Damage evolutions of completely recrystallized W–Y2O3 composite evaluated using the dual effects of electron beam thermal shock and helium ion irradiation

Gang Yao, Zhi-Hao Zhao, Lai-Ma Luo, Ji-Gui Cheng, Xiang Zan, Qiu Xu, Yu-Cheng Wu

Publisher page

Abstract

Abstract Extreme service environments inevitably lead to the recrystallization of tungsten. This study investigates the behavior of completely recrystallized W–Y2O3 composite materials under transient thermal shock and helium irradiation conditions based on first wall service environment. The addition of Y2O3 particles exhibits a significant effect in terms of the crack resistance of the material. After helium ion irradiation, the aggregation of fuzz structures inside the cracks becomes increasingly evident as the crack width in the thermal shock region increases. Moreover, the resistance of Y2O3 particles to irradiation damage improves as the particle size decreases. The phase interface plays an important role in the helium ions irradiation process.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. ASDEX Upgrade Teama, Materials for the plasma-facing components of fusion reactors10.1016/j.jnucmat.2004.04.005 ↗
2. Development of advanced high heat flux and plasma-facing materials10.1088/1741-4326/aa6f71 ↗
3. Plasma facing and high heat flux materials – needs for ITER and beyond10.1016/S0022-3115(02)01175-3 ↗
4. Development of a helium-cooled divertor concept: design-related requirements on materials and fabrication technology10.1016/j.jnucmat.2004.04.137 ↗
5. Preparation of ultrafine-grained/nanostructured tungsten materials: an overview10.1016/j.jallcom.2018.11.279 ↗
6. Grain growth behavior and mechanical properties of zirconium micro-alloyed and nano-size zirconium carbide dispersion strengthened tungsten alloys10.1016/j.ijrmhm.2015.03.019 ↗
7. Microstructure and mechanical properties of HfC reinforced W matrix composites regulated by trace Zr10.1016/j.ijrmhm.2019.105096 ↗
8. Microstructure and helium irradiation performance of W–ZrC/Sc2O3 composites prepared spark plasma sintering10.1016/j.ijrmhm.2018.01.011 ↗
9. Recrystallization kinetics of warm-rolled tungsten in the temperature range 1150–1350 °C10.1016/j.jnucmat.2014.08.037 ↗
10. Plasma facing materials and components for future fusion devices-development, characterization and performance under fusion specific loading conditions10.1088/0031-8949/2006/T123/006 ↗
11. Thermal diffusivity of tungsten irradiated with protons up to 5.8 dpa10.1016/j.jnucmat.2018.06.041 ↗
12. Annealing effect on the microstructure of tungsten irradiated in SINQ target10.1016/j.jnucmat.2017.12.020 ↗
13. Experimental and numerical simulations of ELM-like transient damage behaviors to different grade tungsten and tungsten alloys10.1016/j.jnucmat.2014.12.114 ↗
14. Formation of helium induced nanostructure ‘fuzz’ on various tungsten grades10.1016/j.jnucmat.2010.06.034 ↗
15. Investigation of microstructure and microhardness of pure W and W-2Y2O3 materials before and after ion-irradiation10.1016/j.ijrmhm.2014.06.004 ↗
16. Helium retention and surface blistering characteristics of tungsten with regard to first wall conditions in an inertial fusion energy reactor10.1016/j.nimb.2005.07.060 ↗
17. Response of tungsten surfaces to helium and hydrogen plasma exposure under ITER relevant steady state and repetitive transient conditions10.1088/1741-4326/aa81e4 ↗
18. Mechanical properties of tungsten irradiated with high-energy protons and spallation neutrons10.1016/j.jnucmat.2018.12.003 ↗
19. Helium-induced hardening effect in polycrystalline tungsten10.1016/j.nimb.2017.02.029 ↗
20. Influence of helium ion irradiation damage behavior after laser thermal shock of W-2%vol Y2O3 composites10.1016/j.pnucene.2020.103241 ↗
21. Mat. Numerical and experimental study on the thermal shock strength of tungsten by laser irradiation10.1016/j.msea.2007.04.077 ↗
22. Comparison of thermal shock damages induced by different simulation methods on tungsten
23. ITER relevant high heat flux testing on plasma facing surfaces10.2320/matertrans.46.412 ↗
24. Mechanical properties and microstructural change of W–Y2O3 alloy under helium irradiation10.1038/srep12755 ↗
25. Isotropic thermal conductivity in rolled large-sized W-Y2O3 bulk material prepared by powder metallurgy route and rolling deformation technology, Fusion
26. Development and optimization of STEP-A linear plasma device for plasma-material interaction studies, Fusion
27. SRIM - the stopping and range of ions in matter10.1016/j.nimb.2010.02.091 ↗
28. Baseline high heat flux and plasma facing materials for fusion10.1088/1741-4326/aa6b60 ↗
29. Effect of Y2O3 particles on the helium ion irradiation damage of W-2%Y2O3 composite prepared by wet chemical method
30. Surface damage evolution during transient thermal shock of W-2%vol Y2O3 composite material in different surfaces10.1016/j.fusengdes.2019.01.010 ↗
31. Helium, hydrogen, and fuzz in plasma-facing materials10.1088/2053-1591/aa8c22 ↗
32. Motion of W and He atoms during formation of W fuzz10.1088/1741-4326/aab96a ↗
33. 3D modelling of tungsten fuzz growth under the bombardment of helium plasma10.1016/j.fusengdes.2018.03.019 ↗
34. The effect of Y2O3 addition on He desorption behavior and He bubble evolution in He-charged W-Y2O3 film10.1016/j.tsf.2020.138184 ↗
35. D2 retention behavior and microstructural evolution of W-2wt.%Y2O3 alloy during He-ion irradiation at high temperatures10.1016/j.jnucmat.2020.152273 ↗
36. The interaction of injected helium with lattice defects in a tungsten crystal10.1080/00337577208231184 ↗
37. Surface damages of polycrystalline W and La2O3-doped W induced by high-flux He plasma irradiation10.1016/j.jnucmat.2018.01.047 ↗
38. Effect of starting microstructure on helium plasma-materials interaction in tungsten10.1016/j.actamat.2016.11.042 ↗
39. Mechanism of interaction between interface and radiation defects in metal10.7498/aps.68.20190128 ↗
40. Strong trapping and slow diffusion of helium in a tungsten grain boundary10.1016/j.jnucmat.2017.02.010 ↗
41. Temperature threshold for preferential bubble formation on grain boundaries in tungsten under in-situ helium irradiation10.1016/j.scriptamat.2020.01.013 ↗