journal article·2021-11

Wettability and spreading behavior of Sn–Cr alloys on SiC

Zhenxing Fan, Min Guo, Wei Fu, Yidi Xue, Shengpeng Hu, Xiaoguo Song

Publisher page

Abstract

Abstract Knowing of the wetting of filler alloy on substrate is significant for brazing. Here, the isothermal wetting behavior of Sn-xCr alloys (x = 1, 2, 3, 4 and 5 wt%) on SiC substrates was studied by a modified sessile drop method in the temperature range of 1173 K–1323 K. The interfacial microstructures were characterized by scanning electron microscope (SEM) and X-ray diffraction (XRD) and its evolution was analyzed thermodynamically. Also, the spreading kinetics is calculated and the formation of precursor film is discussed. The spreading of Sn melt on SiC consists of rapid-spreading and sluggish-spreading stages. A better wettability is obtained at higher Cr concentration and isothermal temperature. The direct reaction between Cr and SiC forming metallics Cr–C compounds (Cr3C2, Cr7C3 and Cr23C6) at the interface accounts for the improving wettability of Sn melt on SiC. More metallic Cr–C compound occupies a higher proportion of interfacial layer inducing a lower final contact angle. Temperature has a violent influence on the spreading kinetic constant Kr. The spreading activity energy is calculated to be 312 kJ/mol.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced ceramic materials synthesis · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Self lubrication of pressureless sintered SiC ceramics
2. Monitoring the temperature of reactor experiments using radiation-induced swelling in SiC
3. MCMB–SiC composites; new class high-temperature structural materials for aerospace applications10.1016/j.ceramint.2012.05.098 ↗
4. Microstructure and electronic property of pristine and thermal barrier layers TiN/AlN/ZrB2 buffered 4H-SiC/W interface from first principles study10.1016/j.apsusc.2020.147820 ↗
5. Low frequency dielectric behavior and AC conductivity of polymer derived SiC(O)/HfCxN1-x ceramic nanocomposites10.1016/j.matchemphys.2020.124122 ↗
6. Facile synthesis of ceramic SiC-based nanocomposites and the superior electrochemical lithiation/delithiation performances10.1016/j.matchemphys.2019.122618 ↗
7. Reliable brazing of SiBCN ceramic and TC4 alloy using AgCuTi filler with the assist of laser melting deposited FGM layers10.1007/s10853-018-3025-6 ↗
8. Wetting of AgCu-Ti filler on porous Si3N4 ceramic and brazing of the ceramic to TiAl alloy10.1016/j.ceramint.2017.11.212 ↗
9. Wetting and brazing of Cf/C composite with Si–Zr eutectic alloy: the formation of nano- and coarse-SiC reaction layers10.1016/j.carbon.2020.05.109 ↗
10. Wettability and bonding of graphite by Sn0.3Ag0.7Cu-Ti alloys10.1016/j.carbon.2017.06.030 ↗
11. Wetting of porous graphite by Cu–Ti alloys at 1373K10.1016/j.matchemphys.2010.07.001 ↗
12. Shear strength and wettability of active Sn3.5Ag4Ti(Ce,Ga) solder on Al2O3 ceramics10.1016/j.matdes.2011.03.022 ↗
13. Influence of interfacial reaction on reactive wettability of molten Ag-Cu-X wt.%Ti filler metal on SiC ceramic substrate and mechanism analysis10.1016/j.apsusc.2017.12.106 ↗
14. Effect of Ti addition on the wetting and brazing of Sn0.3Ag0.7Cu filler on SiC ceramic10.1111/jace.16245 ↗
15. A study of the wetting, microstructure and bond strength in brazing SiC by C-X (X=Ti; V, Nb, Cr) alloys10.1007/BF00352679 ↗
16. Wetting and spreading behavior of Sn–Ti alloys on SiC10.1016/j.mtla.2018.10.005 ↗
17. Effect of Cr content in Ni-based amorphous filler on microstructure and shear strength of K4169 nickel-based alloy brazed joint10.1016/j.jmatprotec.2020.116975 ↗
18. Effect of Cr and V coatings on W base material in W-Eurofer brazed joints for fusion applications10.1016/j.fusengdes.2020.111748 ↗
19. Wetting of silicon carbide by chromium contanining alloys10.1016/S1359-6454(98)00037-8 ↗
20. Wettability of Ni–Cr filler on SiC ceramic and interfacial reactions for the SiC/Ni–51Cr system10.1016/j.scriptamat.2011.02.027 ↗
21. Wetting of SiC by molten Cu–20Me–2Cr (Me=Ag, Mn, Si, and Sn) alloys at 1373 K
22. Effect of Ti content on the metallization layer and copper/alumina brazed joint10.1016/j.ceramint.2017.07.016 ↗
23. Study on contact angles of Au, Ag, Cu, Sn, Al and Al alloys to SiC10.1007/BF00372193 ↗
24. Thermal Expansion Coefficient of Silicon Carbide (SiC): Data Extracted from the Landolt-Börnstein Book Series and Associated Databases., Springer-Verlag Berlin Heidelberg, Germany.
25. Microstructure and mechanical strength of SiC joints brazed with Cr3C2 particulate reinforced Ag-Cu-Ti brazing alloy10.1016/j.ceramint.2018.04.002 ↗
26. Experimental study of the influence of interfacial energies and reactivity on wetting in metal/oxide systems10.1007/BF02651601 ↗
27. Effects of the relative contents of silver and copper on the interfacial reactions and bond strength in the active brazing of SiC10.1007/BF00595743 ↗
28. Barin · 1995
29. Precursor film of tin-based active solder wetting on ceramics10.1007/BF00400889 ↗
30. Effect of Cr on the wetting in Cu/graphite system10.1016/j.apsusc.2011.02.060 ↗
31. The Cr-Sn (Chromium-Tin) system10.1007/BF02890556 ↗
32. The nature of the chemical bond in the carbides and nitrides of d metals10.1007/BF00518445 ↗
33. Wettability of porous surfaces10.1039/tf9444000546 ↗
34. Wetting of graphite by molten Cu–xSn–yCr ternary alloys at 1373 K10.1016/j.carbon.2019.12.097 ↗
35. Wetting of polycrystalline α-Al2O3 by molten Zr55Cu30Al10Ni5 metallic glass alloy10.1007/s11661-008-9718-8 ↗
36. Characteristics of precursor film in the wetting of Zr-based alloys on ZrC substrate at 1253K10.1016/j.tsf.2014.02.074 ↗
37. Wetting: statics and dynamics10.1103/RevModPhys.57.827 ↗
38. Brandes · 2013 · vol. 28 · 1
39. High temperature interaction behavior at liquid metal-ceramic interfaces10.1361/105994902770343917 ↗
40. Eustathopoulos · 1999
41. First principles calculations study of crystallographic orientation effects on SiC/Ti and SiC/Cr interfaces10.1016/j.microrel.2018.02.019 ↗
42. Estimation of the surface tensions of binary liquid alloys10.1007/BF02655927 ↗
43. Chemical reaction-limited spreading: the triple line velocity versus contact angle relation10.1016/S1359-6454(02)00309-9 ↗
44. The reactive wetting kinetics of interfacial tension: a reaction-limited model10.1039/C6RA28628C ↗
45. Wetting of polycrystalline SiC by molten Al and Al−Si alloys10.1016/j.apsusc.2014.08.055 ↗
46. The wettability of silicon carbide by liquid aluminium: the effect of free silicon in the carbide and of magnesium, silicon and copper alloy additions to the aluminium10.1007/BF00356199 ↗
47. Wettability of SiC to aluminium and aluminium alloys10.1179/mst.1987.3.5.378 ↗