Microstructure and properties characterization of Ti-containing Ni60/Graphite self-lubricating composite coatings applied on 300M ultra-high strength steel by laser cladding
Source abstract
Abstract
Abstract To improve the wear and corrosion resistance of 300M ultra-high strength (300M) steels, the Ni-based alloy (Ni60)/nickel-coated graphite composite coatings with the addition of titanium (Ti) were claded on 300M by laser. The microstructure, micro-hardness, tribological performance, corrosion resistance, thermal property, and dynamic mechanical property of the coatings were characterized. The cladding-layer microstructure of the Ti-containing (6 wt% Ti) coatings showed an equiaxial tendency. The microhardness of the Ti-containing coatings was higher and more homogeneous. The wear rate of the matrix was 29.4 times higher than that of Ti-containing composite coatings and was 2.4 times larger than that of the Ti-free (0 wt% Ti) composite coatings. However, the friction coefficient of the Ti-containing composite coatings was higher than that of the Ti-free composite coatings. The self-corrosion current densities of the Ti-containing, Ti-free composite coating and 300M were 0.25, 3.16 and 232.51 μA/cm2, respectively, indicating that the corrosion resistance of Ti-containing composite coatings was improved. The impact-resistance of the Ti-containing composite coatings was better than that of the Ti-free composite coatings.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Entropy Alloys Studies · Additive Manufacturing Materials and Processes · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Phase transformation in AISI 410 stainless steel10.1016/S0921-5093(01)01710-5 ↗
2. The growth behavior of austenite grain in the heating process of 300M steel10.1016/j.msea.2011.02.089 ↗
3. Aircraft landing gear greased slider bearing steady-state thermo-elastohydrodynamic concept model10.1016/j.triboint.2014.04.001 ↗
4. In-situ quench and tempering for microstructure control and enhanced mechanical properties of laser cladded AISI 420 stainless steel powder on 300M steel substrates10.1016/j.surfcoat.2017.10.080 ↗
5. A step towards safety: material failure analysis of landing gear
6. Hard chromium composite electroplating on high-strength stainless steel from a Cr (III)-ionic liquid solution10.1016/j.elecom.2019.106537 ↗
7. Influence of WC carbide particle size on the microstructure and abrasive wear behavior of WC–10Co–4Cr coatings for aircraft landing gear10.1016/j.wear.2016.05.022 ↗
8. Evaluation of WC-17Co and WC-10Co-4Cr thermal spray coatings by HVOF on the fatigue and corrosion strength of AISI 4340 steel10.1016/j.surfcoat.2004.08.181 ↗
9. Effects of tungsten carbide thermal spray coating by HP/HVOF and hard chromium electroplating on AISI 4340 high strength steel10.1016/S0257-8972(00)01148-8 ↗
10. Chromium isotope fractionations resulting from electroplating, chromating and anodizing: implications for groundwater pollution studies10.1016/j.apgeochem.2017.03.009 ↗
11. Investigations on ultra-high-speed laser material deposition as alternative for hard chrome plating and thermal spraying10.2351/1.4943910 ↗
12. Investigation into cadmium embrittlement of landing gear wheel axles10.1016/j.engfailanal.2004.12.040 ↗
13. Laser processing of bulk metallic glass: a review10.1016/j.jmatprotec.2017.03.034 ↗
14. Influence of Cu on microstructure and wear resistance of TiC/TiB/TiN reinforced composite coating fabricated by laser cladding10.1016/j.matchemphys.2012.01.082 ↗
15. Microstructural evolution and wear behaviors of laser-clad Stellite 6/NbC/h-BN self-lubricating coatings10.1016/j.surfcoat.2019.04.083 ↗
16. Laser cladding Ti-Ni/TiN/TiW+TiS/WS2 self-lubricating wear resistant composite coating on Ti-6Al-4V alloy10.1016/j.optlastec.2018.12.046 ↗
17. Study on laser cladding coatings of Ni-based alloy/TiC/Nickel-Coated graphite on steel substrate10.4028/www.scientific.net/KEM.450.214 ↗
18. Selective laser melting of stainless-steel/nano-hydroxyapatite composites for medical applications: microstructure, element distribution, crack and mechanical properties10.1016/j.jmatprotec.2015.02.010 ↗
19. Secant-shaped porous slider bearing lubricated with couple stress fluids10.1108/00368790510601716 ↗
20. Microstructures and corrosion resistance of Fe-based amorphous/nanocrystalline coating fabricated by laser cladding10.1016/j.jallcom.2017.08.251 ↗
21. Fatigue behavior of Zn-Ni and Cd coated AISI 4340 steel with scribed damage in saltwater environment10.1016/j.ijfatigue.2016.04.027 ↗
22. Application of Ultra-High-Speed Laser Cladding (UHSLC) for functional coatings deposition in aviation industry
23. Corrosion behaviour and galvanic coupling with steel of Al-based coating alternatives to electroplated cadmium10.1016/j.matchemphys.2013.04.035 ↗
24. Corrosion resistance improvement of 45 steel by Fe-based amorphous coating10.1016/j.vacuum.2018.03.042 ↗
25. Effect of laser cladding process parameters on clad quality and in situ formed microstructure of Fe-TiC composite coatings10.1016/j.surfcoat.2010.08.087 ↗
26. The effect of TiC/Al2O3 composite ceramic reinforcement on tribological behavior of laser cladding Ni60 alloys coatings10.1016/j.surfcoat.2016.02.033 ↗
27. Aircraft engineering and Aerospace Technology Cold spraying and laser cladding as an alternative to electroplating processes
28. Analysis and innovation for penetrant testing for airplane parts10.1016/j.proeng.2014.12.681 ↗
29. High-performance Ti composites reinforced with in-situ TiC derived from pyrolysis of polycarbosilane10.1016/j.msea.2020.139924 ↗
30. Synthesis and characterization of Ni60-hBN high temperature self-lubricating anti-wear composite coatings on Ti6Al4V alloy by laser cladding10.1016/j.optlastec.2015.10.005 ↗
31. Refinement and homogenization of M7C3 carbide in hypereutectic Fe-Cr-C coating by Y2O3 and TiC10.1016/j.matchar.2017.08.004 ↗
32. Refining effect of TiC on primary M7C3 in hypereutectic Fe-Cr-C harden-surface welding coating: experimental research and first principles calculation10.1016/j.jallcom.2016.08.133 ↗
33. Investigation of M7C3, M23C6 and M3C carbides synthesized on austenitic stainless steel and carbon fibers using laser metal deposition10.1016/j.surfcoat.2020.126294 ↗
34. Microstructure evolution, recrystallization and tribological behavior of TiC/WC composite ceramics coating10.1016/j.vacuum.2019.04.049 ↗
35. Laser cladding novel NiCrSiFeBW-CeO(2) coating with both high wear and corrosion resistance
36. Preparation and characterization of Ni-Cr nanocomposite coatings containing TiO2 nanoparticles for corrosion protection10.1108/00035591211274389 ↗
37. Direct and pulse current electrodeposition of Ni-W-TiO2 nanocomposite coatings10.1016/j.ceramint.2012.09.054 ↗
38. A computational study on the benefit of core-shell structured carbides to the erosion resistance of high-Cr cast irons10.1016/j.triboint.2016.08.001 ↗
39. Microstructure, wear, and corrosion characterization of high TiC content Inconel 625 matrix composites10.1016/j.jmrt.2018.09.001 ↗
40. Microstructures and properties of TiN reinforced Co-based composite coatings modified with Y2O3, by laser cladding on Ti-6Al-4V alloy10.1016/j.jallcom.2015.07.295 ↗
41. Investigation of laser cladding high temperature anti-wear composite coatings on Ti6Al4V alloy with the addition of self-lubricant CaF210.1016/j.apsusc.2014.05.196 ↗
42. Friction and wear behavior of tin films against ceramic and steel balls10.1016/j.triboint.2018.03.031 ↗
43. Tribological properties of Ni-base alloy composite coating modified by both graphite and TiC particles10.1016/S1003-6326(11)61031-5 ↗