journal article·2021-01

IMC suppression and phase stabilization of Cu/Sn-Bi/Cu microbump via Zn doping

Rui-Wen Song, Collin Jordon Fleshman, Yu-Ching Wang, Su-Yueh Tsai, Jenq-Gong Duh

Materials Letters· Volume 282
Publisher page

Abstract

Abstract For the advanced 3D-IC application, warpage and low thermal budget requires low temperature soldering for microbumps. Sn-Bi-Zn low temperature solder was studied for its low cost and accessibility. By doping Zn and adding Sn in solder and substrate metallization, not only the solder alloy was strengthened, but the microstructure was improved for better mechanical properties. The stabilization of melting behavior by doping Zn in substrate was analyzed. The exact phase composition was identified by color mapping and the reduction of Kirkendall void was elaborated in this study.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. Low temperature bonding technology for 3D integration10.1016/j.microrel.2011.03.038 ↗
2. The newly developed Sn–Bi–Zn alloy with a low melting point, improved ductility, and high ultimate tensile strength10.1016/j.mtla.2019.100300 ↗
3. Elastic properties, hardness, and indentation fracture toughness of intermetallics relevant to electronic packaging10.1557/JMR.2004.0193 ↗
4. Analysis and experimental verification of the volume effect in the reaction between Zn-doped solders and Cu10.1007/s11664-008-0521-5 ↗
5. Thermodynamic properties and melting behavior of Bi–Sn–Zn alloys10.1007/s00706-005-0457-x ↗
6. Eliminating interfacial segregation and embrittlement of bismuth in SnBi/Cu joint by alloying Cu substrate10.1016/j.scriptamat.2009.04.009 ↗
7. Improving the impact toughness of Sn–Ag–Cu/Cu–Zn Pb-free solder joints under high speed shear testing10.1016/j.jallcom.2013.10.113 ↗
8. Strong Zn concentration effect on the soldering reactions between Sn-based solders and Cu10.1557/jmr.2006.0320 ↗
9. Abnormal Cu3Sn growth through grain boundary penetration in space-confined Ni-Sn-Cu diffusion couples10.1016/j.jallcom.2019.05.328 ↗
10. Grain boundary phase transitions and phase diagrams10.1016/S1466-6049(01)00108-8 ↗