journal article·2021-05

The effect of initial strain in the severe plastic deformation of aluminum on the subsequent work hardening regeneration through low strain amplitude multi-directional forging

Cleber Granato de Faria, Natanael Geraldo Silva Almeida, Karla Balzuweit, Maria Teresa Paulino Aguilar, Paulo Roberto Cetlin

Materials Letters· Volume 290
Publisher page

Abstract

Abstract Work hardening caused by Severe Plastic Deformation (SPD) strengthens ductile metals remarkably but practically annihilates their further work hardening during monotonic post-SPD deformation. Low Strain Amplitude Multi-Directional Forging (LSA-MDF) after one Equal Channel Angular Pressing (ECAP) pass of aluminum causes limited softening and regenerates its work hardening capacity. The full development of an SPD condition in aluminum demands an initial deformation higher than that associated with one ECAP pass. The present research analyzes the application of LSA-MDF to aluminum after 4 ECAP passes. A regeneration of the work hardening capacity of the material was observed. In addition, LSA-MDF caused an increased fraction of High Angle Grain Boundaries (HAGBs) in the material and a decrease in the presence of distorted grains displaying internal dislocation structures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and mechanical properties · Metallurgy and Material Forming · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. Fundamentals of superior properties in bulk nanoSPD materials10.1080/21663831.2015.1060543 ↗
2. Structural evolutions of metallic materials processed by severe plastic deformation10.1016/j.mser.2018.06.001 ↗
3. Nanostructured aluminium alloys produced by severe plastic deformation: New horizons in development10.1016/j.msea.2012.09.020 ↗
4. Increasing the work hardening capacity of equal channel angular pressed (ECAPed) aluminum through multi-axial compression (MAC)10.1016/j.matlet.2016.03.112 ↗
5. Microstructural evolution in the low strain amplitude multi-axial compression (LSA-MAC) after equal channel equal pressing (ECAP) of aluminum10.1016/j.matlet.2018.05.054 ↗
6. Mechanical behavior and microstructures of aluminum processed by low strain amplitude multi-directional confined forging10.1016/j.jmrt.2020.01.065 ↗
7. Twenty-five years of ultrafine-grained materials: Achieving exceptional properties through grain refinement10.1016/j.actamat.2013.08.018 ↗
8. Microstructural evolution in high purity aluminum processed by ECAP10.1016/j.msea.2009.06.032 ↗