journal article·2015-11

Corrosion degradation of powder composite hydride electrodes in conditions of long-lasting cycling

Henryk Bala, Martyna Dymek

Publisher page

Abstract

Abstract The LaNi4.5Co0.5 hydrogen storage material degradation process in 6 M KOH solution fulfills first-order chemical reaction kinetic law. After ca 10 first cycles, up to N = 45 cycle, the logarithm of discharge capacity linearly decreases with cycle number. The slope of logQdisch = f(N) straight lines is a measure of degradation rate constant (kdegr). Corrosion rate of the tested material is directly proportional to kdegr. The LaNi4.5Co0.5 powder encapsulation with electroless Ni–P is prone to evident increase of the hydride electrode corrosion resistance. Additionally, encapsulation improves the charge/discharge kinetics: the exchange currents of H2O/H2 system are 20% greater for the chemically treated powder.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen Storage and Materials · Fuel Cells and Related Materials · Hybrid Renewable Energy Systems

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Pourbaix · 1966
2. Theoretical evaluation for thermodynamic stability of constituents of hydrogen storage alloy in concentrated alkaline solution at higher temperature10.1016/S0925-8388(97)00428-3 ↗
3. Evaluation of the electrochemical hydrogenation and corrosion behaviour of LaNi5-based materials using galvanostatic charge/discharge measurements10.1016/j.ijhydene.2012.07.126 ↗
4. Hydrogen diffusivity, kinetics of H2O/H2 charge transfer and corrosion properties of LaNi5 powder, composite electrodes in 6M KOH solution10.1007/s10008-013-2322-x ↗
5. Progress in evaluation of metal hydride electrode charge time and time of oxide phases reduction
6. Development of metal hydride material efficient surface in conditions of galvanostatic charge/discharge cycling10.1016/j.matchemphys.2014.09.011 ↗
7. Electrochemical hydrogenation and corrosion properties of LaNi4.5Co0.5 alloy doped with aluminum10.1016/j.ssi.2014.11.005 ↗
8. Hydrogen absorption and corrosion resistance of LaNi4.8Al0.2 and LaNi4.8Al0.1Li0.1 alloys10.1016/j.jallcom.2006.07.041 ↗
9. Metal hydride electrodes stability of LaNi5-related compound
10. High cycle life, cobalt free AB5 metal hydride electrodes
11. Cerium content and cycle life of multicomponent AB5 hydride electrodes10.1149/1.2049999 ↗
12. Effect of Ni content on the structure, thermodynamic and electrochemical properties of the non-stoichiometric hydrogen storage alloys10.1016/S0925-8388(00)01049-5 ↗
13. The correlation between composition and electrochemical properties of metal hydride electrodes10.1016/S0925-8388(99)00413-2 ↗
14. Effect of cobalt on the physicochemical properties of a simple LaB5 metal hydride alloy10.1016/S0378-7753(02)00239-2 ↗
15. Pulverization and corrosion studies of bare and cobalt encapsulated metal hydride electrodes10.1016/S0378-7753(99)00399-7 ↗
16. Cycle life and utilization studies on cobalt microencapsulated AB5 type metal hydride10.1016/S0378-7753(99)00283-9 ↗
17. Effect of partial substitution of nickel by tin, aluminum, manganese and palladium on the properties of LaNi5-type metal hydride alloys10.1590/S0103-50532003000400009 ↗
18. Double-phase hydride forming compounds: a new class of highly electrocatalytic materials10.1149/1.2085893 ↗
19. Elaboration and characterization of magnesium-substituted La5Ni19 hydride forming alloys as active materials for negative electrode in Ni-MH battery10.1016/j.electacta.2008.09.069 ↗
20. Electrochemical properties of LaY2Ni9 hydrogen storage alloy used as an anode in nickel-metal hydride batteries10.1007/s10008-014-2448-5 ↗
21. Rechargeable batteries with aqueous electrolytes10.1016/S0013-4686(00)00344-3 ↗
22. Simulation of capacity fade in lithium-ion batteries10.1016/S0378-7753(02)00490-1 ↗
23. Capacity fade study of lithium-ion batteries cycled at high discharge rates10.1016/S0378-7753(03)00029-6 ↗
24. Thermodynamical properties of La-Ni -T (T = Mg, Bi and Sb) hydrogen storage systems10.1016/j.jpowsour.2007.12.018 ↗
25. Effect of cobalt replacement by nickel, manganese, aluminium and iron on the crystallographic and the electrochemical properties of AB5-type alloys10.1016/S0925-8388(03)00087-2 ↗
26. Effect of the pulverization of LaNi5 on the hydrogen absorption rate and the X-ray diffraction patterns10.1016/0022-5088(84)90122-X ↗
27. Influence of cobalt and manganese content on the hydrogenation capacity and kinetics of air-exposed LaNi5+x-type alloys in solid gas and electrochemical reactions10.1016/j.jpowsour.2007.04.003 ↗
28. Perez · 2004 · 90
29. 2000 · 45
30. Atkins · 2006
31. Kiss · 1988
32. The corrosion of iron in sulphate solutions at pH 0–210.1016/0013-4686(84)80050-X ↗
33. Hydrogenation and corrosion properties of LaNi4.5Co0.5-based alloy doped with 1.7 at% Sn10.4028/www.scientific.net/SSP.227.263 ↗
34. Anisotropic diffraction peak broadening and dislocation substructure in hydrogen-cycled LaNi5 and substitutional derivatives10.1107/S0021889800004556 ↗
35. Hydrogen equilibria characteristics of LaNi5-xZnx intermetallics10.1016/S0925-8388(99)00616-7 ↗
36. Electroless encapsulation of LaNi5-powder particles with Ni-P protective layers