Investigations on structural, optical and thermoelectric parameters of spray deposited bismuth selenide thin films with different substrate temperature
Source abstract
Abstract
Abstract A series of Bi 2 Se 3 films was deposited at different substrate temperature in 150–500 °C temperature range using spray pyrolysis technique, in order to study the effect of substrate temperature on structural and thermoelectric properties. The crystallinity of the as-synthesized sample has been analyzed by X-ray diffraction, which shows the formation of hexagonal Bi 2 Se 3 . Scanning electron microscopy examination indicates that the Bi 2 Se 3 microstructure strongly depends upon the change in substrate temperature. The optical absorption study shows that the direct band gap of the film decreases with increase in substrate temperature. The thermoelectrical measurements have shown n-type conductivity in as deposited films and the magnitude of Seebeck coefficient for films has been found to be increasing with increasing deposition temperature. Improved thermoelectric properties at higher substrate temperature shows promising aspect and Bi 2 Se 3 films could be a good thermoelectric material at lower temperature range.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Thermoelectric Materials and Devices · Topological Materials and Phenomena · Heusler alloys: electronic and magnetic properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Heremans · Science · 2008 · 321 · 55410.1126/science.1159725 ↗
2. Bell · Scie · 2008 · 321 · 145710.1126/science.1158899 ↗
3. Rowe · 1995
4. Patil · Chalcogenide Lett. · 2012 · 9 · 133
5. Bailini · Appl. Surf. Sci. · 2007 · 254 · 124910.1016/j.apsusc.2007.09.039 ↗
6. Chung · J. Am. Chem. Soc. · 2004 · 126 · 641410.1021/ja039885f ↗
7. Suriyanarayanan · Arch. Phys. Res. · 2010 · 1 · 81
8. Yadav · Chalcogenide Lett. · 2009 · 6 · 149
9. Torane · Chem. Solids · 2002 · 63 · 184910.1016/S0022-3697(02)00167-1 ↗
10. Hicks · Phys. Rev. B · 1993 · 47 · 1663110.1103/PhysRevB.47.16631 ↗
11. Hicks · Phys. Rev. B · 1993 · 47 · 1272710.1103/PhysRevB.47.12727 ↗
12. Venkatasubramanian · Nature · 2001 · 413 · 59710.1038/35098012 ↗
13. Liufu · Appl. Phys. Lett. · 2007 · 90 · 112106110.1063/1.2712504 ↗
14. Lin · J. Phys. Chem. C · 2007 · 111 · 1853810.1021/jp076886b ↗
15. Xia · Nat. Phys. · 2009 · 5 · 39810.1038/nphys1274 ↗
16. Zhang · Nat. Phys. · 2009 · 5 · 43810.1038/nphys1270 ↗
17. Goncalves · Vacuum · 2008 · 82 · 149910.1016/j.vacuum.2008.03.076 ↗
18. Sheng · Chin. Sci. Bull. · 2012 · 57 · 422010.1007/s11434-012-5018-1 ↗
19. Cho · Mater. Lett. · 2005 · 59 · 96610.1016/j.matlet.2004.10.074 ↗
20. Kim · Thin Solid Films · 2006 · 510 · 14810.1016/j.tsf.2005.12.306 ↗
21. Shafai · J. Vac. Sci. Technol. A · 1997 · 15 · 279810.1116/1.580826 ↗
22. Bottner · J. Microelectromech. Syst. · 2004 · 13 · 41410.1109/JMEMS.2004.828740 ↗
23. Yoo · Electrochim. Acta · 2005 · 50 · 437110.1016/j.electacta.2005.02.016 ↗
24. Takahashi · Thin Solid Films · 1994 · 240 · 7010.1016/0040-6090(94)90696-3 ↗
25. Martin-Gonzalez · J. Electrochem. Soc. · 2002 · 149 · C54610.1149/1.1509459 ↗
26. Miyazaki · J. Cryst. Growth · 2001 · 229 · 54210.1016/S0022-0248(01)01225-8 ↗
27. Takahashi · J. Electrochem. Soc. · 2003 · 150 · C16910.1149/1.1542898 ↗
28. Takahashi · J. Electrochem. Soc. · 1993 · 140 · 255010.1149/1.2220860 ↗
29. Pejova · Thin Solid Films · 2002 · 408 · 610.1016/S0040-6090(02)00085-8 ↗
30. Bari · Indian J. Pure Appl. Phys. · 2010 · 48 · 127
31. Okereke · J. Basic Phys. Res. · 2010 · 1 · 37
32. Venkatasubramanian · J. Cryst. Growth · 1997 · 170 · 81710.1016/S0022-0248(96)00656-2 ↗
33. Garćıa · Semicond. Sci. Tech. · 1997 · 12 · 64510.1088/0268-1242/12/5/020 ↗
34. Toda · Arch. Phys. Res. · 2011 · 3 · 431
35. Michel · J. Cryst. Growth · 2005 · 277 · 27410.1016/j.jcrysgro.2004.12.164 ↗