High temperature tribological behaviors of (WAl)C–Co ceramic composites with the additions of fluoride solid lubricants
Source abstract
Abstract
Abstract The tribological behaviors of the (W0.67Al0.33)C0.67–Co/fluoride (CaF2, BaF2, CaF2/BaF2) composites against SiC ball from room temperature to 600 °C were investigated. A marked increase in the friction coefficient resulting from fluoride oxidation was observed as the temperature increased. The composites containing BaF2 or (Ca, Ba)F2 displayed better integrated wear resistance over a wide temperature range compared with (W0.67Al0.33)C0.67–Co/CaF2. The high temperature tribological characteristics of the three composites were distinct, which originated from the composition difference on the worn surfaces. First, the SiO2/SiC film formed on the worn surfaces of the composites with BaF2 or (Ca, Ba)F2 was favorable for their wear resistance. Second, the oxidation of WC matrix was an important factor influencing the wear resistance of the composites. When mixture oxides of WO2 and WO3 appeared on the surface, wear is severe. In addition, single WO3 formed on the worn surfaces, appeared more adhesive to the underlying substrate and decreased the wear rate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Mechanical properties and chemical bonding characteristics of WC and W2C compounds10.1016/j.ceramint.2013.10.022 ↗
2. Application of fine-grained tungsten carbide-based cemented carbides10.1016/0263-4368(95)92672-7 ↗
3. Synthesis and characterization of WC-VC-Co nanocomposite powders through thermal-processing of a core-shell precursor10.1016/j.ceramint.2013.05.092 ↗
4. Microstructural control of ultrafine and nanocrystalline WC-12Co-VC/Cr3C2 mixture by spark plasma sintering10.1016/j.ceramint.2010.11.026 ↗
5. Sintering of binderless WC-Mo2C hard materials by rapid sintering process10.1016/j.ceramint.2007.03.029 ↗
6. Zirconia-toughened WC with/without VC and Cr3C210.1016/j.ceramint.2013.07.111 ↗
7. Synthesis of WC-Ni composite powders by thermochemical processing method based on co-precipitation10.1016/j.matchemphys.2014.09.057 ↗
8. Fabrication, thermal stability and mechanical properties of novel composite hardmetals obtained by solid-state reaction and hot-pressing sintering10.1016/j.matchemphys.2007.10.009 ↗
9. Synthesis, crystal structure, and density of (W1−xAlx)C10.1016/j.jssc.2004.03.009 ↗
10. Nanostructured bulk novel hard material with “rounded” grains obtained by nanocrystalline “rounded” (W0.5Al0.5)C powders10.1016/j.msea.2008.07.013 ↗
11. Friction and wear behaviors of the carbide tools embedded with solid lubricants in sliding wear tests and in dry cutting processes10.1016/j.wear.2011.01.031 ↗
12. Unlubricated friction and wear behaviors of Al2O3/TiC ceramic cutting tool materials from high temperature tribological tests10.1016/j.ijrmhm.2012.03.011 ↗
13. Tool wear and its effect on microstructure and properties of friction stir processed Ti-6Al-4V10.1016/j.matchemphys.2014.04.002 ↗
14. Tribological properties and cutting performance of boron and silicon doped diamond films on Co-cemented tungsten carbide inserts10.1016/j.diamond.2013.01.004 ↗
15. Progress in high temperature nanomechanical testing of coatings for optimising their performance in high speed machining10.1016/j.surfcoat.2014.02.062 ↗
16. Self-lubrication of sintered ceramic tools with CaF2 additions in dry cutting10.1016/j.ijmachtools.2005.07.047 ↗
17. Tribological behaviors of hot-pressed Al2O3/TiC ceramic composites with the additions of CaF2 solid lubricants10.1016/j.jeurceramsoc.2005.02.010 ↗
18. Friction and wear behaviors of the carbide tools embedded with solid lubricants in sliding wear tests and in dry cutting processes10.1016/j.wear.2011.01.031 ↗
19. Performance of carbide tools with textured rake-face filled with solid lubricants in dry cutting processes10.1016/j.ijrmhm.2011.08.002 ↗
20. Al2O3/(W,Ti)C/CaF2 multi-component graded self-lubricating ceramic cutting tool material10.1016/j.ijrmhm.2014.04.006 ↗
21. Investigation of (WAl)C-Co ceramic composites with the additions of fluoride solid lubricants: preparation, mechanical properties and tribological behaviors10.1016/j.ijrmhm.2013.05.004 ↗
22. Mechanisms of sliding wear of metals and alloys at elevated temperatures10.1016/j.triboint.2007.10.003 ↗
23. High temperature tribological behavior of a Ti-46Al-2Cr-2Nb intermetallics10.1016/j.intermet.2012.06.013 ↗
24. Influence of Cr content on tribological properties of Ni3Al matrix high temperature self-lubricating composites10.1016/j.triboint.2011.05.014 ↗
25. Effect of fluoride content on friction and wear performance of Ni3Al matrix high-temperature self-lubricating composites10.1007/s11249-011-9812-8 ↗
26. The role of atmospheres and lubricants in the oxidational wear of metals10.1016/S0301-679X(02)00034-8 ↗
27. A crystal-chemical approach to lubrication by solid oxides10.1023/A:1019183101329 ↗
28. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗