journal article·2010-09

Electrical discharge machining of ZrO2 toughened WC composites

Olivier Malek, Jef Vleugels, Yeczain Perez, Patrick De Baets, Junhu Liu, Sven Van den Berghe, Bert Lauwers

Materials Chemistry and Physics· Volume 123· Issue 1
Publisher page

Abstract

Abstract The interrelationships between the dispersion of the ZrO 2 phase and the electrical discharge machining (EDM) behaviour of WC based composites with 0, 5 or 10 vol% of ZrO 2 are investigated. Special attention was given to the homogeneity of the ultrafine WC – nanometric ZrO 2 powder based composites which were fully densified by means of pulsed electric current sintering (PECS). X-ray photoelectron spectroscopy (XPS) measurements revealed the presence of a nanometric WO 3 layer on the EDM surface, confirming oxidation as the major material removal mechanism (MRM). The surface roughness after the final EDM finishing regime was strongly influenced by the composite homogeneity and could be reduced down to 0.15 μm ( R a ) on agglomerate-free composites. Residual stress measurements indicated that EDM did not introduce a significant amount of surface stresses, especially not after the final finishing regime. XRD measurements of EDM surfaces however indicated surface depletion of ZrO 2 by the formation of ZrC and W 2 C during spark erosion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced Machining and Optimization Techniques · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. Pressureless sintering and tribological properties of WC–ZrO2 composites10.1016/j.jeurceramsoc.2004.05.021 ↗
2. Influence of the type and grain size of the electro-conductive phase on the wire-EDM performance of ZrO2 ceramic composites10.1016/j.cirp.2008.03.089 ↗
3. Development of ZrO2–WC composites by pulsed electric current sintering10.1016/j.jeurceramsoc.2006.11.079 ↗
4. Processing of ultrafine ZrO2 toughened WC composites10.1016/j.jeurceramsoc.2009.07.013 ↗
5. ZrO2–WC nanocomposites with superior properties10.1016/j.jeurceramsoc.2006.05.028 ↗
6. Hard, tough and strong ZrO2–WC composites from nanosized powders10.1016/j.jeurceramsoc.2004.01.015 ↗
7. Modelling of the temperature distribution during field assisted sintering10.1016/j.actamat.2005.05.042 ↗
8. Thermal Stability of tungsten carbide in 7mol.% calcia–zirconia solid solution matrix heat treated in argon10.1016/j.jeurceramsoc.2005.12.012 ↗