journal article·2024-05

Influences of oxidation and hot corrosion on the tribological properties of CoCrNiWMo alloy and the preliminary exploration of the interaction between hot corrosion and wear

Hui Huang, Wenzhen Wang, Gewen Yi, Yu Shan, Shanhong Wan, Guimin Zhang, Xujing Du, Min Wan

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced materials and composites · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. Sliding tribocorrosion behavior of Fe-based bulk metallic glass under corrosive environments10.1016/j.jnoncrysol.2018.12.024 ↗
2. Methods of measuring wear-corrosion synergism10.1016/0043-1648(94)07108-X ↗
3. Tribocorrosion behavior of 2205 duplex stainless steel in sodium chloride and sodium sulfate environments10.1007/s11249-022-01601-7 ↗
4. Effect of Cl−on the corrosive wear of AISI 321 stainless steel in H2SO4 solution10.1007/BF02711188 ↗
5. Assessing the tribocorrosion performance of three different nickel-based superalloys10.1007/s11249-009-9552-1 ↗
6. High temperature induced “glaze” layer formed in HVOF-sprayed NiCrWMoCuCBFe coating and its wear reduction mechanism10.1007/s40544-021-0557-6 ↗
7. Corrosion performance of heat resistant alloys in Na2SO4–V2O5 molten salts10.1016/j.msea.2006.06.138 ↗
8. Influence of alloying elements on hot corrosion resistance of nickel-based single crystal superalloys coated with Na2SO4 salt at 900 °C10.1016/j.matdes.2020.109197 ↗
9. Influence of the combined-effect of NaCl and Na2SO4 on the hot corrosion behaviour of aluminide coating on Ni-based alloys10.1016/j.jallcom.2019.03.165 ↗
10. Vapour aluminide coating of internal cooling channels, in turbine blades and vanes10.1016/S0257-8972(99)00346-1 ↗
11. Microstructure and sliding wear behaviour of Tribaloy T-800 coatings deposited by laser cladding10.1016/j.wear.2005.04.020 ↗
12. Cobalt-base high-temperature alloys10.1126/science.1121738 ↗
13. Alloying effects and effective alloy design of high-Cr CoNi-based superalloys via a high-throughput experiments and machine learning framework10.1016/j.actamat.2022.118525 ↗
14. A novel wear-resistant Ni-based superalloy via high Cr-induced subsurface nanotwins and heterogeneous composite glaze layer at elevated temperatures10.1016/j.triboint.2023.108383 ↗
15. Remarkable wear resistance in a complex concentrated alloy with nanohierarchical architecture and composition undulation10.34133/research.0160 ↗
16. Effect of annealing treatment on the microstructure, mechanical and tribological properties of chromium carbonitride coatings10.1016/j.surfcoat.2018.12.099 ↗
17. High-temperature oxidation behavior of a Ni-Cr-W-Al alloy10.1016/S1005-0302(11)60152-7 ↗
18. The effect of pre-oxidation on microstructure, mechanical properties and high-temperature tribological behaviors of HVOF-sprayed NiCoCrAlYTa coating10.1016/j.apsusc.2019.05.334 ↗
19. Self-lubrication mechanism via the in situ formed lubricious oxide tribofilm10.1016/j.wear.2005.02.025 ↗
20. Sliding wear characteristics of molybdenum containing Stellite 12 coating at elevated temperatures10.1016/j.triboint.2015.06.006 ↗
21. Role of B2O3 and CaO in Al2O3 matrix composite: in-situ phases, density, hardness and wear resistance10.1016/j.triboint.2022.107588 ↗
22. Reactive wear protection through strong and deformable oxide nanocomposite surfaces10.1038/s41467-021-25778-y ↗
23. The effect of counterface on the tribological performance of a high temperature solid lubricant composite from 25 to 650°C10.1016/S0257-8972(96)02959-3 ↗
24. High temperature wear in CoCrFeNiCux high entropy alloys: the role of Cu10.1016/j.scriptamat.2018.10.007 ↗
25. Wear resistance of FeCoCrNiMnAlx high-entropy alloy coatings at high temperature10.1016/j.apsusc.2020.145736 ↗
26. Effects of sliding amplitude and normal load on the fretting wear behavior of alloy 690 tube exposed to high temperature water10.1016/j.triboint.2017.07.001 ↗
27. Corrosion effects on the nanotribology of a Ni62Nb38 metallic glass10.1016/j.apsusc.2021.151628 ↗
28. High temperature tribological properties of the D-gun WC-12Co coating in fluoride molten salt
29. Tribological behavior of 316H stainless steel in NaNO3-KNO3 molten salt at elevated temperature10.1016/j.solmat.2023.112377 ↗
30. High-temperature corrosion of Zr–Nb alloy for nuclear structural materials10.1016/j.pnucene.2022.104490 ↗
31. Effect of Zr, Ti, Ta and Mo addition on high-temperature oxidation and hot corrosion behavior of NiAlY alloys10.1016/j.jallcom.2022.164614 ↗
32. The iron effect on hot corrosion behaviour of MCrAlX coating in the presence of NaCl at 900 °C10.1016/j.jallcom.2019.152381 ↗
33. Improvement of the oxidation resistance of Tribaloy T-800 alloy by the additions of yttrium and aluminium10.1016/j.corsci.2010.11.038 ↗
34. Hot corrosion behaviour of yttrium and aluminium modified wear resistance coating alloy in mixed sulphate at 900 °C10.1016/j.corsci.2019.108369 ↗
35. Corrosion resistance and interfacial morphologies of a high Nb-containing TiAl alloy with and without thermal barrier coatings in molten salts10.1016/j.corsci.2019.05.011 ↗
36. Waterside corrosion of M5 alloy in lithiated/borated and supercritical water: influences of aqueous environments10.1016/j.supflu.2022.105828 ↗
37. Oxidation of typical Zr-1Nb alloy in high-temperature air under 700–900°C10.1016/j.corsci.2022.110701 ↗
38. Influence of Cr content on hot corrosion and a special tube sealing test of single crystal nickel base superalloy10.1016/j.corsci.2019.05.001 ↗
39. Comparative study of the oxidation and hot corrosion behaviors of TiAl-Cr intermetallic alloy produced by electric current activated sintering10.1016/j.jallcom.2018.11.324 ↗
40. Sulfur induced corrosion (SIC) mechanism of steam generator (SG) tubing at micro scale: a critical review10.1016/j.matchemphys.2019.05.056 ↗
41. Oxide scale adhesion and impurity segregation at the scale/metal interface10.1007/BF00665658 ↗
42. Surface and interface segregation in the oxidation of metals10.1002/1096-9918(200008)30:1<112::AID-SIA777>3.0.CO;2-G ↗
43. Prediction modeling of Type-I hot corrosion performance of Ti–Al–Mo-X (X=Cr, Mn) alloys in (Na, K)2SO4 molten salt mixture environment at 900°C10.1016/j.jallcom.2020.156010 ↗
44. Oxidation and hot corrosion of nickel-based alloys containing molybdenum10.1016/0010-938X(76)90010-X ↗
45. Formation of smooth wear surfaces on alumina ceramics by embedding and tribo-sintering of fine wear particles10.1016/S0043-1648(00)00468-3 ↗
46. Tribofilm formation and mild wear by tribo-sintering of nanometer-sized oxide particles on rubbing steel surfaces10.1016/j.wear.2006.03.046 ↗
47. The evolution mechanism of tribo-oxide layer during high temperature dry sliding wear for nickel-based superalloy10.1016/j.wear.2021.203747 ↗
48. Tribo-chemical wear of various 3d-transition metals against DLC: influence of tribo-oxidation and low-shear transferred layer10.1016/j.triboint.2022.107938 ↗
49. Observation of internal oxidation in a 20% cold-worked Fe-17Cr-12Ni stainless steel through high-resolution characterization10.1016/j.scriptamat.2019.08.019 ↗
50. A study on the surface and crack tip oxidation of alloy 600 through high-resolution characterization10.1016/j.corsci.2020.108616 ↗
51. Role of Cr in the high-temperature oxidation behavior of CrxMnFeNi high-entropy alloys at 800 °C in air10.1016/j.corsci.2022.110211 ↗
52. Structure and nano-mechanical characteristics of surface oxide layers on a metallic glass10.1088/0957-4484/22/9/095704 ↗
53. Effect of surface oxidation on the nm-scale wear behavior of a metallic glass10.1063/1.3573778 ↗
54. Investigation into the wear behaviour of Stellite 6 during rotation as an unlubricated bearing at 600°C10.1016/j.triboint.2011.02.011 ↗
55. Study on the oxidation behaviours and the interactions between friction and oxidation of the Ni-based composites with in-situ carbides reinforcement at 800 °C10.1016/j.corsci.2021.109987 ↗
56. Fretting wear-induced sudden loss of corrosion resistance in a corrosion-resistant Ni-based alloy10.1016/j.matchar.2023.112955 ↗
57. Chlorine-induced high-temperature corrosion characteristics of Ni-Cr alloy cladding layer and Ni-Cr-Mo alloy cladding layer10.1016/j.corsci.2023.111102 ↗
58. AlxCoCrFeNi high entropy alloys with superior hot corrosion resistance to Na2SO4 + 25% NaCl at 900 °C10.1016/j.corsci.2021.109479 ↗
59. A crystal-chemical approach to lubrication by solid oxides10.1023/A:1019183101329 ↗