Abstract The present work investigates the influence of minor-alloying element Ta on the microstructural evolution and mechanical properties of HR3C ASS (Fe-25Cr-22Ni-0.4Nb-0.18N-0.07C, wt. %) at elevated temperatures. Alloy ingots are prepared in a vacuum arc furnace and then hot-rolled, solid-solutioned at 1423 K/0.5 h, stabilized at 1173 K/0.5 h, and finally aged at 973 K for different hours (25–408 h). The microstructure and precipitated phases in different heat-treatment states are characterized with optical microscopy (OM), scanning electron microscopy (SEM), X-ray fluorescence spectrometer (XRF), electron probe microanalysis (EPMA), and transmission electron microscope (TEM), respectively. The experimental results show that Ta minor-alloying can suppress the precipitation of brittle σ and Cr23C6 phases effectively, as evidenced that only a few of σ and Cr23C6 particles appear on the grain boundaries after 408 h aging, exhibiting a high microstructural stability. It is attributed to the amount of Nb and Ta elements, which satisfies the composition rule that the molar ratio of (Nb + Ta)/C is 1/1. In addition, the micro-hardness of Ta-modified alloys doesn't vary significantly with the aging time, which are consistent with the high microstructural stability. The strengthening mechanisms of stabilized alloys are also discussed, which demonstrate that the precipitation strengthening of (Nb, Ta)C carbides is dominant in Ta-modified alloys.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Corrosion mechanisms of candidate structural materials for supercritical water-cooled reactor
2. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
3. The influence and the mechanism of the precipitate/austenite interfacial C-enrichment on the intergranular corrosion sensitivity in 310 S stainless steel10.1016/j.corsci.2016.05.021 ↗
4. Effect of thermal treatment on the corrosion resistance of Type 316L stainless steel exposed in supercritical water10.1016/j.jnucmat.2015.04.030 ↗
5. Alumina-forming austenitic alloys resist high-temperature corrosion
6. Materials challenges for the supercritical water-cooled reactor (SCWR)
7. Materials challenges in nuclear energy10.1016/j.actamat.2012.11.004 ↗
8. Mechanical properties of fuel cladding candidate alloys for Canadian SCWR concept
9. Selection of fuel cladding material for nuclear fission reactors10.1016/j.engfailanal.2011.06.010 ↗
10. Corrosion behavior of Hastelloy C-276 in supercritical water10.1016/j.corsci.2009.05.041 ↗
11. Corrosion behavior of Austenitic and Ferritic steels in supercritical water10.5516/NET.2008.40.2.147 ↗
12. Mikami · 2011 · 408
13. Long term creep properties and microstructure of SUPER304H, TP347HFG and HR3C for A-USC boilers
14. Study on aging embrittlement of new type austenitic heat resistant steel HR3C used in USC boiler
15. Yang · 2006
16. Long term creep properties and microstructure of SUPER304H, TP347HFG and HR3C for A-USC boilers10.1179/174892408X382860 ↗
17. Study on hot workability and optimization of process parameters of a modified 310 austenitic stainless steel using processing maps10.1016/j.matdes.2014.11.041 ↗
18. Influence of Ti, C and N concentration on the intergranular corrosion behaviour of AISI 316Ti and 321 stainless steels10.1016/j.actamat.2006.11.021 ↗
19. Microstructural evolution in two variants of NF709 at 1023 and 1073 K,10.1007/s11661-005-0135-y ↗
20. In situ TEM study of G-phase precipitates under heavy ion irradiation in CF8 cast austenitic stainless steel10.1016/j.jnucmat.2015.04.042 ↗
21. Hot deformation behavior and microstructural evolution of a modified 310 austenitic steel10.1016/j.matdes.2014.08.001 ↗
22. Influences of Mo/Zr minor-alloying on the phase precipitation behavior in modified 310S austenitic stainless steels at high temperatures10.1016/j.matdes.2017.04.095 ↗
23. Effect of tantalum content on microstructure and tensile properties of CLAM steel10.1016/j.fusengdes.2016.01.016 ↗
24. Study on hot workability and optimization of process parameters of a modified 310 austenitic stainless steel using processing maps10.1016/j.matdes.2014.11.041 ↗
25. Microstructural analysis on creep properties of dissimilar materials joints between T92 martensitic and HR3C austenitic steels10.1016/j.msea.2011.04.057 ↗
26. Microstructural characterization and the effect of phase transformations on toughness of the UNS S31803 duplex stainless steel aged treated at 850 °C10.1590/S1516-14392002000300026 ↗
27. Microstructural analysis of heat-resistant welded pipes10.1016/j.matchar.2003.09.005 ↗
28. Evolution of secondary phases in austenitic stainless steels during long-term exposures at 600, 650 and 800 °C10.1016/j.matchar.2008.04.009 ↗
29. Basic creep models for 25Cr20NiNbN austenitic stainless steels10.1179/1433075X13Y.0000000120 ↗
30. Transformation of austenite during isothermal annealing at 600 - 900 °C for heatresistant stainless steel10.1016/j.jallcom.2013.03.102 ↗
31. TEM examination of precipitation behaviour of M23C6 and sigma phases and dislocations in SS 310S under creep deformation at 800 °C, Microsc
32. Hot deformation behavior and microstructural evolution of a modified 310 austenitic steel10.1016/j.matdes.2014.08.001 ↗
33. Phase equilibria in the Fe-Nb system10.1007/s11669-010-9808-3 ↗
34. Experimental study and thermodynamic re-assessment of the binary Fe–Ta system10.1016/j.intermet.2011.03.018 ↗
35. Averbach · 1971
36. The isotropic shear modulus of multicomponent Fe-base solid solutions10.1016/S1359-6454(02)00096-4 ↗
37. The negative effect of Zr addition on the high temperature strength in alumina-forming austenitic stainless steels10.1016/j.matchar.2013.10.029 ↗
38. Hosford · 2005
39. Particle strengthening of metals and alloys
40. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al(Sc) alloys10.1016/S1359-6454(02)00201-X ↗
41. Mechanical properties of Al(Sc,Zr) alloys at ambient and elevated temperatures10.1016/S1359-6454(03)00320-3 ↗
42. The strength of a precipitation hardened AlZnMg alloy10.1016/0001-6160(78)90127-X ↗
43. Precipitation hardening caused by a difference in shear modulus between particle and matrix10.1002/pssa.2210780223 ↗
44. First-principles study of structural, elastic, and electronic properties of chromium carbides10.1063/1.2838345 ↗
45. First-principles study of structural, electronic, elastic, phonon, and thermodynamical properties of the niobium carbide10.4028/www.scientific.net/SSP.171.67 ↗