journal article·2005-08

The anodic bonding between K4 glass and Si

P. Yu, Ch. Pan, J. Xue

Materials Letters· Volume 59· Issue 19-20
Publisher page

Abstract

Abstract This paper presents a systematic analysis of anodic bonding between silicon and K 4 glass at a relatively low temperature in air. The loop current increases rapidly at the beginning of bonding and then decreases gradually, which proves the migration of ions during bonding. Results show that the intimately contacted area of K 4 glass and Si increases with the bonding temperature increases from 300 °C to 400 °C. And the increase of bonding voltage also can increase the intimately contacted area. Good bonding can be achieved with different bonding temperatures (300–450 °C) and anodic voltages (700–850 V). The bonding mechanism is investigated by analyzing the microstructure of the bonding interface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: 3D IC and TSV technologies · Electronic Packaging and Soldering Technologies · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. A batch-fabricated silicon capacitive pressure transducer with low temperature sensitivity [J]
2. A capacitive pressure sensor with low impendence output and active suppression of parasitic effect10.1016/0924-4247(90)85021-U ↗
3. Precision. Accelerometers with μ g resolution10.1016/0924-4247(90)85059-D ↗
4. Silicon micro-accelerometer with μ g resolution, high linearity and large frequency bandwidth fabricated with two mask bulk process10.1016/S0924-4247(99)00051-5 ↗
5. The mechanism of field-assisted silicon-glass bonding10.1016/0924-4247(90)87064-P ↗
6. Electrostatic bonding of silicon solar cells
7. Experimental evaluation of anodic bonding process based on the Taguchi analysis of inter fracture toughness
8. Rate processes during anodic bonding10.1111/j.1151-2916.1992.tb05483.x ↗