11664-001-0137-5 ↗
28. Viscosity and surface tension of liquid Sn-Cu lead-free solders10.1007/s11664-008-0611-4 ↗
29. Review of non-reactive and reactive wetting of liquids on surfaces10.1016/j.cis.2007.04.009 ↗
30. Knowledge about polymer surfaces from contact angle measurements10.1016/0001-8686(90)80012-O ↗
31. Rough ideas on wetting10.1016/S0378-4371(02)01033-6 ↗
32. Multiple equilibrium droplet shapes and design criterion for rough hydrophobic surfaces10.1021/la0268348 ↗
33. Contact angle hysteresis on rough hydrophobic surfaces10.1016/j.colsurfa.2004.09.006 ↗
34. Anisotropy in the wetting of rough surfaces10.1016/j.jcis.2004.07.038 ↗
35. Thermodynamic modeling of contact angles on rough, heterogeneous surfaces10.1016/j.cis.2005.07.004 ↗
36. Adamson · 1967 · 465
37. The relation between Young's equilibrium contact angle and the hysteresis on rough paraffin wax surfaces10.1016/S0927-7757(99)00079-5 ↗
38. Decomposition mechanism of formic acid on Cu (111) surface: a theoretical study10.1016/j.apsusc.2016.11.042 ↗
39. A combined process of formic acid pretreatment for low-temperature bonding of copper electrodes10.1149/2.010306jss ↗
40. Formic acid treatment with Pt catalyst for Cu direct bonding at low temperature
41. Effect of formic acid vapor in situ treatment process on Cu low-temperature bonding10.1109/TCPMT.2014.2315761 ↗
42. Direct bonding for dissimilar metals assisted by carboxylic acid vapor10.7567/JJAP.54.030217 ↗
43. Thermal desorption study of formic acid decomposition on a clean cu (110) surface10.1016/0021-9517(80)90338-3 ↗
44. XPS, UPS and thermal desorption studies of the reactions of formaldehyde and formic acid with the cu (110) surface10.1016/0039-6028(81)90045-5 ↗
45. An IRAS study of formic acid and surface formate adsorbed on Cu (110)10.1016/0039-6028(83)90021-3 ↗
46. Hosking · 2012
47. Formic acid adsorption and oxidation on Cu (1 1 0)10.1016/j.susc.2008.03.013 ↗
48. Formation of tin-based crystals from a SnAgCu alloy under formic acid vapor10.1039/C8NJ04173C ↗
49. Characterization of tin-oxides and tin-formate crystals obtained from SnAgCu solder alloy under formic acid vapor10.1039/C9NJ02135C ↗
50. Impact strength of Sn–3.0 Ag–0.5 Cu solder bumps during isothermal aging10.1016/j.microrel.2014.03.007 ↗
51. A review: on the development of low melting temperature Pb-free solders10.1016/j.microrel.2014.02.025 ↗
52. Effect of formic acid surface modification on bond strength of solid-state bonded interface of tin and copper10.2320/matertrans.MJ201019 ↗
53. Rozhitsina · 2011 · vol. 2011 · 118