Dielectric relaxation of fulleroid materials filled PA 6 composites and the study of its mechanical and tribological performance

Alex N. Sinitsin, Vjacheslav V. Zuev

Publisher page

Abstract

Abstract The effect of fulleroid materials (fullerene С60 and fullerene soot which is used for fullerenes production) on the mechanical and tribological properties of polymer nanocomposites based on polyamide 6 (PA6) was investigated. Composites were synthesized by direct mixing in an extruder. The use of the nanoparticles was an effective way to decrease the friction coefficient of the polymer composites because the fillers had the same size as the segments of the surrounding polymer chains. The steady state coefficients of friction with addition of fulleroid fillers were lower than that of unfilled PA6. The lowest coefficient of friction was observed for PA6 filled with 1 wt % fullerene soot. Dielectric spectroscopy was used to investigate the influence of nanoparticles on the relaxation processes in the polymer matrix. It is found that the segmental relaxation processes becomes faster with the addition of fullerene С60. In contrast, the secondary processes of PA6/fullerene C60 nanocomposites were observed to slow down with the addition of fullerene C60. This means that the local “molecular stiffness” is increased, and a phenomenological link between the secondary relaxation times and the mechanical properties explains the increase in the Young's modules of the nanocomposites upon the addition of С60. These observations suggest that nanoparticles can have a qualitatively different effect on the matrix polymer dynamics at different length scales, and caution must be taken in comparing the changes in the dynamics associated with different relaxation processes.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Tribology and Wear Analysis · Polymer Nanocomposites and Properties · Fullerene Chemistry and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Influence of fillers and fiber reinforcement on abrasive wear resistance of some polymeric composites10.1016/0043-1648(90)90169-B ↗
2. Nanoparticles as reinforced agents10.1038/381678a0 ↗
3. Strobl · 2007
4. [60] Fullerene chemistry for material science applications10.1039/a700080d ↗
5. How nano are nanocomposites10.1021/ma070356w ↗
6. Carbon nanotube–polymer composites: chemistry, processing, mechanical and electrical properties10.1016/j.progpolymsci.2009.09.003 ↗
7. Dielectric normal mode relaxation10.1016/0079-6700(93)90018-8 ↗
8. Mechanical and electrical properties of polyamide-6 based nanocomposites reinforced by fulleroid fillers10.1002/pen.22188 ↗
9. Kawauchi · Macromolecules · 2009 · 42 · 613610.1021/ma901235b ↗
10. Polyamide 12/fullerene C60 composites: investigation on their mechanical and dielectric properties10.1007/s10965-012-9925-2 ↗
11. Polymer nanocomposites containing carbon nanotubes10.1021/ma060733p ↗
12. Thermal and mechanical characterization of films from nylon 6/EVOH blends10.1016/S0014-3057(98)00197-9 ↗
13. Opportunities and challenges in the use of inorganic fullerene-like nanoparticles to produce advanced polymer nanocomposites10.1016/j.progpolymsci.2013.04.001 ↗
14. Effects of reprocessing on the structure and properties of polyamide 6 nanocomposites10.1016/j.polymdegradstab.2008.07.030 ↗
15. Secondary structure and elevated temperature crystallite morphology of nylon-6/layered silicate nanocomposites10.1016/S0032-3861(00)00414-6 ↗
16. Reinforcing efficiency of nanoparticles: a simple comparison for nanocomposites10.1016/j.compscitech.2007.10.033 ↗
17. Morphology and mechanical properties of multiwalled carbon nanotubes reinforced nylon-6 composites10.1021/ma049132t ↗
18. Polymorphism in nylon 6/clay nanocomposites10.1002/1521-3935(20001201)201:18<2820::AID-MACP2820>3.0.CO;2-4 ↗
19. Effects of crystalline forms on the deformation behaviour of nylon-610.1016/S0032-3861(97)10132-X ↗
20. Experimental characterization and modeling stiffness of polymer/clay nanocomposites within a hierarchical multiscale framework10.1002/app.30547 ↗
21. Implications of dielectric response for the mechanism of changes in oxygen transport due to traces of moisture in amorphous nylons10.1021/ma00016a033 ↗
22. Water absorption effect on the dynamic properties of nylon-6 by dielectric spectroscopy10.1021/ma034954w ↗
23. Moisture effect on the low- and high-temperature dielectric relaxations in nylon-610.1002/(SICI)1099-0488(199712)35:17<2879::AID-POLB11>3.0.CO;2-4 ↗
24. Water sorption and thermally stimulated depolarization currents in nylon-610.1002/(SICI)1099-0488(199608)34:11<1853::AID-POLB2>3.0.CO;2-T ↗
25. A complex plane analysis of α-dispersions in some polymer systems10.1002/polc.5070140111 ↗
26. A complex plane representation of dielectric and mechanical relaxation processes in some polymers10.1016/0032-3861(67)90021-3 ↗
27. Theories and simulations of polymer based nanocomposites: from chain statistics to reinforcement10.1016/j.progpolymsci.2008.02.003 ↗
28. Nanofillers in polymeric matrix: a study on silica reinforced PA610.1016/S0032-3861(01)00446-3 ↗
29. In-situ synthesis and characterization of polyamide 6/POSS nanocomposites10.1002/masy.200750348 ↗
30. Kremer · 2003
31. Relaxation in glassforming liquids and amorphous solids10.1063/1.1286035 ↗
32. The effect of fullerene C60 on the dielectric behaviour of epoxy resin at low nanofiller loading10.1016/j.cplett.2014.03.056 ↗
33. Polymers containing fullerene or carbon nanotube structures10.1016/j.progpolymsci.2004.08.001 ↗
34. Polymer nanocomposites containing fullerene C60 nanofillers10.1002/masy.201150320 ↗
35. Improvement of frictional properties and abrasive wear resistance of polyamide/graphite composite by oil impregnation10.1016/S0043-1648(02)00302-2 ↗
36. Sliding wear of polyimide/fullerene C60 composite coating10.1016/S0043-1648(03)00139-X ↗
37. Wear experiments with selected engineering polymers and polymer composites under dry reciprocating sliding conditions10.1016/S0043-1648(01)00795-5 ↗
38. Dry wear sliding characteristics of some industrial polymers against steel counterface10.1016/j.triboint.2004.03.002 ↗