Abstract Al2024 and Ti-6Al-4V alloy were joined by diffusion bonding in two successive stages. In first stage, Transient Liquid Phase of two dissimilar aerospace alloys, Ti-6Al-4V and Ti-6Al-4V welded at 620 °C using 50 µm thick Sn-5.3Ag-4.2Bi interlayer under argon by Transient Liquid phase method. In second stage, Al2024 was welded to Ti-6Al-4V at 453 °C by 50 µm thick Sn-5.3Ag-4.2Bi interlayer. Welded joints were observed and examined using optical, SEM, XRD and mapping Element showing, formation of Ag 3 Al, Ag 2 Al, and Al 3 Ti inter-metallic phases and Sn as solid solution bonding. Bi homogenized in two base metals. Welding tensile strength of Al2024 to Ti-6Al-4V is 62 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (9)

Show source-provided references
1. Transient liquid phase (TLP) bonding of Al7075 to Ti-6Al-4V alloy10.1016/j.matchar.2009.12.014 ↗
2. ASM. Aerospace Specification Metals Inc- ASM Material Data Sheet-800 398-4345. Aluminum 2024-O and Titanium Ti-6Al-4V (Grade 5), Annealed.
3. Evaluate of braze joint strength and microstructure characterize of titanium-CP with Ag-based filler alloy10.1016/j.matdes.2012.01.045 ↗
4. Friction stir welding of titanium alloy TiAl6V4 to aluminum alloy AA2024-T310.1016/j.msea.2009.07.006 ↗
5. Diffusion bonding of Al7075 to Ti–6Al–4V using Cu coatings and Sn–3.6Ag–1Cu interlayers10.1016/j.jallcom.2010.01.037 ↗
6. A study on the effect of bonding time on the properties of Al7075 to Ti-6Al-4V diffusion bonded joint10.1016/j.matlet.2012.02.104 ↗
7. An investigation on microstructure and mechanical properties of Al7075 to Ti-6Al-4V Transient Liquid Phase (TLP) bonded joint10.1016/j.matdes.2012.01.046 ↗
8. Microstructure and mechanical properties of Ti–6Al–4V/Al1060 joints by ultrasonic-assisted brazing in air10.1016/j.matlet.2012.12.105 ↗
9. Interaction behaviors at the interface between liquid Al–Si and solid Ti–6Al–4V in ultrasonic-assisted brazing in air10.1016/j.ultsonch.2012.06.011 ↗