Photoluminescence enhancement of nanoporous alumina using one-step anodization of high- and low-purity aluminum at room temperature
Source abstract
Abstract
Abstract In this article, we investigate the enhanced photoluminescence (PL) behavior of nanoporous anodic aluminum oxide (AAO) formed by one-step anodization of aluminum (Al) in oxalic acid at room temperature (25 °C) from both high- (99.99%) and low-purity (99%) Al. Compared with studies using the traditional two-step direct-current anodization at low temperature (0–10 °C), we introduce hybrid-pulse anodization to synthesize AAO from high- and low-purity Al at 25 °C for enhancing the PL. The PL intensity of high-purity AAO was stronger than the low-purity one due to the reduced surface scattering and intrinsic impurity inhibition. Besides the purity effect, AAO formed at the elevated temperature of 25 °C also greatly enhanced the PL intensity compared to that at the low temperature of 5 °C. Experimental results showed that both the high- and low-purity AAOs synthesized at 25 °C led to enhancements of the intensity of the PL peak by about 3.7–5.5-fold, depending on the Al purity and deconvoluted peak wavelength. These improvements were attributed to the high temperature enhancing the AAO thickness and reaction rate, thereby enabling more fluorescent ions to diffuse into the AAO for increased vacancy defects.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Anodic Oxide Films and Nanostructures · Semiconductor materials and devices · Ga2O3 and related materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (15)
Show source-provided references
1. Thompson · Nature · 1981 · 290 · 23010.1038/290230a0 ↗
2. Ghrib · Appl. Surf. Sci. · 2012 · 258 · 499510.1016/j.apsusc.2011.12.056 ↗
3. Juang · Microsyst. Technol. · 2005 · 11 · 95010.1007/s00542-005-0563-z ↗
4. Schlörb · Phys. Status Solidi B · 2010 · 247 · 236410.1002/pssb.201046189 ↗
5. Juhasz · Thin Solid Films · 2009 · 517 · 619810.1016/j.tsf.2009.04.010 ↗
6. Tasaltın · J. Alloys Compounds · 2011 · 509 · 470110.1016/j.jallcom.2011.01.081 ↗
7. Mateo · Nanotechnology · 2011 · 22 · 03570310.1088/0957-4484/22/3/035703 ↗
8. Buijnsters · ACS Appl. Mater. Interfaces · 2013 · 5 · 322410.1021/am4001425 ↗
9. Yamamoto · Nature · 1981 · 289 · 57210.1038/289572a0 ↗
10. Huang · J. Appl. Phys. · 2003 · 93 · 58210.1063/1.1529075 ↗
11. Khan · J. Luminescence · 2013 · 134 · 77210.1016/j.jlumin.2012.06.050 ↗
12. Kure-Chu · J. Electrochem. Soc. · 2015 · 162 · C2410.1149/2.0511501jes ↗
13. Belwalkar · J. Membr. Sci. · 2008 · 319 · 19210.1016/j.memsci.2008.03.044 ↗
14. Chung · Nanotechnology · 2009 · 20 · 05530110.1088/0957-4484/20/5/055301 ↗
15. Chung · Mater. Lett. · 2012 · 88 · 10410.1016/j.matlet.2012.08.047 ↗