Enhancement of electrical, mechanical and thermal properties of silicone based coating with aluminatrihydrate/silica for ceramic insulators
Source abstract
Abstract
The present work explores durability enhancement in various properties of room temperature vulcanized silicone rubber (RTV-SiR) coating with the incorporation of alumina trihydrate (ATH) and silica (SiO2) fillers. Test samples i.e., neat RTV-SiR, RTV-SiR +10% μSiO2, and RTV-SiR filled with micro-ATH/SiO2 (10% each) were chosen for experimentation. Long-term (10,000 h) lab aging of composite coatings is performed under bipolar direct current (DC) voltage with simulated environmental stresses in a test chamber. The effect of fillers against stresses is quantified through characterization results comparison of filled composites with unfilled RTV-SiR samples. Moreover, the polarity effect on degradation is evaluated through the relative performance of each composite under the positive and negative polarity of the voltage. Findings revealed that samples filled with a mixture of additives bring enhanced improvement into the base matrix of RTV-SiR. Amongst unfilled and micro-silica filled specimens aged under positive DC, the samples S-3 with combined silica-ATH fillers offered superior hydrophobic behavior showing hydrophobicity class HC3 and demonstrated a minimum final leakage current of 6.13 μA. Fourier transform infrared spectroscopy (FTIR) and scanning electron microscopy (SEM) results showed relatively lower variations in the chemical and morphological structure of cross-filed specimens (S-3). Furthermore, results of mechanical properties (tensile strength, elasticity, and weight) show a significant loss, whereas the hardness of composite increased with aging. Hybrid samples (S-3) exhibited the minimum deviation of 29.77% and 43.12% in tensile strength and elongation-at-break (EAB), respectively under positive DC voltage. Similarly, it shows enhanced resistance against weight loss and change in hardness due to aging. Moreover, thermogravimetric analysis (TGA) confirmed that filled composite gets enabled to offers the least alteration in thermal properties. In the context of the polarity, positive DC voltage incurred more devaluation of desirable properties as compared to negative polarity.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High voltage insulation and dielectric phenomena · Dielectric materials and actuators · Advanced Sensor and Energy Harvesting Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Comparison of surface pollution flashover characteristics of RTV (room temperature vulcanizing) coated insulators under different coating damage modes10.1109/ACCESS.2019.2907689 ↗
2. Pollution flashover characteristics of coated insulators under different profiles of coating damage10.3390/coatings11101194 ↗
3. Aging of silicone rubber-based composite insulators under multi-stressed conditions: an overview10.1088/2053-1591/ab3f0d ↗
4. Effect of AC corona discharge on hydrophobic properties of silicone rubber nanocomposites
5. Multi-stressed nano and micro-silica/silicone rubber composites with improved dielectric and high-voltage insulation properties10.3390/polym13091400 ↗
6. Hydrophobicity investigation and life estimation of silicone rubber nanocomposites
7. Review on RTV silicone rubber coatings insulator for transmission lines
8. Partial discharge performance improvement of covered conductor (CC)/high voltage insulator based electrical distribution systems10.1016/j.epsr.2021.107601 ↗
9. Investigation of hydrothermally stressed silicone rubber/silica micro and nanocomposite for the coating high voltage insulation applications10.3390/ma14133567 ↗
10. Application of coatings in outdoor high-voltage installations
11. Hydrophobic, dielectric and water immersion performance of 9000 h multi-stresses aged silicone rubber composites for high voltage outdoor insulation10.1016/j.engfailanal.2021.105223 ↗
12. Accelerated aging investigation of silicone rubber/silica composites for coating of high-voltage insulators10.1007/s00202-016-0498-7 ↗
13. Life estimation and investigation of dielectric strength and siloxane backbone of high voltage silicone rubber composites under accelerated multistress conditions10.1007/s13369-019-03839-1 ↗
14. Investigation of electrical properties of silica-reinforced RTV nanocomposite coatings10.1007/s10854-021-05855-0 ↗
15. Transfer of hydrophobicity of polymeric insulating materials for high voltage outdoor application10.1109/TDEI.2017.006146 ↗
16. Performance of silicone rubber insulators under thermal and electrical stress10.1109/TIA.2017.2672667 ↗
17. Influence of corona discharge on hydrophobicity of silicone rubber used for outdoor insulation10.1016/j.polymertesting.2018.12.011 ↗
18. Reliability assessment of RTV and nano-RTV-coated insulators concerning contamination severity10.1016/j.epsr.2020.106892 ↗
19. Suppression of silicone rubber erosion by alumina trihydrate and silica fillers from dry-band arcing under DC10.1109/TDEI.2014.004484 ↗
20. DC inclined-plane tracking and erosion test of insulating materials10.1109/TDEI.2014.004991 ↗
21. Comparative study of AC and DC inclined plane tests on silicone rubber (SiR) insulation<? show [AQ="" ID=" Q1]"?10.1049/hve.2016.0102 ↗
22. Effects of thermal properties on tracking and erosion resistance of micro-ATH/AlN/BN filled silicone rubber composites10.1109/TDEI.2018.007125 ↗
23. Analyzing the role of filler interface on the erosion performance of filled RTV silicone rubber under DC dry-band Arcing10.1109/TDEI.2021.009337 ↗
24. Tracking/erosion resistance analysis of Nano-Al (OH) 3 filled silicone rubber insulating materials for high voltage dc applications10.5370/JEET.2015.10.1.355 ↗
25. Thermal conductivity and dielectric properties of silicone rubber nanocomposites
26. Degradation analysis of RTV-SiR based composites under both polarities DC voltage for insulators coating10.1016/j.mtcomm.2021.102890 ↗
27. Anti-aging characteristics of RTV-SiR aided HV insulator coatings: impact of DC polarity and fillers10.1016/j.matchemphys.2021.125634 ↗
28. Standard · 1992 · vol. 1109
29. Guide for the selection of insulators in respect of polluted conditions
30. Online hydrophobicity measurement for silicone rubber insulators on transmission lines10.1109/TPWRD.2008.2005654 ↗
31. Accelerated multi stress aging and life estimation of polymeric insulators
32. Hydrophobicity loss and recovery of silicone HV insulation10.1109/TDEI.1999.9286763 ↗
33. Performance of silicone rubber in DC inclined plane tracking tests10.1109/TDEI.2010.5448108 ↗
34. Performance of silicone rubber composites with SiO2 micro/nano-filler under AC corona discharge10.1109/TDEI.2016.7736840 ↗
35. Tracking and erosion of silicone rubber nanocomposites under DC voltages of both polarities10.1109/TDEI.2012.6148506 ↗
36. RTV silicone rubber degradation induced by temperature cycling10.3390/en10071054 ↗
37. Accelerated aging effect on high temperature vulcanized silicone rubber composites under DC voltage with controlled environmental conditions10.1016/j.engfailanal.2020.104870 ↗
38. Accelerated ultraviolet weathering investigation on micro‐/nano‐SiO2 filled silicone rubber composites10.1049/hve.2018.5004 ↗
39. Resistance against AC corona discharge of micro-ATH/nano-Al2O3 co-filled silicone rubber composites10.1109/TDEI.2018.006914 ↗
40. In-service aging and degradation of 345 kV EPDM transmission line insulators in a coastal environment10.1109/TDEI.2004.1285906 ↗
41. Multi-stress aging investigations of HTV silicone rubber filled with Silica/ATH composites for HVAC and HVDC transmission10.1016/j.engfailanal.2020.104449 ↗
42. Photodegradation and photostabilization of polymers, especially polystyrene10.1186/2193-1801-2-398 ↗
43. Mechanical, thermal, and morphological behavior of silicone rubber during accelerated aging10.1080/03602559.2017.1419487 ↗
44. Investigation of multiple-stresses on mechanical and thermal properties of 9000 h Aged RTV-SiR composites for high-voltage insulation10.1177/0095244320953588 ↗
45. Mahmood · 2020
46. Measuring electrical, thermal and mechanical properties of DC-stressed HTV silicone rubber loaded with nano/micro-fillers exposed to long-term aging10.1007/s13204-020-01381-3 ↗
47. AC performance of HTV-SR and its hybrids loaded with nano-/micro-silica/ATH fillers10.1007/s13369-020-04938-0 ↗
48. Photodegradation and photostabilization of polymers, especially polystyrene10.1186/2193-1801-2-398 ↗
49. Preparation and thermo-mechanical properties of functionalized graphene/silicone rubber nanocomposites
50. Aging evaluation of silicone rubber insulators using leakage current and flashover voltage analysis10.1109/TDEI.2013.6451360 ↗
51. Characteristics of silicone composites for high voltage insulations10.1515/rams-2018-0040 ↗