Abstract
Two series of tungsten thin films are sputtered on silicon and glass substrates by oblique angle co-deposition technique with an original configuration. Two opposite distinct tungsten targets are simultaneously used, both tilted with an oblique angle of 80°. The growth is performed at low (0.33 Pa) and high (1.5 Pa) argon sputtering pressure and the current intensity applied to the targets varies between 50 and 250 mA. The effect of these deposition parameters on the films microstructure and electrical properties is investigated by scanning and transmission electron microscopy, X-ray diffraction and pole figures, and van der Pauw method. Due to self-shadowing effect, all tungsten sputtered thin films are porous and columnar. At low pressure, the columnar tilt angle β can be tuned with the target current intensity until obtaining vertical columns. X-ray diffraction and pole figure analyses point out a A15 crystal structure (β-W) and a uniaxial fiber texture with a <100> growth direction. In contrast, tungsten thin films deposited at high pressure present a cauliflower structure and are poorly crystallized. Both deposition parameters also affect the films electrical resistivity and anisotropy. These behaviors are discussed and linked to the microstructure and crystallography.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Optical Coatings and Gratings · Photonic Crystals and Applications · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Dependence of geometric magnetic anisotropy in thin iron films10.1103/PhysRev.113.1039 ↗
2. Anisotropy in Permalloy films10.1063/1.2185921 ↗
3. Tailoring growth and local composition by oblique-incidence deposition: a review and new experimental data10.1016/0927-796X(94)90021-3 ↗
4. Columnar microstructure in vapor-deposited thin films10.1016/0040-6090(77)90037-2 ↗
5. Oblique evaporation and surface diffusion10.1016/S0040-6090(97)00095-3 ↗
6. Optical, structural, and magnetic properties of cobalt nanostructure thin films10.1063/1.3138809 ↗
7. Grain structure and magnetic anisotropy of Fe film evaporated obliquely from two sources10.1143/JJAP.20.1249 ↗
8. Resistivity anisotropy of tilted columnar W and W–Cu thin films10.1016/j.surfcoat.2021.127412 ↗
9. Platinum-doped CeO2 thin film catalysts prepared by magnetron sputtering10.1021/la100399t ↗
10. Perspectives on oblique angle deposition of thin films: from fundamentals to devices10.1016/j.pmatsci.2015.06.003 ↗
11. Tailoring of highly porous SnO2 and SnO2-Pd thin films10.1016/j.matchemphys.2018.11.022 ↗
12. Fabrication of thin films with highly porous microstructures10.1116/1.579579 ↗
13. K. Robbie and M. J. Brett, J. Vac. Sci. Technol., A 15 (1197) 1460–1465 “Sculptured thin films and glancing angle deposition: growth mechanics and applications” https://doi.org/10.1116/1.580562.10.1116/1.580562 ↗
14. Advanced techniques for glancing angle deposition10.1116/1.590019 ↗
15. Hawkeye · 2014
16. Advanced multi-component nanostructures designed by dynamic shadowing growth10.1039/c1nr10103j ↗
17. Inhomogeneous concentration distribution in obliquely evaporated Fe-Cu films10.1143/JJAP.25.1668 ↗
18. Catalytic properties of thin films by simultaneous oblique sputter deposition of two materials from different directions10.1016/0040-6090(94)06279-X ↗
19. Two-component nanopillar arrays grown by glancing angle deposition10.1016/j.tsf.2005.08.128 ↗
20. Designing catalytic nanomotors by dynamic shadowing growth10.1021/nl070461j ↗
21. Multi-component nanostructure design by atomic shadowing10.1016/j.tsf.2008.05.049 ↗
22. Origin of anomalous magnetic anisotropy of iron films evaporated at oblique incidence10.1143/JPSJ.28.254 ↗
23. Anisotropic broadening of Cu nanorods during glancing angle deposition10.1063/1.2388861 ↗
24. Influence of thickness and sputtering pressure on electrical resistivity and elastic wave Propagation in oriented columnar tungsten thin films10.3390/nano10010081 ↗
25. Architectured columns with a metal-dielectric periodic nanostructure10.1016/j.matlet.2016.02.161 ↗
26. Correlation between structure and electrical resistivity of W-Cu thin films prepared by GLAD co-sputtering10.1016/j.surfcoat.2017.01.039 ↗
27. Contrasted morphologies in nanostructured Janus W-Cu columns10.1016/j.mtcomm.2021.102331 ↗
28. Microstructural analysis and electrical behaviours of co-sputtered W–Ag thin films with a tilted columnar architecture10.1088/1361-6463/abf312 ↗
29. Mobility and carrier density in materials with anisotropic conductivity revealed by van der Pauw measurements10.1103/PhysRevB.70.165307 ↗
30. Measuring anisotropic resistivity of single crystals using the van der Pauw technique10.1103/PhysRevB.92.045210 ↗
31. Oblique-incidence anisotropy in evaporated Permalloy films10.1063/1.1735441 ↗
32. Alpha- vs. beta-W nanocrystalline thin films: a comprehensive study of sputter parameters and resulting materials' properties10.1016/j.tsf.2015.01.030 ↗
33. Morphology control of tungsten nanorods grown by glancing angle RF magnetron sputtering under variable argon pressure and flow rate10.1016/j.physleta.2010.08.066 ↗
34. Scaling during shadowing growth of isolated nanocolumns10.1103/PhysRevB.68.125408 ↗
35. Tilt angle control of nanocolumns grown by glancing angle sputtering at variable argon pressures10.1063/1.3506502 ↗
36. Composition dependent nanocolumn tilting angle during the oblique angle co-deposition10.1063/1.3676665 ↗
37. Microfractography of thin films
38. Modelling and characterization of columnar growth in evaporated films10.1016/0040-6090(93)90378-3 ↗
39. Microstructure and magnetism in amorphous rare-earth–transition-metal thin films. I. Microstructure10.1063/1.325249 ↗
40. β-phase tungsten nanorod formation by oblique-angle sputter deposition10.1063/1.1618944 ↗
41. The formation of vertically aligned biaxial tungsten nanorods using a novel shadowing growth technique10.1088/0957-4484/20/46/465609 ↗
42. Phase transformation of sputter deposited tungsten thin films with A15 structure10.1063/1.362584 ↗
43. Influences of oxygen on the formation and stability of A15 β-W thin films10.1016/S0921-5093(00)00745-0 ↗
44. The phase transformation of thin sputter-deposited tungsten films at room temperature10.1116/1.1506905 ↗
45. Creation of biaxial body center cubic tungsten nanorods under dynamic shadowing effect10.1016/j.tsf.2013.04.151 ↗
46. Structure and stability of sputter deposited beta-tungsten thin films10.1063/1.111318 ↗
47. Unravelling oxygen driven α to β phase transformation in tungsten10.1038/s41598-020-71650-2 ↗
48. Structure and properties of stacking faulted A15 tungsten thin films10.1023/A:1004847009613 ↗
49. Impact of deposition rate, underlayers, and substrates on β−tungsten formation in sputter deposited films10.1116/1.5003628 ↗
50. Surface energies of elemental crystals10.1038/sdata.2016.80 ↗
51. Lide · 1991