Abstract The BaCo0.7Nb0.2Ta0.1O3−δ (BCNT) perovskite-type oxide was prepared by the conventional solid phase reaction method as a potential electrocatalyst for the oxygen reduction reaction. Its electrochemical properties were characterized. The results indicated that the BCNT oxide sintered at 1100 °C for 10 h had formed a single-phase cubic perovskite structure. And the BCNT–Sm0.2Ce0.8O1.9 (SDC) mixture co-sintered at the same conditions showed good chemical compatibility and stability between BCNT and SDC. The BCNT cathode sintered at 1000 °C for 4 h on SDC electrolyte exhibited the lowest the polarization resistance (about 0.0495 Ω·cm2 at 800 °C). Moreover, with a 351 μm-thick SDC as electrolyte and BCNT as the cathode, maximum power densities of the single cell reached 466.81 and 626.41 mW·cm−2 at 750 and 800 °C, respectively, and the corresponding total interface polarization resistance of the cell were 0.0913 Ω·cm2 and 0.0552 Ω·cm2. Short-term stability of the cell showed that the cell was quite stable at 750 °C for 15 h. This suggested that BCNT was a very promising cathode material for IT-SOFCs.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Electronic and Structural Properties of Oxides · Electrocatalysts for Energy Conversion

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Lin · J. Power Sources · 2008 · 180 · 1510.1016/j.jpowsour.2008.02.044 ↗
2. Nomura · Solid State Ionics · 1997 · 98 · 22910.1016/S0167-2738(97)00101-X ↗
3. Zhang · Ceram. Int. · 2010 · 36 · 63510.1016/j.ceramint.2009.09.040 ↗
4. Zhou · Electrochem. Commun. · 2008 · 10 · 164710.1016/j.elecom.2008.08.033 ↗
5. Cascos · Int. J. Hydrogen Energy · 2014 · 39 · 1434910.1016/j.ijhydene.2014.03.100 ↗
6. Nagai · Solid State Ionics · 2007 · 177 · 343310.1016/j.ssi.2006.10.022 ↗
7. Li · Nat. Commun. · 2017 · 8 · 1399010.1038/ncomms13990 ↗
8. Shao · Sep. Purif. Technol. · 2001 · 25 · 41910.1016/S1383-5866(01)00071-5 ↗
9. Zhu · J. Membr. Sci. · 2006 · 283 · 3810.1016/j.memsci.2006.06.010 ↗
10. Yang · J. Power Sources · 2011 · 196 · 916410.1016/j.jpowsour.2011.06.096 ↗
11. Zhu · Electrochem. Commun. · 2009 · 11 · 95810.1016/j.elecom.2009.02.034 ↗
12. Zhu · Ceram. Int. · 2005 · 31 · 11510.1016/j.ceramint.2004.03.042 ↗
13. Jin · Mater. Lett. · 2017 · 187 · 5310.1016/j.matlet.2016.10.047 ↗
14. Zhu · J. Alloy Compd. · 2016 · 694 · 87710.1016/j.jallcom.2016.09.297 ↗