The influence of Y3+ and Mg2+ dopants on the transparency behavior of alumina ceramics
Source abstract
Abstract
Abstract The effect of salt solution of magnesium and yttrium addition on the transparent alumina polycrystalline was investigated in the present study. This solution is ionized in the slurry. The ions were adsorbed onto the charged alumina surface by the electrostatic mechanism. Due to the addition of salts solution at the casting stage, the distribution of dopant was uniform. Therefore no secondary phase has been formed in the sample after sintering. The added salts eliminated the intragranular porosity and prevented the growth of the grains. After optimizing the amount of the dispersant (1.3 wt%) and preparing the slurry by using a 3D-mixer, the samples were sintered at a temperature of 1250 °C and at the rate of 20 °C/min by the SPS method, the transparency was increased from 18 to 33% by adding salt solution of the Mg2+ and Y3+ as dopant. Also, the grain size was decreased from 27.37 to 4.29 μm in the sample with dopant, therefore the hardness was increased from 1814 to 2279 HV10.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Glass properties and applications · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Transparent ceramic lamp envelope materials10.1088/0022-3727/38/17/S07 ↗
2. Transparent sintered sub-μm Al2O3 with IR transmissivity equal to sapphire
3. Electrophoretic shaping of sub-micron alumina in ethanol10.1016/j.ceramint.2008.10.033 ↗
4. Effects of heating rate on microstructure and transparency of spark-plasma-sintered alumina10.1016/j.jeurceramsoc.2008.03.015 ↗
5. Effects of high concentrations of liquid phase and magnesia on the grain growth of alumina10.1016/S0272-8842(97)00075-8 ↗
6. Coble · 1962
7. Structure-transmittance relationship in transparent ceramics10.1016/j.jallcom.2019.01.124 ↗
8. Light scattering in MgO-doped alumina fabricated by spark plasma sintering10.1016/j.actamat.2010.04.049 ↗
9. Transparent polycrystalline alumina using spark plasma sintering: effect of Mg, Y and La doping10.1016/j.jeurceramsoc.2009.12.001 ↗
10. Effect of amount of doping agent on sintering, microstructure and optical properties of Zr- and La-doped alumina sintered by SPS10.1016/j.jeurceramsoc.2013.11.015 ↗
11. The influence of dopants on loss tangent of polycrystalline alumina ceramics
12. Nettleship · 2003 · vol. 352 · 287
13. Preparation of SiO2 glass from model powder compacts: II, sintering10.1111/j.1151-2916.1984.tb19165.x ↗
14. The effect of slip casting parameters on the green density of MgAl2O4 spinel10.1016/j.ceramint.2017.01.151 ↗
15. Optical and mechanical properties of compaction and slip cast processed transparent polycrystalline spinel ceramics10.1016/j.ceramint.2013.10.149 ↗
16. Yodel: a yield stress model for suspensions10.1111/j.1551-2916.2005.00888.x ↗
17. Lead zirconate titanate particle dispersion in thick‐film ink formulations10.1111/j.1151-2916.2000.tb01402.x ↗
18. The effect of slip casting parameters on the green density of MgAl2O4 spinel10.1016/j.ceramint.2017.01.151 ↗
19. Çinar · 2013 · 161
20. Cinar · 2013
21. Suspension stability: why particle size, zeta potential and rheology are important
22. Effect of particle size on the shaping of ceramics by slip casting10.1016/j.jeurceramsoc.2010.03.019 ↗
23. Colloidal processing of ceramics10.1111/j.1151-2916.2000.tb01560.x ↗
24. Critical rotation speed for ball-milling10.1016/S0032-5910(99)00031-5 ↗
25. Fine‐grained transparent spinel windows by the processing of different nanopowders10.1111/j.1551-2916.2010.03814.x ↗
26. Atomistic simulation of Y-doped a -alumina interfaces
27. The effect of slip casting and spark plasma sintering (SPS) temperature on the transparency of MgAl2O4 spinel10.1016/j.ceramint.2017.10.228 ↗
28. The effect of yttrium on densification and grain growth in α-alumina10.1016/S1359-6454(02)00159-3 ↗
29. Yttria doping and sintering of submicrometer‐grained α‐alumina10.1111/j.1151-2916.1996.tb08950.x ↗