Abstract
Abstract The availability of large high-quality silicon carbide (SiC) single crystals is a key issue in the development of the full potential of SiC-based device technology. In this letter, 4H-SiC crystals were grown on the (000 1 ¯ ) substrates with 4° off-orientation toward 1 ¯ 00>. It had been found that there existed high density stacking faults (SFs) at the boundary between the 15R- and 4H-polytype. The HR-TEM observation revealed that this kind of SFs was of the 3C-SiC polytype. Meanwhile, the Raman spectra from these SFs suggested that the peaks at ~ 782 and ~ 796 cm− 1 were both sensitive to SFs. Especially, the band at ~ 782 cm− 1 can be the feature peak for identifying SFs with 15R inclusion.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon Carbide Semiconductor Technologies · Silicon and Solar Cell Technologies · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. Synthesis and characterization of bamboo-like SiC nanofibers10.1016/j.matlet.2005.10.115 ↗
2. A novel approach for the synthesis of 6H-SiC at a low temperature of 460°C10.1016/j.matlet.2006.02.003 ↗
3. Synthesis and characterization of nanostructured silicon carbide
4. Formation and suppression of misoriented grains in 6H-SiC crystals10.1039/c0ce00646g ↗
5. Formation and evolution of micropipes in SiC crystals10.1039/C1CE05806A ↗
6. Degradation of hexagonal silicon-carbide-based bipolar devices10.1063/1.2159578 ↗
7. Formation and properties of stacking faults in nitrogen-doped 4H-SiC10.1016/j.physb.2005.12.087 ↗
8. Deformation tests on 4H-SiC single crystals between 900°C and 1360°C and the microstructure of the deformed samples10.4028/www.scientific.net/MSF.338-342.517 ↗
9. The relationship between activation parameters and dislocation glide in 4H-SiC single crystals10.1002/1521-3951(200011)222:1<75::AID-PSSB75>3.0.CO;2-0 ↗
10. Plasticity and deformation microstructure of 4H-SiC below the brittle-to-ductile transition10.1002/pssc.200675438 ↗
11. Polytypic transformations in SiC: the role of TEM10.1016/0304-3991(93)90146-O ↗
12. Defects created in N-doped 4H-SiC in the brittle regime: Stacking fault multiplicity and dislocation cores10.1080/14786430902919497 ↗
13. Characterization of major in-grown stacking faults in 4H-SiC epilayers10.1016/j.physb.2009.08.189 ↗
14. Sources of epitaxial growth-induced stacking faults in 4H-SiC10.1007/s11664-010-1192-6 ↗
15. Sublimation growth of 6H- and 4H-SiC single crystals10.1016/S0022-0248(97)00289-3 ↗
16. Identification and control of SiC polytypes in PVT method10.1007/s10854-009-9914-3 ↗
17. Stacking fault energy of 6H-SiC and 4H-SiC single crystals10.1080/01418610008212090 ↗
18. Detection of stacking faults in 6H-SiC by Raman scattering10.1063/1.1329629 ↗
19. Raman investigation of SiC polytypes10.1002/1521-396X(199707)162:1<39::AID-PSSA39>3.0.CO;2-L ↗