Abstract Si-filler-loaded poly(methylsilsesquioxane) was pyrolyzed in nitrogen atmosphere between 1250 and 1600 °C to fabricate Si–O–C–N micro-composite materials. The evolution of the microstructure and the resulting nanocomposition were studied by X-ray diffraction, scanning electron microscopy (SEM), high-voltage electron microscopy, high-resolution electron microscopy, electron energy-loss spectroscopy (esp. energy-loss near-edge structures), and porosity analysis. At pyrolysis temperatures below the melting point of Si (1414 °C) the silicon oxynitride (Si2ON2) formation proceeds via a vapor phase reaction between SiO and N2 in the pores and results in fiber-like aggregates with distinct core–shell structures containing nanocrystalline regions. At higher temperatures the molten Si filler is involved in the silicon oxynitride formation reactions, and above 1500 °C a complete conversion of the Si filler and the Si–C–O matrix into Si2ON2 takes place with a significant reduction of the porosity in comparison to the gas phase reaction regime.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Walker · Bull. Am. Ceram. Soc. · 1983 · 62 · 916
2. Wynne · Ann. Rev. Mater. Sci. · 1984 · 14 · 29710.1146/annurev.ms.14.080184.001501 ↗
3. Peuckert · Adv. Mater. · 1990 · 2 · 39810.1002/adma.19900020903 ↗
4. Bill · Adv. Mater. · 1995 · 7 · 77510.1002/adma.19950070903 ↗
5. Greil · Adv. Eng. Mater. · 2000 · 2 · 33910.1002/1527-2648(200006)2:6<339::AID-ADEM339>3.0.CO;2-K ↗
6. Greil · J. Am. Ceram. Soc. · 1995 · 78 · 83510.1111/j.1151-2916.1995.tb08404.x ↗
7. Seyferth · J. Am. Ceram. Soc. · 1991 · 74 · 268710.1111/j.1151-2916.1991.tb06824.x ↗
8. Suttor · J. Am. Ceram. Soc. · 1997 · 80 · 254110.1111/j.1151-2916.1997.tb03156.x ↗
9. Renlund · J. Mater. Res. · 1991 · 6 · 271610.1557/JMR.1991.2716 ↗
10. Hurwitz · Ceram. Eng. Sci. Proc. · 1989 · 10 · 75010.1002/9780470310557.ch25 ↗
11. Pippel · J. Eur. Ceram. Soc. · 1997 · 17 · 125910.1016/S0955-2219(96)00228-2 ↗
12. Colombo · J. Mater. Sci. · 1998 · 33 · 240510.1023/A:1004312109836 ↗
13. Colombo · Mater. Res. Soc. Symp. Proc. · 1994 · 346 · 40310.1557/PROC-346-403 ↗
14. Lightfoot · Ceram. Eng. Sci. Proc. · 1995 · 16 · 65310.1002/9780470314784.ch6 ↗
15. Wei · Mater. Chem. Phys. · 2002 · 73 · 28110.1016/S0254-0584(01)00395-9 ↗
16. Scheffler · Key Eng. Mater. · 2002 · 206–213 · 289
17. Vogt · Key Eng. Mater. · 1994 · 89–91 · 29
18. Chollon · J. Mater. Sci. · 1998 · 33 · 152910.1023/A:1017555518483 ↗
19. Chollon · J. Eur. Ceram. Soc. · 1998 · 18 · 53510.1016/S0955-2219(97)00162-3 ↗
20. Boch · J. Mater. Sci. · 1979 · 14 · 37910.1007/BF00589829 ↗
21. Ohashi · Ceram. Int. · 1997 · 23 · 2710.1016/0272-8842(95)00136-0 ↗
22. Heim · J. Eur. Ceram. Soc. · 1997 · 17 · 90510.1016/S0955-2219(96)00201-4 ↗
23. Olsson · J. Eur. Ceram. Soc. · 1996 · 16 · 53510.1016/0955-2219(95)00126-3 ↗
24. Hajji · Thin Film Solids · 1999 · 354 · 910.1016/S0040-6090(99)00650-1 ↗
25. Modreanu · Thin Film Solids · 1999 · 337 · 8210.1016/S0040-6090(98)01189-4 ↗
26. Lichtenberger · Phys. Stat. Sol. A · 1995 · 150 · 66110.1002/pssa.2211500209 ↗
27. Schneider · J. Phys. D: Appl. Phys. · 1996 · 29 · 17010.1088/0022-3727/29/7/005 ↗
28. Schneider · Mikrochim. Acta Suppl. · 1996 · 13 · 545
29. Pippel · J. Mater. Sci. Lett. · 2000 · 19 · 205910.1023/A:1026748027434 ↗
30. M. Scheffler, T. Gambaryan-Roisman, T. Takahashi, J. Kaschta, H. Muenstedt, P. Buhler, P. Greil, Ceram. Trans. 108 (2001) 239 [Innovative Processing and Synthesis of Ceramics, Glasses, and Composites IV].