Abstract

Abstract Sol–gel silica coatings increase wear and corrosion resistance of aluminium matrix composites, but a heat treatment stage at temperatures as high as 500 °C is usually required to consolidate the ceramic coating. Under these thermal conditions, sol–gel ceramic coatings tend to crack and the aluminium matrix hardness strongly reduces. Present paper describes how the combination of a certain sol–gel procedure accompanied with quenching treatment in silicone oil allows recovering most of the hardness of the substrate, while keeping undamaged the sol–gel silica coating deposited.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Electrophoretic Deposition in Materials Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. Pepe · Mater Lett · 2005 · 59 · 221910.1016/j.matlet.2005.03.001 ↗
2. Hamdy · Surf Coat Technol · 2006 · 201 · 40110.1016/j.surfcoat.2005.11.142 ↗
3. Smagorinski · Mater Sci Eng A · 1998 · 244 · 8610.1016/S0921-5093(97)00830-7 ↗
4. Niskanen · Adv Mater Process · 1988 · 3 · 39
5. Duralcan composites-mechanical and physical properties, in: Foundry Composites, SI Units, Duralcan USA, San Diego, CA, 1992.
6. Rams · Surf Coat Technol · 2006 · 201 · 371510.1016/j.surfcoat.2006.09.004 ↗
7. Rams · Surf Coat Technol · 2007 · 202 · 114410.1016/j.surfcoat.2007.07.059 ↗
8. Lopez · Surf. Coat. Tecnol. · 2008 · 202 · 375510.1016/j.surfcoat.2007.12.043 ↗
9. Cullity · Adv X-Ray Anal · 1977 · 60 · 25910.1007/978-1-4613-9981-0_22 ↗
10. Sengupta · J Appl Phys · 1998 · 83 · 229110.1063/1.366971 ↗